废陶瓷再生砂对砂浆性能影响的研究
Effects of Waste Recycled Ceramic Mixed Sand on Properties of Mortar
2011年第7期
陶瓷再生混合砂;强度;对比试验;脆性;干缩性
Recycled ceramic mixed sand; Strength; Contrast test; Brittleness; Shrinkage
2011年第7期
1000-4637(2011)07-54-04
河南省教育厅自然科学基金资助项目(2010A560003)
张承志1,刘凤利1,刘俊华2
1. 河南大学土木建筑学院, 开封 475004; 2.开封大学土木建筑工程学院, 475004

张承志1,刘凤利1,刘俊华2

浏览量:
1000
摘 要:将废陶瓷破碎成细骨料,部分取代特细砂配成废陶瓷再生混合砂。固定稠度和胶砂比,通过试验,对比了陶瓷再生混合砂砂浆、天然中砂砂浆、特细砂砂浆和陶瓷再生粗砂砂浆的抗压强度、抗折强度和干缩性能的差异。结果表明,陶瓷再生混合砂砂浆能够达到工程应用的强度要求且后期强度较高;其相对脆性低、干缩小,有利于提高抗裂性。 Abstract : Waste ceramic is crushed as recycled ceramic coarse sand, and recycled ceramic mixed sand is made through recycled ceramic coarse sand partly replacing super-fine sand. By fixed consistence and cement-aggregate ratio, the compressive strength, flexural strength and shrinkage performance between mortar respectively made from natural medium sand, super-fine sand, recycled ceramic coarse sand and recycled ceramic mixed sand are contrasted. The results show that the mortar using recycled ceramic mixed sand as fine aggregate can achieve the project’s strength request and it has higher strength at later age. And by adding recycled ceramic coarse sand in mortar, the brittleness and shrinkage of mortar can be decreased, thus, the crack resistance of the concrete can be improved.
英文名 : Effects of Waste Recycled Ceramic Mixed Sand on Properties of Mortar
刊期 : 2011年第7期
关键词 : 陶瓷再生混合砂;强度;对比试验;脆性;干缩性
Key words : Recycled ceramic mixed sand; Strength; Contrast test; Brittleness; Shrinkage
刊期 : 2011年第7期
DOI :
文章编号 : 1000-4637(2011)07-54-04
基金项目 : 河南省教育厅自然科学基金资助项目(2010A560003)
作者 : 张承志1,刘凤利1,刘俊华2
单位 : 1. 河南大学土木建筑学院, 开封 475004; 2.开封大学土木建筑工程学院, 475004

张承志1,刘凤利1,刘俊华2

摘要
参数
结论
参考文献
引用本文

摘   要:将废陶瓷破碎成细骨料,部分取代特细砂配成废陶瓷再生混合砂。固定稠度和胶砂比,通过试验,对比了陶瓷再生混合砂砂浆、天然中砂砂浆、特细砂砂浆和陶瓷再生粗砂砂浆的抗压强度、抗折强度和干缩性能的差异。结果表明,陶瓷再生混合砂砂浆能够达到工程应用的强度要求且后期强度较高;其相对脆性低、干缩小,有利于提高抗裂性。

Abstract : Waste ceramic is crushed as recycled ceramic coarse sand, and recycled ceramic mixed sand is made through recycled ceramic coarse sand partly replacing super-fine sand. By fixed consistence and cement-aggregate ratio, the compressive strength, flexural strength and shrinkage performance between mortar respectively made from natural medium sand, super-fine sand, recycled ceramic coarse sand and recycled ceramic mixed sand are contrasted. The results show that the mortar using recycled ceramic mixed sand as fine aggregate can achieve the project’s strength request and it has higher strength at later age. And by adding recycled ceramic coarse sand in mortar, the brittleness and shrinkage of mortar can be decreased, thus, the crack resistance of the concrete can be improved.

关键词:
陶瓷再生混合砂;强度;对比试验;脆性;干缩性
扫二维码用手机看
未找到相应参数组,请于后台属性模板中添加
(1)采用50%陶瓷再生砂和50%特细砂配出的陶瓷再生混合砂砂浆,各龄期抗折强度明显高于天然中砂砂浆抗折强度,龄期110d前的抗压强度略低于天然中砂砂浆,而110d后的抗压强度高于天然中砂砂浆,可满足设计强度,同时降低砂浆的脆性系数,有利于抗裂性能的提高。
(2)与预湿轻集料例如陶粒对混凝土可以起到“内养护”作用类似,再生陶瓷粗砂表观密度小,吸水率高,也可以起到一定的“内养护”作用,可以提高强度,降低干缩,对实际工程中由于环境、构件形式等限制只能进行的浇水、覆盖等简单养护方式养护的砂浆强度发展和减少开裂作用更明显。
(3)利用废弃陶瓷再生粗砂部分取代特细砂用作工程细骨料是可行的,将这两种资源结合起来,既可以为建筑业开辟新的资源,又可以有效地减少环境污染,还可以改善砂浆的性能,也必将带来极其显著的经济效益和社会效益。
 
[1] 周文娟, 陈家珑, 路宏波. 绿色再生砂浆试验研究[J]. 武汉理工大学学报2009(7):15-18.
[2] 周健儿,李平. 关于我国建筑陶瓷业发展的几点思考[J]. 中国陶瓷工业2003(10):45-48.
[3] 李光瑞. 特细砂混凝土的力学性能研究[D]. 郑州大学硕士学位论文,2007.
[4] 蔡基伟,等. 石粉对中低强度机制砂混凝土性能的影响[J].武汉理工大学学报,2006(4):27-30.
[5] 苏达根,赵一翔. 陶瓷废料的组成与火山灰活性研究[J]. 水泥技术,2009(2):24-26.
[6] 刘数华, 曾力, 吴定燕.水泥矿物成分对砂浆脆性系数的影响[J]. 水泥技术,2005(3):63-64.
[7] 刘数华,方坤河,曾力. 降低高强混凝土脆性的试验研究[J].建筑材料学报,2005(2):150-153. 

相关文件

暂时没有内容信息显示
请先在网站后台添加数据记录。

关注《混凝土与水泥制品》

总访问量 468,401   网站统计

官方微信公众号关闭
苏州混凝土水泥制品研究院有限公司

关于我们    |    联系我们    |    订购杂志    |    回到顶部

版权所有:中国混凝土与水泥制品网  苏ICP备10086386号   网站建设:中企动力 苏州

版权所有:中国混凝土与水泥制品网

苏ICP备10086386号

网站建设:中企动力 苏州