全部文章

超高性能及特种工程水泥基材料

唐 涛,夏艳晴,康阳阳,张柯莹,张雨晴

唐涛,夏艳晴,康阳阳,等.免蒸养超高性能混凝土的设计及在桥面铺装中的应用进展综述[J].混凝土与水泥制品,2025(12):45-49. TANG T,XIA Y Q,KANG Y Y,et al.A review on design and application of non-steam curing ultra-high performance concrete in bridge deck pavement[J].China Concrete and Cement Products,2025(12):45-49.
徐俊.既有混凝土结构加固修复用UHPC的性能研究与工程应用[J].混凝土与水泥制品,2025(12):39-44. XU J.Performance research and engineering application of UHPC for strengthening and repairing existing concrete structures[J].China Concrete and Cement Products,2025(12):39-44.

蒋 涛1,2,夏如茜1,2,张 华3,许志杨1,2,曹鑫铖1,2,田 寅1,2,鲜佳志3,刘 腾4

摘   要:研发了一种路桥伸缩缝修补用预拌高保坍早强混凝土,通过正交试验得到最佳m硅酸盐水泥∶m硫铝酸盐水泥、石膏掺量和水胶比组合,在此基础上,研究了缓凝剂掺量(1.3%、1.5%、1.7%、1.9%、2.1%)对混凝土性能的影响,并在实际工程中验证了该混凝土的修补效果。结果表明:路桥伸缩缝修补用预拌高保坍早强混凝土的最佳配合比为m硅酸盐水泥∶m硫铝酸盐水泥=7∶3、石膏掺量为3.0%、水胶比为0.25、缓凝剂掺量为1.7%;在实际工程中,该混凝土各项性能均满足该桥梁伸缩缝修补工程要求,施工性能良好,能在较短时间内完成修补并迅速开放交通,提高了道路通行效率。Abstract: A ready-mixed high slump and early-strength concrete for repairing road and bridge expansion joints was developed. The optimal combination of mPortland cement∶msulfoaluminate cement, gypsum content, and water-binder ratio was obtained through orthogonal experiments. Based on this, the influence of retarder content (1.3%, 1.5%, 1.7%, 1.9%, 2.1%) on concrete performance was studied, and the repair effect of the concrete was verified in practical engineering. The results show that the optimal mix proportion of ready-mixed high slump and early-strength concrete for repairing road and bridge expansion joints is as follows: mPortland cement∶msulfoaluminate cement=7:3, gypsum content is 3.0%, water-binder ratio is 0.25, and retarder content is 1.7%. In practical engineering, all the properties of the concrete meet the requirements of the bridge expansion joint repair project, and the construction performance is good. It can complete the repair in a short time and quickly open up traffic, improving road traffic efficiency.
蒋涛,夏如茜,张华,等.路桥伸缩缝修补用预拌高保坍早强混凝土的性能优化与应用研究[J].混凝土与水泥制品,2025(12):34-38,44. JIANG T,XIA R X,ZHANG H,et al.Performance optimization and application research of ready-mixed high slump and early-strength concrete for repairing road and bridge expansion joints[J].China Concrete and Cement Products,2025(12):34-38,44.
摘   要:为响应智能建造与新型建筑工业化协同发展的要求,针对传统大型轻质超高性能混凝土(Ultra-high performance concrete,UHPC)-钢框架复合外墙挂板在应用中存在的变形不协同与开裂风险问题,提出了“刚柔并济”的协同变形连接系统。该系统通过刚性连接组件与柔性连接组件的组合设计,结合整装悬浮定位技术、螺栓松解释放内力技术,有效解决了异质材料界面应力集中、收缩应变累积导致的UHPC损伤问题,为大型轻量化外墙工程提供了可靠的协同解决方案。Abstract: In response to the requirements of the coordinated development of intelligent construction and new building industrialization, a collaborative deformation connection system that combines rigidity and flexibility is proposed to address the problems of deformation incompatibility and cracking risk in the application of traditional large lightweight ultra-high performance concrete (UHPC)-steel frame composite exterior wall panels. The system effectively solves the problem of UHPC damage caused by stress concentration and accumulated shrinkage strain at heterogeneous material interfaces through the combination design of rigid and flexible connection components, combined with integrated suspension positioning technology and bolt loosening and releasing internal stress technology, which can provide a reliable collaborative solution for large lightweight exterior wall engineering.
姚海明,蒋勤俭,黄清杰,等.大型轻质UHPC钢框架复合外墙挂板协同变形及开裂控制研究[J].混凝土与水泥制品,2025(12):29-33. YAO H M,JIANG Q J,HUANG Q J,et al.Research on collaborative deformation and crack control of large lightweight UHPC and steel frame composite exterior wall panels[J].China Concrete and Cement Products,2025(12):29-33.

叶国林1,2,宋 祯3,濮 琦1,2,宋秋磊1,2,*,周大卫1,2,吴 浩1,2,陈劲戈1,2

摘   要:参考P·LH 42.5级水泥,通过调控三率值(石灰饱和系数、硅率、铝率)优化了生料配合比,并经低温煅烧、薄料快烧、快速冷却工艺处理后制得强度等级为42.5的超低热硅酸盐水泥(Ultra-low-heat Portland cement,ULHC),研究了粉煤灰掺量(0、20%、40%、60%)和柠檬酸钠掺量(0、0.1%、0.5%)对ULHC水化放热行为的影响。结果表明:ULHC的石灰饱和系数、硅率、铝率分别为0.71、2.54、0.70,7 d累计水化放热量为163.5 J/g;ULHC的水化放热历程与P·LH 42.5级水泥基本相同,但水化放热量和水化放热速率显著降低;随着粉煤灰掺量的增加,ULHC的水化温峰值、水化放热速率峰值、累计水化放热量均降低;掺入0.1%柠檬酸钠会延长ULHC的水化放热时间,降低水化放热速率峰值,但对累计水化放热量几乎无影响;掺入0.5%柠檬酸钠后,ULHC未出现明显的水化放热峰。Abstract: Referring to P·LH 42.5 grade cement, the raw material mix proportion was optimized by adjusting the three ratio values (lime saturation coefficient, silicon ratio, aluminum ratio), and after low-temperature calcination, thin material rapid burning, and rapid cooling processes, ultra-low-heat Portland cement (ULHC) with a strength grade of 42.5 was prepared. The effects of fly ash content (0, 20%, 40%, 60%) and sodium citrate content (0, 0.1%, 0.5%) on the hydration heat release behavior of ULHC were studied. The results show that the lime saturation coefficient, silicon content, and aluminum content of ULHC are 0.71, 2.54, and 0.70, respectively, with a 7 d cumulative hydration heat release of 163.5 J/g. The hydration heat release process of ULHC is basically the same as that of P·LH 42.5 grade cement, but the hydration heat release and hydration heat release rate are significantly reduced. With the increase of fly ash content, the peak hydration temperature, peak hydration heat release rate, and cumulative hydration heat release of ULHC all decrease. Adding 0.1% content of sodium citrate can prolong the hydration heat release time of ULHC, reduce the peak hydration heat release rate, but has almost no effect on the cumulative hydration heat release. After adding 0.5% content of sodium citrate, there is no significant hydration heat release peak observed in ULHC.
叶国林,宋祯,濮琦,等.超低热硅酸盐水泥(ULHC)的研制及水化放热行为研究[J].混凝土与水泥制品,2025(12):24-28,33. YE G L,SONG Z,PU Q,et al.Research on development and hydration heat release behavior of Ultra-low-heat Portland cement (ULHC)[J].China Concrete and Cement Products,2025(12):24-28,33.
摘   要:选取了抗爆结构中较有代表性的水泥基吸能材料(泡沫混凝土、陶粒混凝土、陶粒泡沫混凝土、橡胶混凝土),介绍了国内外关于这几种材料在吸能能力方面的研究进展,讨论了目前水泥基吸能材料研究存在的不足,并展望了未来的发展趋势。Abstract: The representative cement-based energy absorbing materials (foamed concrete, ceramsite concrete, ceramsite foamed concrete, rubber concrete) in anti-explosion structures are selected, and the research progress of these materials in energy absorpting capacity at home and abroad is introduced. The shortcomings in the current research on cement-based energy absorbing materials are discussed, and the future development trends are prospected.
屈津疆,李硕标,王振.抗爆结构中水泥基吸能材料研究综述[J].混凝土与水泥制品,2025(12):16-23. QU J J,LI S B,WANG Z.A review of research on cement-based energy absorbing materials in anti-explosion structures[J].China Concrete and Cement Products,2025(12):16-23.