单轴压缩下不同含水率混凝土力学特性及本构模型研究

Study on the mechanical properties and constitutive model of concrete with varying moisture contents under uniaxial compression

浏览量:

关键词:

混凝土;含水率;单轴压缩;力学特性;破坏形态;本构模型

Key words:

Concrete; Moisture content; Uniaxial compression; Mechanical property; Failure mode; Constitutive model

刊期:

2026年第5期

DOI:

10.19761/j.1000-4637.26030094

文章编号:

基金项目:

新疆维吾尔自治区重大科技专项资助项目(2018A03003-2)。

作者:

陈兆志1,郭春志2,*

单位:

1.北京云星宇交通科技股份有限公司,北京 100070;2.中国船级社质量认证有限公司北京分公司, 北京 100007

摘要

摘   要:公路桥梁隧道混凝土结构常因地下水、雨水等因素处于不同含水率状态,易引发结构损伤并削弱其承载能力,威胁工程运营安全。为了明确不同含水率下混凝土的力学特性,建立适配的单轴压缩本构模型,本文以饱和度表征混凝土含水状态,设置了0、0.3、0.5、0.7、1.0 共5种工况,开展了单轴压缩试验,分析了饱和度对混凝土应力-应变曲线、力学参数及破坏形态的影响,拟合了各力学参数与饱和度的关系,构建了分段式本构模型并进行了验证。结果表明:不同饱和度混凝土峰前应力-应变曲线均含压密、弹性、裂纹扩展三个阶段,饱和度升高使曲线趋缓、峰值强度降低、塑性增强,破坏模式由剪切为主转为张拉为主;各力学参数与饱和度拟合相关性良好;所建模型(以弹性起始点为分界)计算值与实测值一致性良好,可有效描述不同饱和度混凝土单轴压缩力学行为。研究成果可为公路桥梁隧道工程中不同含水率混凝土承重构件的施工建设、结构设计及运营维护提供参考,也可为后续不同含水率混凝土压缩本构模型的建立提供理论依据。

Abstract: Concrete structures of highway bridges and tunnels are often subjected to different moisture content conditions due to groundwater, rainwater and other factors, which can easily cause structural damage, weaken their  load-bearing capacity and threaten the operational safety of engineering projects. To clarify the mechanical properties of concrete under different moisture contents and establish a suitable uniaxial compression constitutive model, this study employed the saturation degree to characterize the moisture state of concrete. Five saturation  degrees (0, 0.3, 0.5, 0.7, and 1.0) were designed, and a series of uniaxial compression tests were conducted. The effects of saturation degree on the stress-strain curves, mechanical parameters and failure modes of concrete were analyzed. The relationships between the mechanical parameters and the saturation degree were fitted, and a piecewise constitutive model was established and verified. The results show that the pre-peak stress-strain curves of concrete with different saturation degrees all exhibit three stages, namely compaction, elasticity and crack propagation. With the increase of saturation degree, the curve becomes flatter, the peak strength decreases, and the plasticity is enhanced, while the failure mode transforms from shear-dominated to tension-dominated. The mechanical parameters show good fitting correlation with saturation degree. The calculated values of the established model (taking the initial elastic point as the boundary) agree well with the measured ones, indicating that it can effectively describe the uniaxial compressive mechanical behavior of concrete with different saturation degrees. The research findings can provide references for the construction, structural design, operation and maintenance of load-bearing concrete Abstract: Concrete structures of highway bridges and tunnels are often subjected to different moisture content conditions due to groundwater, rainwater and other factors, which can easily cause structural damage, weaken their  load-bearing capacity and threaten the operational safety of engineering projects. To clarify the mechanical properties of concrete under different moisture contents and establish a suitable uniaxial compression constitutive model, this study employed the saturation degree to characterize the moisture state of concrete. Five saturation  degrees (0, 0.3, 0.5, 0.7, and 1.0) were designed, and a series of uniaxial compression tests were conducted. The effects of saturation degree on the stress-strain curves, mechanical parameters and failure modes of concrete were analyzed. The relationships between the mechanical parameters and the saturation degree were fitted, and a piecewise constitutive model was established and verified. The results show that the pre-peak stress-strain curves of concrete with different saturation degrees all exhibit three stages, namely compaction, elasticity and crack propagation. With the increase of saturation degree, the curve becomes flatter, the peak strength decreases, and the plasticity is enhanced, while the failure mode transforms from shear-dominated to tension-dominated. The mechanical parameters show good fitting correlation with saturation degree. The calculated values of the established model (taking the initial elastic point as the boundary) agree well with the measured ones, indicating that it can effectively describe the uniaxial compressive mechanical behavior of concrete with different saturation degrees. The research findings can provide references for the construction, structural design, operation and maintenance of load-bearing concrete

结论

(1)不同饱和度混凝土试件的峰前应力-应变曲线变化趋势一致,均包含压密段、弹性段和裂纹扩展段三个阶段;随着含水率升高,曲线整体趋于平缓,塑性变形与延性特征更显著,峰值强度逐步降低,塑性阶段范围扩大,破坏模式由剪切破坏为主向张拉破坏为主转变。
(2)单轴抗压强度随饱和度升高呈指数递减趋势,弹性模量、初始模量随饱和度升高呈对数递减趋势,峰值应变、弹性起始点应变随饱和度升高呈线性递增趋势,弹性起始点应力随饱和度升高呈线性递减趋势,各参数与饱和度的拟合关系均具有良好相关性。
(3)基于应力-应变曲线分段特征(以弹性起始点为分界),结合饱和度与各力学参数的拟合关系,建立了分段式不同饱和度混凝土单轴压缩本构模型。模型验证结果表明,除饱和度为0.3的试件在弹性变形段后的计算应变略大于实测值外,其余各饱和度下,模型计算值与试验实测值的一致性良好,说明模型参数取值合理,可有效描述不同饱和度混凝土的单轴压缩力学行为。

参考文献

[1] 时旭东,张备,韩源海.不同含水率预应力混凝土给定超低温有效预压性能试验研究[J/OL].工程力学,2026-04-14.https://link.cnki.net/urlid/11.2595.O3.20250317.1116.008.
[2] WU S S,FANG Q,ZHANG H G,et al.Investigation of damage mechanism of sawdust-magnesium oxychloride cement composites under uniaxial compressive load using AE and DIC techniques[J].Construction and Building Materials,2025,496:143762.
[3] 张国辉,倪新兰,陈现帆,等.高渗透水压力环境下混凝土湿度响应试验研究[J].水利水电科技进展,2024,44(5):55-59.
[4] 王海龙,田宇,银文文,等.不同湿度混凝土动力抗压性能数值模拟分析[J].水利学报,2020,51(4):421-429.
[5] QIU Y,TANG Y J,RUAN P Z,et al.Experimental study on effect of temperature and moisture on piezoresistive effect of carbon nanotube concrete[J].Smart Materials and Structures,2023,32(10):105031.
[6] 宁建国,杨帅,李玉辉,等.低温/常温养护下混凝土的本构模型和抗爆试验[J].兵工学报,2023,44(10):2932-2943.
[7] 马芹永,赵慧敏,袁璞,等.不同含水率蒸压轻质混凝土拉压性能试验研究[J].安徽理工大学学报(自然科学版),2022,42(1):50-55.
[8] 刘恒杰,李宗利,谭聪,等.不同含水率混凝土断裂过程声发射试验研究[J].工程科学与技术,2020,52(6):153-161.
[9] 刘琨,严武建,牛富航,等.含水率对掺硅灰混凝土声学特性的影响研究[J].混凝土与水泥制品,2019(9):15-18.
[10] 邵珠山,张鹏举,魏玮,等.微波辐射下含水率对混凝土力学性能影响[J].工程科学与技术,2021,53(6):93-102.
[11] 李俊贤,张宁宁.不同含水率条件下路面疏水混凝土冻融循环性能研究[J].中国新技术新产品,2024(8):81-83.
[12] 王中平,杨浩宇,赵亚婷,等.孔隙率及含水率对混凝土气体渗透系数的影响[J].混凝土,2019(6):8-12.
[13] 康续荣,秦育阳,魏匡民,等.基于广义塑性理论的沥青混凝土本构模型研究及应用[J].水电能源科学,2026(4):157-161,191.
[14] 何浩祥,王峥,程时涛,等.约束混凝土受压力学性能实测及修正本构模型[J].应用基础与工程科学学报,2024,32(4):1170-1185.
[15] 赛冬拉·马学义,崔溦,江志安,等.考虑损伤效应的塑性混凝土本构模型构建及数值实现[J].水利学报,2025,56(7):920-932.
[16] 郭志禄,柴军瑞,张鹏远.考虑纤维间距效应和界面相互作用的功能梯度高掺量纤维混凝土本构模型[J/OL].工程力学,2026-04-14.https://link.cnki.net/urlid/11.2595.o3.2025101
6.0914.006.
[17] 王凯,蒋一峰,徐超.不同含水率煤体单轴压缩力学特性及损伤统计模型研究[J].岩石力学与工程学报,2018,37(5):1070-1079.
[18] 吴亮,杨旭风,梁志坚.基于近场动力学单轴压缩下宏观孔隙混凝土的损伤破裂模拟[J].混凝土,2022(9):72-77.
[19] FENG G,XIN X,XIAO C S,et al.Mechanical property deterioration characteristics and a new constitutive model for rocks subjected to freeze-thaw weathering process[J].International Journal of Rock Mechanics and Mining Sciences,2021,140:104642.
[20] LEMAITRE J.A continuous damage mechanics model for ductile fracture[J].Journal of Engineering Materials and Technology,1985,107(1):83-89.

引用本文

陈兆志,郭春志.单轴压缩下不同含水率混凝土力学特性及本构模型研究[J].混凝土与水泥制品,2026,53(5):54-60. CHEN Z Z,GUO C Z.Study on the mechanical properties and constitutive model of concrete with varying moisture contents under uniaxial compression[J].China Concrete and Cement Products,2026,53(5):54-60 (in Chinese). 


上一个: 纳米SiO2与SAP复掺对水泥水化热的影响 及BP神经网络预测研究

下一个: 基于BO-SVR-BO的机制砂除云母工艺参数优化方法

相关文件