碱激发全固废胶凝材料力学与干燥收缩性能研究
Study on mechanical properties and drying shrinkage of alkali-activated all-solid-waste cementitious materials
关键词:
磷尾矿;矿渣;硅灰;碱激发全固废胶凝材料;水胶比;抗压强度;干燥收缩;微观结构
Key words:
Phosphorus tailing; Slag; Silica fume; Alkali-activated all-solid-waste cementitious material; Water-binder ratio; Compressive strength; Drying shrinkage; Microstructure
刊期:
2026年第8期
DOI:
10.19761/j.1000-4637.26040132
文章编号:
基金项目:
中铁十八局集团建筑安装工程有限公司2025年度科技发展计划项目(CR18GJA-KJ09X-2025)。
作者:
杨大伟
单位:
中铁十八局集团建筑安装工程有限公司,天津 300450
摘要
摘 要:针对磷尾矿堆存造成的环境与资源利用问题,为推进大宗固废资源化利用与低碳胶凝材料研发,本文以磷尾矿、矿渣、硅灰为复合原材料制备碱激发全固废胶凝材料,系统研究了水胶比、碱性激发剂模数、碱当量及胶凝组分比例对该材料抗压强度与干燥收缩的影响,并进行了微观分析。结果表明:随着水胶比的增大,碱激发全固废胶凝材料各龄期抗压强度降低,干燥收缩值增大;随着碱性激发剂模数与碱当量的升高,碱激发全固废胶凝材料各龄期抗压强度均先增后降,干燥收缩值增大;增大磷尾矿占比、减小矿渣占比会导致碱激发全固废胶凝材料抗压强度下降,干燥收缩值增大;适量掺入硅灰可提升碱激发全固废胶凝材料各龄期抗压强度,但掺量过大会导致抗压强度回缩,加剧干燥收缩;兼顾固废消纳量、力学性能与体积稳定性,碱激发全固废胶凝材料的最优配合比为水胶比0.30,碱性激发剂模数1.3,碱当量5%,m磷尾矿∶m矿渣∶m硅灰=65∶30∶5;适宜的碱当量能够有效激发矿物组分,水化凝胶连续均匀,基体密实度高,但当碱当量过高时,水化产物包裹固相颗粒,阻碍原材料进一步解聚,基体密实度降低。研究成果可为实现磷尾矿资源化利用及碱激发全固废胶凝材料性能优化提供参考。
Aiming at the environmental problems and low resource utilization caused by accumulated phosphorus tailings, this study develops low-carbon cementitious materials and promotes the resource recovery of bulk solid wastes. Alkali-activated all-solid-waste cementitious materials were prepared using phosphorus tailings, slag and silica fume as composite raw materials. The effects of water-binder ratio, modulus of alkali activator, alkali equivalent and cementitious components ratio on compressive strength and drying shrinkage were systematically investigated, combined with microscopic characterizations. The results show that increasing the water-binder ratio of alkali-activated all-solid-waste cementitious materials reduces the compressive strength at all curing ages and raises drying shrinkage value. With the rise of modulus of alkali activator and alkali equivalent, the compressive strengths of alkali-activated all-solid-waste cementitious materials first increase and then decrease at all ages, while the drying shrinkage value increases. Increasing the ratio of phosphorus tailings and decreasing the ratio of slag leads to a decrease in the compressive strength of alkali-activated all-solid-waste cementitious materials and an increase in drying shrinkage value. Moderate addition of silica fume improves mechanical properties, whereas excessive silica fume leads to strength regression and aggravated shrinkage. Considering solid waste consumption, mechanical performance and volume stability, the optimal mix proportion of alkali-activated all-solid-waste cementitious materials is determined as follows: water-binder ratio of 0.30, modulus of alkali activator of 1.3, alkali equivalent of 5%, mphosphorus tailings∶mslag∶msilica fume = 65∶30∶5. Appropriate alkali equivalent can effectively activate mineral phases and form continuous hydration gels, resulting in a highly dense matrix, whereas excess alkali will form a coating layer on solid particles, restrain further mineral depolymerization and reduce matrix compactness. The research can provide experimental support for high-value utilization of phosphorus tailings and performance optimization of alkali-activated all-solid-waste cementitious materials.
结论
(1)水胶比对碱激发全固废胶凝材料力学性能与体积稳定性影响显著。随着水胶比的提高,碱激发全固废胶凝材料各龄期抗压强度持续下降,干燥收缩值不断增大。
(2)随着碱性激发剂模数与碱当量的升高,碱激发全固废胶凝材料各龄期抗压强度均先增后降,干燥收缩值均持续增大。
(3)增大磷尾矿占比、减小矿渣占比会导致碱激发全固废胶凝材料抗压强度下降,干燥收缩值增大;适量掺入硅灰可提升抗压强度,但硅灰掺量过大会导致抗压强度回缩,加剧干燥收缩。
(4)适宜的碱当量能够有效激发矿物组分,消耗活性SiO2,水化凝胶连续均匀,基体孔隙少、结构致密;当碱当量过高时,水化产物包裹固相颗粒,阻碍原材料进一步解聚,基体出现结构缺陷。
(5)综合考虑固废资源化利用率、力学性能与体积稳定性,碱激发全固废胶凝材料的最优配合比为水胶比0.30,碱性激发剂模数1.3,碱当量5%,m磷尾矿∶m矿渣∶m硅灰=65∶30∶5。
参考文献
[1] 林升鉴,饶峰,郑艳金,等.磷尾矿、磷石膏和黄磷渣的地质聚合反应资源化利用研究进展[J].矿产保护与利用,2021,41(4):150-156.
[2] 秦玲,杨俊翼,孙建伟,等.碱激发煤矸石-矿渣胶凝材料的制备及性能[J].复合材料学报,2026,43(2):1008-1021.
[3] 张远永,张随雨,刘远,等.反浮选磷尾矿基地聚物的制备及其水化机制研究[J].无机盐工业,2026,58(4):114-120.
[4] Liu Xinyu,Liu Xiaoming,Zhang Zengqi,et al.Investigation of the pozzolanic activity improvement of yellow phosphorus slag with thermal activation[J].Materials,2023,16(17):6047.
[5] Yong C L,Kim H M,Suhana K.Phosphorus slag in supplementary cementitious and alkali activated materials: A review on activation methods[J].Construction and Building Materials,2022,352:129028
[6] Wang Jianbin,Sun Mingjing,Li Jing,et al.Effect of phosphate slag on the properties of silicate cement mortars[J].Journal of Materials in Civil Engineering,2025,37(7):04025027.
[7] Chen Xia,Zeng Li,Fang Kunhe.Anti-crack performance of phosphorus slag concrete[J].Construction and Building Materials,2023,395:132308.
[8] Liu Leping,Xu Yue,Liu Hainan,et al.Drying shrinkage and microstructure of alkali-activated slag with different mixing time at low temperatures (-5 to 5 ℃)[J].Construction and Building Materials,2022,360:129529.
[9] Zhang Siyi,Zhang Zhihong,Guo Lijie,et al.Synergistic effects of RHA, UFA, and GGBS on alkali-activated grouting materials[J].Journal of Materials in Civil Engineering,2025,38(3):04025027.
[10] Alassane C,Jean-Yves N K T,Desmond E P K,et al.Foam concrete with mineral additives: from microstructure to mechanical/physical properties, workability and durability[J].Open Ceramics,2025,23:100812.
[11] Nobre J,Ahmed H,Bravo M,et al.Magnesia (MgO) production and characterization, and its influence on the performance of cementitious materials:A review[J].Materials,2021,13(21):4752.
[12] Ruan S,Unluer C.Influence of supplementary cementitious materials on the performance and environmental impacts of reactive magnesia cement concrete[J].Journal of Cleaner Production,2022,359:132129.
[13] Dung N T,Hay R,Lesimple A,et al.Influence of CO2 concentration on the performance of MgO cement mixes[J].Cement and Concrete Composites,2021,115:103826.
[14] Unluer C,Al-Tabbaa A.Enhancing the carbonation of MgO cement porous blocks through improved curing conditions[J].Cement and Concrete Research,2024,156:107899.
[15] Nambiar E K,Ramamurthy K.Influence of filler type on properties of foam concrete[J].Cement and Concrete Composites,2022,133:104727.
[16] Sun Xiaowei,Gao Miao,Zhou Honghong,et al.Influence of fiber on properties of graphite tailings foam concrete[J].Lecture Notes in Civil Engineering,2022,213:508-515.
[17] Fatemeh O,Reza N.Effect of diatomite and silica fume as silica sources on compressive strength and shrinkage percentage of fly ash–based geopolymer[J].Journal of Materials in Civil Engineering,2025,38(3):20652.
[18] He Yuecheng,Jian Yue,Huang Qian,et al.Treatment of high-concentration phosphorus wastewater based on foamed concrete[J].Journal of Environmental Science and Health, Part A: Toxic/Hazardous Substances and Environmental Engineering,2022,57(6):479-486.
[19] 付明明,王梦瑶,刘亚楠,等.赤泥-偏高岭土-硅灰-水泥-脱硫石膏多元堵漏风材料的制备及性能[J].煤炭学报,2025,50(增刊1):407-417.
[20] Ma Binhui,Li Yuqi,Lan Tian,et al.Hydration mechanism and mechanical properties of slag-phosphogypsum solid waste-based cementitious composite incorporated silica fume[J].Construction and Building Materials,2025,485:141923.
引用本文
杨大伟.碱激发全固废胶凝材料力学与干燥收缩性能研究[J].混凝土与水泥制品,2026,53(8):90-95,100. Yang Dawei.Study on mechanical properties and drying shrinkage of alkali-activated all-solid-waste cementitious materials[J].China Concrete and Cement Products,2026,53(8):90-95,100 (in Chinese).
上一个: 氮气膨胀剂对碱激发矿渣胶凝材料工作性、收缩与力学性能的影响
下一个: 物理发泡矿渣-粉煤灰基地聚物地热井保温复合材料的制备及性能研究
相关文件