骨料改性技术与低碳高值化利用

胡玉娇,苏有文,文江.陶粒掺量对自密实混凝土力学及收缩性能的影响[J].混凝土与水泥制品,2025(10):70-73,79. HU Y J,SU Y W,WEN J.Influence of ceramic particle content on the mechanical and shrinkage properties of self-compacting concrete[J].China Concrete and Cement Products,2025(10):70-73,79.
摘   要:研究了单掺、复掺陶瓷球和钢纤维对橡胶混凝土抗压、劈裂抗拉、抗折性能及韧性的影响,并进行了方差和相关性分析。结果表明:单掺陶瓷球提高了橡胶混凝土的抗压、抗折性能,降低了劈裂抗拉性能;单掺钢纤维提升了橡胶混凝土的抗压、劈裂抗拉、抗折性能,且复掺陶瓷球后增强效果更显著;陶瓷球和钢纤维的协同作用显著改善了橡胶混凝土的抗变形能力,使破坏形态呈现出“裂而不散”的特征;单掺陶瓷球降低了橡胶混凝土的韧性,而单掺钢纤维或复掺陶瓷球和钢纤维均能有效提高韧性;钢纤维的掺入对橡胶混凝土抗压强度、劈裂抗拉强度和抗折强度的影响显著,陶瓷球的掺入仅对橡胶混凝土抗压强度的影响显著。Abstract: The effects of individual and compound addition of ceramic ball and steel fiber on the compressive, splitting tensile and flexural properties, and toughness of rubber concrete were investigated, and variance analysis and correlation analysis were conducted. The results show that individual addition of ceramic ball enhances the compressive and flexural properties of rubber concrete, while reducing the splitting tensile properties. The individual addition of steel fiber enhances the compressive, splitting tensile, and flexural properties of rubber concrete, with the effect more significant when compounded with ceramic ball. The synergistic effect of ceramic ball and steel fiber significantly improves the deformation resistance of rubber concrete, resulting in a damage morphology characterized by "cracking without disintegration". The individual addition of ceramic ball reduces the toughness of rubber concrete, while the individual addition of steel fiber or the compound addition of ceramic ball and steel fiber effectively improves the toughness. The incorporation of steel fiber exerts significant effect on all three mechanical properties, whereas the incorporation of ceramic ball demonstrates significant effect only on compressive strength. 
姚爱梅,邓勇军.陶瓷球和钢纤维对橡胶混凝土力学性能的影响研究[J].混凝土与水泥制品,2025(10):74-79. YAO A M,DENG Y J.Study on the effect of ceramic ball and steel fiber on the mechanical properties of rubber concrete[J].China Concrete and Cement Products,2025(10):[J].China Concrete and Cement Products,2025(10):74-79.

王丕祥1,黄俊钧1,李超颖1,刘金亮2,曾德湛1,姚锦铭1,修振宇1,*

摘   要:用纳米SiO2预浸泡法改性工艺对再生粗骨料(Recycled coarse aggregate,RCA)进行性能强化,研究了纳米SiO2分散液浓度(1%、2%、3%)与浸泡时间(24、48、72 h)对RCA性能的影响,并对比研究了天然粗骨料混凝土、未改性RCA混凝土、改性RCA混凝土的自收缩性能差异,并对RCA周边砂浆进行了微观分析。结果表明:纳米SiO2改性能有效降低RCA的吸水率和压碎指标,其效果随分散液浓度升高或浸泡时间延长而增强,其中,2%浓度浸泡48 h时对RCA性能的优化效果相对较好;附着于骨料表面的纳米SiO2与水泥水化产物Ca(OH)2反应生成了C-S-H凝胶,提升了界面过渡区密实度;未改性RCA混凝土各龄期自收缩值均高于天然粗骨料混凝土,而经纳米SiO2改性处理后的RCA混凝土自收缩效应进一步加剧,且以2%浓度纳米SiO2分散液浸泡48 h的改性工艺对混凝土自收缩产生的负面效应更显著。  Abstract: The performance of recycled coarse aggregate (RCA) was enhanced by nano- SiO2 pre-soaking modification. The effects of nano-SiO2 dispersion solution concentration (1%, 2%, 3%) and soaking time (24, 48, 72 h) on RCA performance were investigated. A comparative study was conducted on the autogenous shrinkage behavior of natural coarse aggregate concrete, unmodified RCA concrete, and modified RCA concrete, and a microscopic analysis of the surrounding mortar of RCA was performed. The results show that nano-SiO2 modification effectively reduces the water absorption rate and crushing index of RCA, with the effect intensifying as the dispersion solution concentration increases or the soaking time extends. Notably, the relative optimal enhancement in RCA performance is achieved under the condition of a 2% nano-SiO2 dispersion solution concentration with the soaking time of 48 h. The nano-SiO2 adhered to the aggregate surface reacts with cement hydration products Ca(OH)2 to form C-S-H gel, thereby enhancing the compactness of the interfacial transition zone. The autogenous shrinkage values of unmodified RCA concrete at all testing ages are higher than those of natural coarse aggregate concrete. Furthermore, the application of nano-SiO2 modification exacerbates the autogenous shrinkage effect in RCA concrete, with the most pronounced adverse impact observed in specimens treated with a 2% nano-SiO2 dispersion solution soaked for 48 h.
王丕祥,黄俊钧,李超颖,等.纳米SiO2改性再生粗骨料(RCA)的性能及其对混凝土体积稳定性的影响[J].混凝土与水泥制品,2025(10):80-84,90. WANG P X,HUANG J J,LI C Y,et al.Performance of nano-SiO2 modified recycled coarse aggregate (RCA) and its effect on concrete volume stability[J].China Concrete and Cement Products,2025(10):80-84,90.
摘   要:以部分钢渣作为粗骨料制备了钢渣混凝土,研究了钢渣掺量(等体积替代0、20%、40%、60%、80%、100%的天然粗骨料)对混凝土断裂性能的影响,得到了破坏形态、断裂能、断裂韧度等结果,分析了钢渣对混凝土断裂性能的影响机理。结果表明:钢渣的掺入影响了混凝土的断裂破坏模式,使混凝土在面临断裂时展现出了更强的抵抗能力;在混凝土掺入适量钢渣,可以提高混凝土的断裂能、断裂韧度、起裂韧度、失稳韧度;钢渣的掺入能在一定程度上提高骨料与水泥基体间的黏结强度,从而改善混凝土的断裂性能。Abstract: Steel slag concrete was prepared by using a portion of steel slag as coarse aggregates, and the effect of replacing 0, 20%, 40%, 60%, 80%, and 100% of natural coarse aggregates with equal volume of steel slag on the fracture performance of concrete was studied. The failure mode, fracture energy, fracture toughness, and other results were obtained, and the influence mechanism of steel slag on the fracture performance of concrete was analyzed. The results indicate that the addition of steel slag affects the fracture failure mode of concrete, making it exhibit stronger resistance when facing fracture. Adding an appropriate content of steel slag can improve the fracture energy, fracture toughness, initiation toughness, and instability toughness of concrete. The addition of steel slag can improve the bonding strength between aggregates and cement matrix to a certain extent, thereby enhancing the fracture performance of concrete.
摘   要:以聚乙烯醇(Polyvinyl alcohol,PVA)纤维掺量(0、0.10%、0.15%、0.20%、0.30%)和玄武岩纤维(Basalt fiber,BF)掺量(0、0.10%、0.20%)为主要变量,研究了二者的混杂方式对轻骨料混凝土(Lightweight aggregate concrete,LAC)力学性能和抗氯离子渗透性能的影响。结果表明:适量单一或混杂纤维的掺入均能提高LAC的抗氯离子渗透性能和抗压强度,混杂纤维对LAC的强化效果明显优于单掺纤维;当PVA纤维与BF的掺量分别为0.15%和0.10%时,混杂纤维增强LAC的性能达到最佳;建立的混杂纤维增强LAC的氯离子渗透深度和迁移系数计算模型具有较高精度,可用于混杂纤维增强LAC的抗氯离子渗透性能预测。Abstract: Using polyvinyl alcohol (PVA) fiber content (0, 0.10%, 0.15%, 0.20%, 0.30%) and basalt fiber (BF) content (0, 0.10%, 0.20%) as the main variables, the influence of the hybrid method of PVA fiber and BF on the mechanical properties and chloride ion penetration resistance of lightweight aggregate concrete (LAC) was studied. The results show that the addition of appropriate contents of single or hybrid fiber can improve the chloride ion penetration resistance and compressive strength of LAC, and the strengthening effect of hybrid fiber on LAC is significantly better than that of single fiber. When the content of PVA fiber and BF is 0.15% and 0.10% respectively, the performance of hybrid fiber reinforced LAC reaches its optimal level. The established models for calculating the chloride ion penetration depth and migration coefficient of hybrid fiber reinforced LAC have high accuracy and can be used to predict the chloride ion penetration resistance of hybrid fiber reinforced LAC.
张茫茫,董辉,沈伟.PVA-BF混杂纤维增强轻骨料混凝土(LAC)力学和抗氯离子渗透性能研究[J].混凝土与水泥制品,2025(10):91-96. ZHANG M M,DONG H,SHEN W.Study on mechanical properties and chloride ion penetration resistance of PVA-BF hybrid fiber reinforced lightweight aggregate concrete (LAC)[J].China Concrete and Cement Products,2025(10):91-96.

李晓东1,王 艳1,吴健波1,李建新2,3,4,*,李儒光2,5,徐 浩2,周双喜2,谢朵超2,3,5

李晓东,王艳,吴健波,等.镍铁渣的环境安全性及其对砂浆和透水混凝土性能的影响[J].混凝土与水泥制品,2025(10):97-101,106. L X D,WANG Y, WU J B,et al.Environmental safety of nickel iron slag and its impact on the performance of mortar and pervious concrete[J].China Concrete and Cement Products,2025(10):97-101,106.