煅烧活化油页岩渣水化特性及其作为水泥混合材的应用研究

Hydration characteristics of calcined oil shale residue and its application as cement admixture

浏览量:

关键词:

油页岩渣(OSR);煅烧活化;火山灰质混合材料;火山灰水泥;复合水泥;活性指数;固废资源化

Key words:

Oil shale residue (OSR); Calcination activation; Pozzolanic material; Pozzolanic cement; Composite cement; Activity index; Solid waste resource utilization

刊期:

2026年第10期

DOI:

10.19761/j.1000-4637.25100447

文章编号:

基金项目:

辽宁省重点研发计划项目(102800029)。

作者:

刘小敏1,伍思则1,2,*,孙其星1,蒋建国2,钱若滢1

单位:

1.辽宁贝泽能源有限公司,辽宁 朝阳 122000;2.清华大学,北京 100084

摘要

摘   要:油页岩渣(Oil shale residue,OSR)是油页岩干馏提油过程产生的固废,存在资源化利用率低、处置方式粗放等问题,有一定环境风险。为实现OSR高值资源化利用,本文采用600 ℃煅烧工艺对OSR进行了活化改性,探究了煅烧活化对OSR物相组成、火山灰性、活性指数、水化特性的影响,并研究了大掺量煅烧活化油页岩渣(Calcined oil shale residue,COSR)单掺制备火山灰水泥、以及与矿渣-粉煤灰复掺制备复合水泥的可行性。结果表明:煅烧处理可破坏OSR中伊利石、碳酸盐等矿物结构,生成大量无定形硅铝活性组分,显著提升其活性,COSR的28 d活性指数可达105%,且各项性能指标均满足火山灰质混合材料相关标准要求;单掺25%~35% COSR可制备强度等级P·P 42.5R火山灰水泥,40%高掺量COSR配制的火山灰水泥仍可满足P·P 32.5R强度等级;COSR与矿渣、粉煤灰复掺可形成协同增强效应,改善单掺大掺量COSR水泥早期强度偏低的问题,30%COSR、35%COSR复掺体系可分别制备P·C 42.5R、P·C 42.5级复合水泥;600 ℃煅烧改性可有效提升OSR活性,将大掺量COSR应用于水泥制备具备良好技术可行性。研究成果可为油页岩固废规模化、低碳化、资源化利用与低碳水泥研发提供参考。

Abstract: Oil shale residue (OSR) is a solid waste generated during the dry-distillation process for extracting oil from oil shale. It suffers from low resource utilization rate and rough disposal, posing certain environmental risks. To achieve high-value resource utilization of OSR, this study activated OSR via calcination at 600 °C. The effects of calcination activation on the phase composition, pozzolanicity, activity index and hydration behavior of OSR were investigated, and the feasibility of preparing pozzolanic cement with high-content calcined oil shale residue (COSR) as a single admixture, as well as composite cement by co-blending COSR with slag and fly ash, was examined. The results show that calcination breaks the mineral structures of illite and carbonates in OSR and produces abundant amorphous reactive silica-alumina components, which markedly improve its reactivity. The 28-day activity index of COSR reaches 105%, and all performance indicators meet the relevant standards for pozzolanic blended materials. Pozzolanic cement of grade P·P 42.5R can be produced by individually incorporating 25%~35% COSR, and pozzolanic cement formulated with a high COSR content of 40% still satisfies the requirement for grade P·P 32.5R. Co-blending COSR with slag and fly ash yields a synergistic strengthening effect and mitigates the low early strength of cement containing high-content single COSR. The blends with 30% COSR and 35% COSR can produce composite cement of grades P·C 42.5R and P·C 42.5, respectively. Modification via calcination at 600 ℃ effectively enhances the reactivity of OSR, and the use of high-content COSR in cement production exhibits favorable technical feasibility. The research findings provide reference for large-scale, low-carbon resource utilization of oil shale solid waste and the development of low-carbon cement.

结论

(1)煅烧处理能够破坏OSR中伊利石、碳酸盐等矿物结构,生成无定形硅铝氧化物及活性钙镁水化组分,使COSR具备合格火山灰性,提升其水化活性,其28 d活性指数达105%。COSR掺入水泥不会改变水化产物种类,可有效消耗Ca(OH)2,促进熟料进一步水化,优化浆体微观结构。同时,COSR各项性能指标均符合相关标准要求,可作为火山灰质混合材料使用。
(2)大掺量COSR可制备性能合格的火山灰水泥。25%、30%、35%COSR掺量的火山灰水泥均满足P·P 42.5R强度等级;40%高掺量COSR会导致水泥早期强度降低,但对应的火山灰水泥仍满足P·P 32.5R强度等级。所有火山灰水泥的凝结时间、安定性、细度、SO3、MgO和Cl-含量均符合相关标准要求。
(3)COSR与矿渣、粉煤灰可发挥多组分协同效应,提升复合水泥后期力学性能。30%COSR+8%矿渣+2%粉煤灰复配体系制备的复合水泥满足P·C 42.5R强度等级,35%COSR+13%矿渣+2%粉煤灰复配体系制备的复合水泥满足P·C 42.5强度等级。
(4)本研究证实600 ℃煅烧可有效改性OSR,大掺量COSR单掺、复掺均可制备符合相关标准、不同强度等级的水泥,具备良好的工程应用潜力。但研究仅聚焦材料活性与水泥基本力学性能,存在一定局限性。后续可重点探究大掺量COSR水泥的长期耐久性能,同时开展碳减排效益与经济效益分析,为固废资源化利用及水泥低碳化发展提供参考。

参考文献

[1] 马玲,尹秀英,孙昊,等.世界油页岩资源开发利用现状与发展前景[J].世界地质,2012,31(4):772-777.
[2] 马跃,向卿谊,丁康乐.国内外油页岩工业发展现状[J].世界石油工业,2024,31(1):16-25.
[3] 张荣华,苟余江,关素敏.电石渣低碳混凝土的制备及其性能研究[J].混凝土与水泥制品,2026(1):76-80.
[4] 胡忠帅,杨勇,王永康,等.固废基泡沫混凝土的研究现状及性能优化研究进展[J].混凝土与水泥制品,2025(9):97-100.
[5] 刘远祥,杨婷丽,张华献,等.低碳复合胶凝材料对水泥和混凝土性能的影响[J].混凝土与水泥制品,2024(7):89-93,102.
[6] Li Xiaohui,Zhang Weifeng,Ma Huiqiang,et al.Enhancement mechanism of early age strength in cement paste induced by oil shale residue[J].Construction and Building Materials,2025,465:140277.
[7] Yan Yulin,Zhang Weifeng,Li Xiaohui,et al.Utilization of oil shale residue from Alberta Taciuk process in phosphogypsum slag cement: compressive strength, hydration behavior, and microstructural characteristics[J].Journal of Building Engineering,2025,107:112771.
[8] 权长青,焦楚杰,杨云英,等.油页岩渣对混凝土抗压强度和抗氯离子侵蚀的影响[J].材料导报,2021,35(22):22079-22084.
[9] Wang Yunyi,Zeng Cong,Wang Yingshuai,et al.Study on the durability of high-content oil shale concrete[J].Buildings,2024,14(8):14082547.
[10] Wang Zihao,Wang Boxin.Experimental and numerical study on compressive failure mechanism of concrete with oil shale residue as a replacement for coarse aggregate[J].Construction and Building Materials,2025,504:144599.
[11] Shi Chenglin,Shi Zijian.Investigation on the properties of concrete containing oil shale waste ash as a substitute for cement[J].Advances in Civil Engineering,2022,2022:4024270.
[12] 陈立军,孔令炜,黄德馨,等.油页岩渣-矿渣碱胶凝材料的研究[J].建筑材料学报,2010,13(6):841-846.
[13] 张延年.油页岩灰渣基多固废碱激发胶凝材料水化特性研究[D].辽宁:沈阳建筑大学,2023.
[14] Luo Chenchen,Zheng Bo,Li Yi,et al.Preparation of alkali-activated oil shale residue-slag geopolymer-based binder using calcium carbide slag and sodium carbonate as alkali activator[J].PloS One,2025,20(1):0317341.
[15] Ling Hao,Li Xilin,Wang Dayin,et al.Acid reduction and corrosion resistance of alkaline full solid waste backfill based on oil shale residue[J].Environmental Research,2025,273:121216.
[16] Chen Xiang,Zhang Siqi,Liu Yuhang,et al.Effect of clinker/Ca(OH)2 external blending on the hydration mechanism of oil shale ash-MSWI FA based cementitious material[J].Process Safety and Environmental Protection,2025,199:107269.
[17] Zhao Xiaosheng,Wang Hongru,Wang Yulu,et al.An oil shale ash-based X-type zeolite with rapid and high-capacity Cd2+ adsorption[J].Materials Letters,2025,394:138601.
[18] Bai Shuxia,Chang Zhibin,Ren Zhengchun,et al.Adsorption of Cd2+ ions onto zeolites synthesized from a mixture of coal fly ash and oil shale ash in aqueous media[J].RSC Advances,2025,15(15):11293-11300.
[19] Xie Rui,Liu Shi,Wang Zhonghuai,et al.Effect of MnO2 content on properties of oil shale residue ceramsite[J].Journal of Physics: Conference Series,2025,2954(1):012018.
[20] Li Yongtao,Liu Geying,Ai Weidong,et al.High-quality glass-ceramics from oil shale ash and phosphorus slag for architectural decoration application:Preparation, characterization and heavy metals immobilization[J].Ceramics International,2025,51(18PB):26799-26810.
[21] GB/T 2847—2022 用于水泥中的火山灰质混合材料[S].
[22] GB 175—2023 通用硅酸盐水泥[S].
[23] 曹万智,韩广兴,叶骐瑞,等.碱激发矿渣粉-粉煤灰-废玻璃粉基泡沫混凝土性能研究[J].混凝土与水泥制品,2025(8):77-81,86.
[24] 顾晓薇,艾莹莹,孙维.改性油页岩渣-粉煤灰二元复掺的水化特征[J].科学技术与工程,2022,22(34):15277-15283.
[25] 刘敏,李酽,元敬顺,等.不同煅烧温度对页岩作为水泥掺合料活性影响的研究[J].硅酸盐通报,2014,33(10):2620-2625.
[26] Liu Xiaomin,Long Yu,Wu Qingyong,et al.Preparation and performance of AACM with red mud and GGBFS: Effectiveness of alkali activator[J].Materials and Structures,2023(56):1-14.
[27] 王冲,刘勇兵,曹占义,等.白云石煅烧组织的转变过程[J].材料热处理学报,2013,34(2):23-26.
[28] 孙斌.油页岩矿物质分解特性研究[D].吉林:东北电力大学,2013.
[29] 王栋民,房奎圳.煤矸石资源化利用技术[M].北京:中国建材工业出版社,2021.
[30] 刘志强,王越,杨斌,等.电石渣激发矿渣-尾矿粉复合固废基胶凝材料性能试验研究[J].混凝土与水泥制品,2025(9):93-96.

引用本文

刘小敏,伍思则,孙其星,等.煅烧活化油页岩渣水化特性及其作为水泥混合材的应用研究[J].混凝土与水泥制品,2026,53(10):27-32. Liu Xiaomin,Wu Size,Sun Qixing,et al.Hydration characteristics of calcined oil shale residue and its application as cement admixture[J].China Concrete and Cement Products,2026,53(10):27-32 (in Chinese). 


上一个: 活化白云石粉改性纤维增强水泥基复合材料强度及变形性能的研究

下一个: 石英粉与粉煤灰对砂浆性能、水化特性与碳排放的影响

相关文件