碱激发胶凝材料配合比优化及微观机理分析

Mix proportion optimization and microscopic mechanism analysis of alkali-activated cementitious materials

浏览量:

关键词:

碳酸钠;硅酸钠;粉煤灰;碱激发胶凝材料;正交试验;凝结时间;抗压强度;干燥收缩;微观分析

Key words:

Sodium carbonate; Sodium silicate; Fly ash; Alkali-activated cementitious material; Orthogonal test; Setting time; Compressive strength; Drying shrinkage; Microanalysis

刊期:

2026年第7期

DOI:

10.19761/j.1000-4637.24110610

文章编号:

基金项目:

作者:

秦节发

单位:

华新建材集团股份有限公司,湖北 武汉430070

摘要

摘   要:为制备绿色低碳、低收缩的碱激发胶凝材料,以矿粉、粉煤灰为原材料,碳酸钠与硅酸钠为碱性激发剂,通过正交试验研究了粉煤灰掺量(A)、硅酸钠掺量(B)、碳酸钠掺量(C)对碱激发胶凝材料凝结时间、抗压强度与干燥收缩的影响,并结合水化热、XRD、SEM揭示微观作用机理。结果表明:JD1、JD2、JD4、JD5、JD7组初凝时间满足相关标准要求;各因素对碱激发胶凝材料初、终凝时间影响程度排序均为B>A>C,对3 d抗压强度影响程度排序为B>A>C,对28 d抗压强度影响程度排序为C>A>B,对90 d干燥收缩值影响程度排序为B>C>A;综合性能优选出较优配合比为A2B1C2(粉煤灰20%、硅酸钠4%、碳酸钠8%);硅酸钠激发体系的水化速率更快、第二放热峰出现时间更早,对凝结时间与3 d抗压强度作用更显著;碳酸钠激发体系后期水化更充分、结构更致密,对28 d抗压强度影响显著。该研究成果可为低收缩、高性能碱激发胶凝材料的制备与工程应用提供理论依据。

Abstract: To prepare green, low-carbon, and low-shrinkage alkali-activated cementitious materials, mineral powder and fly ash were used as raw materials, while sodium carbonate and sodium silicate as alkaline activators. Orthogonal tests were conducted to investigate the effects of fly ash content (A), sodium silicate content (B) and sodium carbonate content (C) on the setting time, compressive strength, and drying shrinkage of alkali-activated cementitious materials. Hydration heat analysis, XRD and SEM were employed to reveal the microscopic mechanism. The results show that the initial setting times of groups JD1, JD2, JD4, JD5 and JD7 meet the relevant standard requirements. The influence sensitivity ranking for initial and final setting time follows B>A>C, for the 3-day compressive strength is B>A>C, for the 28-day compressive strength is C>A>B, and for the 90-day drying shrinkage value is B>C>A. The optimal mix proportion based on comprehensive performance is A2B1C2 (fly ash 20%, sodium silicate 4%, sodium carbonate 8%). The sodium silicate-activated system exhibits a faster hydration rate and an earlier occurrence of the second exothermic peak, exerting a significant influence on the setting time and 3-day compressive strength. The sodium carbonate-activated system presents more sufficient later hydration and a denser microstructure, showing a remarkable effect on the 28-day compressive strength. The research findings can provide a theoretical basis for the preparation and engineering application of high-performance and low-shrinkage alkali-activated cementitious materials.

结论

(1)凝结时间方面,随着粉煤灰、硅酸钠、碳酸钠掺量的增加,碱激发胶凝材料初、终凝时间整体呈缩短趋势,各因素对初、终凝时间影响程度的高低顺序均为:B>A>C。JD1、JD2、JD4、JD5、JD7组初凝时间满足相关标准要求。
(2)抗压强度方面,随着硅酸钠、碳酸钠掺量增加,碱激发胶凝材料3 d、28 d抗压强度均有所提高;随粉煤灰掺量增加,3 d抗压强度持续降低,28 d抗压强度先小幅上升后下降。各因素对3 d抗压强度影响程度的排序为B>A>C,对28 d抗压强度影响程度的排序为C>A>B。
(3)干燥收缩方面,碱激发胶凝材料收缩主要发生在早期,中后期收缩趋于平缓。随着粉煤灰掺量的增加,90 d干燥收缩值先增大后减小;随着硅酸钠、碳酸钠掺量的增加,90 d干燥收缩值持续增大,各因素对90 d干燥收缩值影响程度的排序为 B>C>A。
(4)综合施工可行性、力学性能与体积稳定性,确定A2B1C2(粉煤灰20%、硅酸钠4%、碳酸钠8%)为较优配合比;若工程对强度要求更高,且对干燥收缩要求可适当放宽,可选用A2B2C3(粉煤灰20%、硅酸钠8%、碳酸钠12%)作为备选配合比。
(5)水化速率、水化产物与微观结构差异是2种碱性激发剂对碱激发胶凝材料宏观性能影响程度不同的内在机制。碳酸钠组早期水化放热更快、第一放热峰更高,水化前20 h内总水化放热量更高;硅酸钠组第二放热峰出现更早、峰值更高,20~60 h总水化放热量反超碳酸钠组,60 h后两组放热速率均趋于平缓。碳酸钠激发体系水化产物更细腻、结构更致密、微裂纹更少;硅酸钠激发体系早期蜂窝状产物较多,微裂纹相对较多。

参考文献

[1] Shi Caijun,Jimenez F A,Palomo A.New cements for the 21st century: The pursuit of an alternative to Portland cement[J].Cement and Concrete Research,2011,41(7):750-763.
[2] Shi Caijun,Roy D,Krivenko P.Alkali-activated cements and concretes[M].London:CRC Press,2003.
[3] Huang Muyang,Bao Shenxu,Zhang Yimin,et al.Durability of alkali-activated cementitious materials at freeze-thaw environment: Damage and protection mechanism [J].Construction and Building Materials,2025,488:142102. 
[4] Kan Lili,Chen Hongran,Gan Yuanqiao.Synergistic activation of high ductility slag-based geopolymer composite using red mud and NaOH-Na2SiO3 mixture[J].Construction and Building Materials,2025,491:142739.
[5] Mishra J,Soren S,Nanda B,et al.Compressive strength and durability analysis of geopolymer concrete manufactured with rice husk ash-derived alkaline activator[J].Journal of Material Cycles and Waste Management,2025,27(6):1-15.
[6] Azar P,Patapy C,Samson G,et al.Effect of natural and accelerated carbonation on microstructure and pH of sodium carbonate alkali-activated slag[J].Cement and Concrete Research,2024,181:107525.
[7] Azar P,Samson G,Patapy C,et al.Durability of sodium carbonate alkali-activated slag concrete assessed by a performance-based approach[J].Construction and Building Materials,2024,423:135873.
[8] Chen Haiming,Chen Xiang,Tan Weibo,et al.Durability performance of waste glass powder and calcium oxide added sodium carbonate-activated slag mortar[J].Materials Today Communications,2023,36:106472.
[9] Li Yongde,Sun Yao.Preliminary study on combined-alkali-slag paste materials[J].Cement and Concrete Research,2000,30(6):963-966. 
[10] Kovtum M,Kearsley E P,Shekhovtssova J.Chemical acceleration of a neutral granulated blast-furnace slag activated by sodium carbonate[J].Cement and Concrete Research,2015,72:1-9.
[11] You Nanqiao,Chen Zhenzhong,Gao Zhihai,et al.The effect of copper slag as a precursor on the mechanical properties, shrinkage and pore structure of alkali-activated slag-copper slag mortar[J].Journal of Building Engineering,2024,98:111151.
[12] 何娟,杨长辉,康苏芳.碱-矿渣水泥缓凝问题的研究进展[J].硅酸盐通报,2010,29(5):1093-1097.
[13] 刘志勇,蒋金洋,李洋,等.聚丙烯酸乳液改性碱激发矿渣修补材料的力学耐久性能和作用机理[J].硅酸盐学报,2024,52(2):498-512.
[14] Thomas R,Lezama D,Peethamparan S.On drying shrinkage in alkali-activated concrete:Improving dimensional stability by aging or heat-curing[J].Cement and Concrete Research,2017,91:13-23.
[15] Yang Liangyan,Jia Zhijian,Zhang Yamei,et al.Effect of nano-TiO2 on strength,shrinkage and microstructure of alkali activated slag pastes[J].Cement and Concrete Composites,2015,57:1-7.
[16] Melo A,Cincotto M,Repette W.Drying and autogenous shrinkage of pastes and mortars with activated slag cement[J].Cement and Concrete Research,2008,38(4):565-574.
[17] 彭玉清,郭荣鑫,林志伟,等.粉煤灰-矿渣基地聚合物砂浆的凝结时间及力学性能试验研究[J].新型建筑材料,2021,48(12):138-144.
[18] 王爱国,王小尧,孙道胜,等.地质聚合物凝结硬化及其调节技术的研究进展[J].材料导报.2021,35(13):5-14.
[19] 王新.碳酸钠对碱激发水泥性能的影响研究[D].重庆:重庆大学,2016.
[20] Paillard C,Sanson N,Lacaillerie D D B J,et al.An experimental review of the reaction paths followed by alkali-activated slag pastes[J].Cement and Concrete Research,2025,189:107765.

引用本文

秦节发.碱激发胶凝材料配合比优化及微观机理分析[J].混凝土与水泥制品,2026,53(7):126-133. Qin Jiefa.Mix proportion optimization and microscopic mechanism analysis of alkali-activated cementitious materials[J].China Concrete and Cement Products,2026,53(7):126-133 (in Chinese). 


上一个: 粉煤灰微珠轻质混凝土力学与热工性能研究

下一个: 钢骨增强轻质混凝土复合外墙挂板的力学性能试验研究与数值分析