工程现场自密实混凝土配比设计研究
Research on Proportion Design of Self-compacting Concrete (SCC) in Actual Production
2015年第1期
自密实混凝土;坍落扩展度;质量控制;缓凝剂;高效减水剂
Self-compacting concrete; Slump spread; Quality control; Retarder; Super plasticizer
2015年第1期
1000-4637(2015)01-05-05
国家自然科学基金项目(51178218)
陈 浩1,2,叶燕华1,薛洲海1
1. 南京工业大学土木工程学院,210009;2. 国电南自新能源工程技术有限公司,南京 210032

陈 浩1,2,叶燕华1,薛洲海1

浏览量:
1000
摘 要:针对工程现场自密实混凝土生产时工作性能降低的问题,通过坍落扩展度、混凝土搅拌等试验探讨分析了环境温度、搅拌时间、外加剂以及原材料堆放对自密实混凝土的影响。综合考察影响因素后,通过现场配制对不满足要求的自密实混凝土提出了配比调整方案,并对自密实混凝土质量控制提出了措施。研究结果表明,温度越高自密实混凝土坍落扩展度损失越快,掺入适量的缓凝剂可以阻止坍损;搅拌时间存在一临界值,需根据现场实际情况作具体调整;自密实混凝土拌合物出现离析泌水现象时,应优先调整高效减水剂的用量;露天堆放会导致砂石含水率和含泥量发生变化,从而影响混凝土拌合物的流动性能,应实行封闭式材料管理。 Abstract: In order to solve the problems that the working performance of self-compacting concrete (SCC) decreased in actual production, the main affect factors including ambient temperature, mixing time, admixtures and raw material stacking on SCC were analyzed by slump spread test and mixing test. According to the actual situation of mixing, the adjustment aiming at working performance was raised. The measures for the quality control of SCC were put forward. The research results indicated that the slump spread would lose quickly with the increase of temperature, which could be effectively prevented by the retarder. There was a critical value of the mixing time which should be adjusted according to actual situation. The dosage of super plasticizer needed to be adjusted to avoid segregation or bleeding. Stacking of sand and stone in open-air would make water content and mud content change which influenced the fluidity of SCC. Closed material management should be implemented.
英文名 : Research on Proportion Design of Self-compacting Concrete (SCC) in Actual Production
刊期 : 2015年第1期
关键词 : 自密实混凝土;坍落扩展度;质量控制;缓凝剂;高效减水剂
Key words : Self-compacting concrete; Slump spread; Quality control; Retarder; Super plasticizer
刊期 : 2015年第1期
DOI :
文章编号 : 1000-4637(2015)01-05-05
基金项目 : 国家自然科学基金项目(51178218)
作者 : 陈 浩1,2,叶燕华1,薛洲海1
单位 : 1. 南京工业大学土木工程学院,210009;2. 国电南自新能源工程技术有限公司,南京 210032

陈 浩1,2,叶燕华1,薛洲海1

摘要
参数
结论
参考文献
引用本文

摘   要:针对工程现场自密实混凝土生产时工作性能降低的问题,通过坍落扩展度、混凝土搅拌等试验探讨分析了环境温度、搅拌时间、外加剂以及原材料堆放对自密实混凝土的影响。综合考察影响因素后,通过现场配制对不满足要求的自密实混凝土提出了配比调整方案,并对自密实混凝土质量控制提出了措施。研究结果表明,温度越高自密实混凝土坍落扩展度损失越快,掺入适量的缓凝剂可以阻止坍损;搅拌时间存在一临界值,需根据现场实际情况作具体调整;自密实混凝土拌合物出现离析泌水现象时,应优先调整高效减水剂的用量;露天堆放会导致砂石含水率和含泥量发生变化,从而影响混凝土拌合物的流动性能,应实行封闭式材料管理。

Abstract: In order to solve the problems that the working performance of self-compacting concrete (SCC) decreased in actual production, the main affect factors including ambient temperature, mixing time, admixtures and raw material stacking on SCC were analyzed by slump spread test and mixing test. According to the actual situation of mixing, the adjustment aiming at working performance was raised. The measures for the quality control of SCC were put forward. The research results indicated that the slump spread would lose quickly with the increase of temperature, which could be effectively prevented by the retarder. There was a critical value of the mixing time which should be adjusted according to actual situation. The dosage of super plasticizer needed to be adjusted to avoid segregation or bleeding. Stacking of sand and stone in open-air would make water content and mud content change which influenced the fluidity of SCC. Closed material management should be implemented.

关键词:
自密实混凝土;坍落扩展度;质量控制;缓凝剂;高效减水剂
扫二维码用手机看
未找到相应参数组,请于后台属性模板中添加
(1)周围环境温度越高,自密实混凝土坍落扩展度损失越快,在相同温度条件下,掺入缓凝剂可以有效阻止坍落扩展度损失。
(2)搅拌时间存在一临界值,拌合物在这一临界值时,和易性和流动性最佳,搅拌时间需根据现场实际情况作具体调整,夏天适当缩短拌合物搅拌时间,冬天适当延长拌合物搅拌时间。
(3)减水剂能减少拌合用水量且能够提高混凝土强度,增稠剂有助于增加拌合物的粘性并阻止拌合物离析,但是添加增稠剂的高粘度自密实混凝土拌合物内部气泡自排除比较困难,建议对配合比进行优化(调整高效减水剂用量)以避免离析,尽量减少使用增稠剂。
(4)混凝土实际生产中的砂石一般都是露天堆放,这会导致砂石的含泥量和含水率发生变化,而自密实混凝土的流动性对于砂石的含泥量和含水率极其敏感,因此,工程现场生产时,建议对砂石进行封闭式管理。
[1] 白震伟. 自密实混凝土研究与应用初探[J]. 山西建筑, 2007(13): 171-172.
[2] 郭鹏, 邓亮亮, 柳凤阳. 外加剂超掺对混凝土性能的影响[J]. 中国建材科技, 2014(2): 20-21.
[3] 朱铁梅, 叶燕华, 魏威, 等. 自密实混凝土模板侧向压力初探[J]. 混凝土, 2011(7): 14-16.
[4] 杨勇, 郭子雄, 薛建阳, 等. 型钢混凝土粘结滑移性能试验研究[J]. 建筑结构学报, 2005(4): 4-12.
[5] 叶燕华, 陈丽华, 杜艳静, 等. 高效减水剂和增黏剂对自密实混凝土性能的影响[J]. 混凝土, 2008(6): 72-75.
[6] 薛洲海. 现场自密实混凝土配比设计及叠合墙模板侧压试验研究[D]. 南京:南京工业大学,2014.
[7] 魏建立. 温度对聚羧酸系减水剂性能影响情况的研究[J]. 中国新技术新产品, 2013(3): 9-10.
[8] 陈永霞. 混凝土中水泥的水化过程及主要水化产物特性[J]. 青海交通科技, 2013(3): 7-8.
[9] 刘国栋, 关志梅, 魏春涛, 等. 砂子含泥量对掺用聚羧酸高效减水剂混凝土性能的影响及有效对策[J]. 商品混凝土, 2008(3): 20-23.
      

相关文件

暂时没有内容信息显示
请先在网站后台添加数据记录。

关注《混凝土与水泥制品》

总访问量 468,401   网站统计

官方微信公众号关闭
苏州混凝土水泥制品研究院有限公司

关于我们    |    联系我们    |    订购杂志    |    回到顶部

版权所有:中国混凝土与水泥制品网  苏ICP备10086386号   网站建设:中企动力 苏州

版权所有:中国混凝土与水泥制品网

苏ICP备10086386号

网站建设:中企动力 苏州