全部文章

碱激发材料与地聚物

童 胜1,王成云1,胡爽子1,王 莹2,翟鹏昊3,徐 方3,*

摘   要:设计制备了不同水固比(0.28~0.42)地质聚合物泡沫混凝土,分析了不同流变性能料浆中泡沫的受力性能和气孔结构特征,揭示了地质聚合物泡沫混凝土的成孔机理。结果表明:随着水固比的增加,净浆的初始和最终极限剪切应力均减小;泡沫在浆体内主要受到浆体黏滞产生的挤压力、浆体流动产生的浮力、泡沫液膜泌水产生的泌水力和泡沫与浆体之间的摩擦力作用;随着净浆极限剪切应力的减小,地质聚合物泡沫混凝土的孔径分层现象加剧,各层的泡沫平均Feret直径和孔隙率差异越来越大。Abstract: Geopolymer foamed concrete with different water-solid ratio(0.28~0.42) was designed and prepared. The mechanical properties and pore structure characteristics of foam in slurry with various rheological properties were analyzed, and the pore forming mechanism of geopolymer foamed concrete was revealed. The results indicate that as the water-solid ratio increases, the initial ultimate shear stress and final ultimate shear stress of the slurry decrease. The foam in the slurry is mainly affected by the squeezing force generated by the slurry viscosity, the buoyancy generated by the slurry flow, the bleeding generated by the bleeding of the foam liquid film, and the friction between the foam and the slurry. With the decrease of the ultimate shear stress of slurry, the pore size stratification of geopolymer foamed concrete intensifies, and the average Feret diameter of foam and porosity in each layer are more and more different.
童胜,王成云,胡爽子,等.料浆流变性能对地质聚合物泡沫混凝土成孔机理的影响[J].混凝土与水泥制品,2025(8):95-99. TONG S,WANG C Y,HU S Z,et al.Influence of rheological property of slurry on pore forming mechanism of geopolymer foamed concrete[J].China Concrete and Cement Products,2025(8):95-99.
摘   要:介绍了不同地区锂渣粉的性能差异,综述了其对混凝土力学性能的影响规律及其活性激发方式(物理激发、化学激发、高温激发),总结了其在混凝土中的作用机理(火山灰效应、填充效应、成核效应),指出了当前研究存在的不足,并对未来发展前景进行了展望。Abstract: The performance differences of lithium slag powder in different regions are introduced, and its effect on the mechanical properties of concrete and the activity activation modes (physical activation, chemical activation, high-temperature activation) are overviewed. The action mechanism of lithium slag powder in concrete(pozzolanic effect, filling effect, nucleation effect) is summarized, the shortcomings of the current research are pointed out, and the prospects for future development are outlooked.
范泽辉,杨隽.锂渣粉对混凝土力学性能影响研究进展[J].混凝土与水泥制品,2025(8):91-94. FAN Z H,YANG J.Research progress on the effect of lithium slag powder on the mechanical properties of concrete[J].China Concrete and Cement Products,2025(8):91-94.

梁海波1,姜迎春1,魏兆赫1,毛启松1,岳公冰2,刘 程2,*

摘   要:设计制备了不同强度等级(C30、C40、C50)的碱激发再生混凝土,研究了其抗硫酸侵蚀性能,并通过显微硬度试验揭示了其损伤机制。结果表明:随着干湿循环次数的增加,试件的抗压强度耐蚀系数先略微增大后减小;硫酸盐侵蚀会劣化混凝土的微观结构,导致骨料-新砂浆、新-旧砂浆界面的界面过渡区(ITZ)显微硬度降低,ITZ宽度增大;提高混凝土强度等级可在一定程度上改善混凝土的微观结构,提升抗硫酸盐侵蚀性能。Abstract: The alkali-activated recycled concrete with different strength grades (C30, C40, C50) was designed and prepared, and its resistance to sulfate attack was studied. The damage mechanism was revealed through microhardness testing. The results show that with the increase of wet-dry cycles, the corrosion resistance coefficient of compressive strength for the specimens first slightly increases and then decreases. Sulfate attack can degrade the microstructure of concrete, leading to a decrease in microhardness of interfacial transition zone(ITZ) and an increase in ITZ width between aggregate and new mortar, and new mortar and old mortar. Improving the strength grade of concrete can enhance the microstructure and improve the resistance to sulfate attack to some extent.
梁海波,姜迎春,魏兆赫,等.硫酸盐侵蚀环境下碱激发再生混凝土的ITZ显微硬度分析[J].混凝土与水泥制品,2025(8):87-90. LIANG H B,JIANG Y C,WEI Z H,et al.Analysis of ITZ microhardness of alkali-activated recycled concrete under sulfate attack environment[J].China Concrete and Cement Products,2025(8):87-90.

唐兴滨1,陈 强1,单体庆2,刘海滨1,岳公冰3,王鑫焱3,*

摘   要:设计制备了碱激发再生混凝土路缘石,研究了混凝土强度等级、粉煤灰、再生粗骨料对其力学性能、吸水率、抗冻性能、抗盐冻性能和外观质量的影响。结果表明:碱激发再生混凝土路缘石的强度、吸水率、质量损失率、抗盐冻质量损失和外观质量均满足相关标准要求;随着混凝土强度等级的增加,碱激发混凝土路缘石的抗压、抗折强度增大,吸水率、质量损失率和抗盐冻质量损失基本呈减小趋势;粉煤灰的掺入对碱激发混凝土的力学性能影响不大,但会降低抗冻及抗盐冻性能,并增大吸水率;与碱激发天然混凝土相比,碱激发再生混凝土的性能略差。Abstract: The alkali activated recycled concrete curbs were designed and prepared, and the effects of concrete strength grade, fly ash, and recycled coarse aggregate on the mechanical properties, water absorption rate, frost resistance, salt frost resistance, and appearance quality were studied. The results indicate that the strength, water absorption rate, mass loss rate, mass loss of salt frost resistance, and appearance quality of alkali activated recycled concrete curbs all meet the requirements of relevant standard. As the concrete strength grade increases, the compressive strength and flexural strength of the alkali activated concrete curbs increase, while the water absorption rate, mass loss rate, and mass loss of salt frost resistance generally decrease. The addition of fly ash has little effect on the mechanical properties of alkali activated concrete, but it will reduce the frost resistance and salt frost resistance, and increase the water absorption rate. Compared with alkali activated natural concrete, the performance of alkali activated recycled concrete is relatively inferior.
唐兴滨,陈强,单体庆,等.碱激发再生混凝土路缘石的配合比设计及性能研究[J].混凝土与水泥制品,2025(8):82-86. TANG X B,CHEN Q,SHAN T Q,et al.Mix proportion design and performance study of alkali activated recycled concrete curbs[J].China Concrete and Cement Products,2025(8):82-86.

曹万智1,2,韩广兴1,叶骐瑞1,陈炳旭1,郭浩翔1

摘   要:研究了废玻璃粉掺量(0、10%、20%、30%、40%、50%,等质量取代粉煤灰)对碱激发矿渣粉-粉煤灰-废玻璃粉基泡沫混凝土流动度、凝结时间、抗压强度、吸水率、导热系数的影响,并进行了微观分析。结果表明:随着废玻璃粉掺量的增加,碱激发矿渣粉-粉煤灰-废玻璃粉基泡沫混凝土的流动度和凝结时间均先增后降再增,吸水率先减后增,7 d、28 d抗压强度和导热系数均先增后降;掺入适量废玻璃粉有效促进了体系水化程度,提高了水化产物生成量,减少了孔隙,改善了基体密实度;考虑碱激发矿渣粉-粉煤灰-废玻璃粉基泡沫混凝土的综合性能,推荐废玻璃粉最佳掺量为30%。Abstract: The effects of waste glass powder content(0, 10%, 20%, 30%, 40%, 50%,replacing fly ash by equal mass) on the fluidity, setting time, compressive strength, water absorption rate and thermal conductivity of alkali-activated slag powder-fly ash-waste glass powder-based foamed concrete were investigated,and microanalysis was conducted. The results show that, with the increase of waste glass powder content, the fluidity and setting time of alkali-activated slag powder-fly ash-waste glass powder-based foamed concrete first increase, then decrease and finally increase, the water absorption rate first decreases and then increases, the 7 d and 28 d compressive strength and thermal conductivity all first increase and then decrease. Adding an appropriate content of waste glass powder can effectively promote the hydration degree of the system, increase the amount of hydration products, reduce pores, and improve the matrix compactness. Considering the comprehensive performance of alkali-activated slag powder-fly ash-waste glass powder-based foamed concrete, the recommended optimal content of waste glass powder is 30%.
曹万智,韩广兴,叶骐瑞,等.碱激发矿渣粉-粉煤灰-废玻璃粉基泡沫混凝土性能研究[J].混凝土与水泥制品,2025(8):77-81,86. CAO W Z,HAN G X,YE Q R,et al.Study on the performance of alkali-activated slag powder-fly ash-waste glass powder-based foamed concrete[J].China Concrete and Cement Products,2025(8):77-81,86.