固废基胶凝材料对生态混凝土性能的影响

Effect of solid waste-based cementitious materials on the performance of ecological concrete

浏览量:

关键词:

再生微粉;赤泥;生态混凝土;孔隙率;抗压强度;抗硫酸盐侵蚀

Key words:

Recycled micro powder; Red mud; Ecological concrete; Porosity; Compressive strength; Sulfate resistance

刊期:

2025年第6期

DOI:

10.19761/j.1000-4637.2025.06.091.05

文章编号:

基金项目:

国家重点研发计划项目 (2018YFC0706000)。

作者:

户广旗1,任福民2,刘君实2,丁泰安2

单位:

1.威海中恒管桩有限公司,山东 威海 264405;2.北京交通大学威海研究院,山东 威海 264401

摘要

摘   要:研究了再生微粉与赤泥复掺比例(4∶0、3∶1、2∶2、1∶3、0∶4)对生态混凝土工作性、孔隙率、抗压强度和抗硫酸盐侵蚀性能的影响。结果表明:随着赤泥比例的增加,净浆的流动度降低,生态混凝土的总孔隙率、连通孔隙率、28 d抗压强度均先增大后降低;再生微粉与赤泥复掺降低了生态混凝土的抗硫酸盐侵蚀性能;综合考虑生态混凝土的各项性能,推荐再生微粉与赤泥的复掺比例为3∶1。

Abstract: The effects of the compound ratios(4∶0, 3∶1, 2∶2, 1∶3, 0∶4) of recycled micro powder and red mud on the workability, porosity, compressive strength and sulfate resistance of ecological concrete were investigated. The results show that with the increase of the proportion of red mud, the fluidity of the slurry decreases, the total porosity, the connected porosity, and the 28 d compressive strength of the ecological concrete first increase and then decrease. The compound mixing of recycled micro powder and red mud reduces the sulfate resistance of ecological concrete. Comprehensive consideration of the performance of ecological concrete, the recommended compound ratio of recycled micro powder and red mud is 3∶1.

结论

(1)随着赤泥比例的增加,净浆的流动度降低,仅当m再生微粉∶m赤泥为4∶0时,净浆的流动度高于JZ组,而当m再生微粉∶m赤泥为0∶4时,净浆几乎无流动性。
(2)随着赤泥比例的增加,试件的总孔隙率、连通孔隙率均先增后降,且二者之间的差值增大,当m再生微粉∶m赤泥为3∶1时,试件的总孔隙率最接近目标孔隙率。
(3)复掺再生微粉与赤泥降低了生态混凝土的28 d抗压强度,随着赤泥比例的增加,生态混凝土试件的28 d抗压强度先增大后降低;复掺适量再生微粉与赤泥对生态混凝土抗压强度的贡献效果优于单掺再生微粉或赤泥。
(4)复掺再生微粉与赤泥降低了试件的抗硫酸盐侵蚀性能,但不同m再生微粉∶m赤泥对试件抗压强度耐蚀系数的影响无明显规律;复掺适量再生微粉与赤泥对生态混凝土抗硫酸盐侵蚀性能的贡献效果优于单掺再生微粉或赤泥。在硫酸盐侵蚀初期,基体内部生成的膨胀性腐蚀产物AFt填充了部分孔隙,提高了基体密实度,但随着侵蚀的持续,AFt积累会导致试件膨胀开裂。
(5)综合考虑生态混凝土的各项性能,本试验推荐m再生微粉∶m赤泥为3∶1。

参考文献

[1] 全洪珠.多孔透水混凝土与植物共生性能试验研究[J].硅酸盐通报,2015,34(7):4.
[2] 杨慧,房辉,程志远,等.赤泥资源化综合利用研究进展[J].中国资源综合利用,2023,41(6):109-115.
[3] 马连涛,盛彦清,高大魁.赤泥在建筑材料制备中的资源化利用研究进展[J].新型建筑材料,2025,52(4):126-133.
[4] 黄鑫,程涵,游欣悦.赤泥资源化利用及放射性研究进展[J].再生资源与循环经济,2025,18(3):25-31.
[5] 郝跃鹏.氧化铝生产废渣赤泥的资源化综合利用[J].中国金属通报,2024(4):1-5.
[6] SONG W,GUO T T,HAN P J,et al.Durability study and mechanism analysis of red mud-coal metakaolin geopolymer concrete under a sulfate environment[J].Construction and Building Materials,2023,409:133990.
[7] 孟跃辉,张喜刚.2023年赤泥绿色利用十大进展[J].资源再生,2024(1):17,19.
[8] 刘松辉,管学茂,冯春花,等.赤泥安全堆存和综合利用研究进展[J].硅酸盐通报,2015,34(8):7.

[9] LI S J,CHEN G F,ZHAO Y S,et al.Investigation on the reactivity of recycled brick powder[J].Cement and Concrete Composites,2023,139:105042.
[10] 李述俊,赵霄龙,李秋义,等.再生微粉基本性能及活性试验研究[J].硅酸盐通报,2019,38(10):7.
[11] ZHAO Y S,GAO J M,XU Z H,et al.Long-term hydration and microstructure evolution of blended cement containing ground granulated blast furnace slag and waste clay brick[J].Cement and Concrete Composites,2021,118:103982.
[12] SINGH S B,MURUGAN M.Effect of metakaolin on the properties of pervious concrete[J].Construction and Building Materials,2022,346:128476.
[13] 张朝辉.多孔植被混凝土的研究[D].重庆:重庆大学,2006.
[14] 国家市场监督管理总局,国家标准化管理委员会.混凝土外加剂匀质性试验方法:GB/T 8077—2023[S].北京:中国标准出版社,2023.
[15] 汲博生.大孔生态混凝土实验研究[D].青岛:青岛理工大学,2013.
[16] HOU D S,WU D,WANG X P,et al.Sustainable use of red mud in ultra-high performance concrete (UHPC): Design and performance evaluation[J].Cement and Concrete Composites,2021,115:103862.
[17] 吕涛.冻融循环与动水冲刷交替作用下透水混凝土的试验研究[D].镇江:江苏大学,2018.
[18] 刘开伟,王爱国,孙道胜,等.硫酸盐侵蚀下钙矾石的形成和膨胀机理研究现状[J].硅酸盐通报,2016,35(12):6.
[19] 黄炳银,崔素萍,王亚丽,等.石膏溶解特性对无水硫铝酸钙水化进程的影响[J].硅酸盐通报,2023,42(5):1804-1813.

引用本文

户广旗,任福民,刘君实,等.固废基胶凝材料对生态混凝土性能的影响[J].混凝土与水泥制品,2025(6):91-94,99.

HU G Q,REN F M,LIU J M,et al.Effect of solid waste-based cementitious materials on the performance of ecological concrete[J].China Concrete and Cement Products,2025(6):91-94,99.


上一个: 低碳复合胶凝材料的制备及其对混凝土性能的影响

下一个: 盐冻环境下聚合物改性再生混凝土的损伤机制及寿命预测

相关文件