全部文章
第三期
郑云生,曹元辉,陈苏芹
郑云生,曹元辉,陈苏芹.GB/T 45592—2025《建筑材料产品追溯体系通用要求》标准解读[J].混凝土与水泥制品,2026,53(3):116-119. ZHENG Y S,CAO Y H,CHEN S Q.Interpretation of GB/T 45592—2025 General requirements for building materials products traceability system[J].China Concrete and Cement Products,2026,53(3):116-119 (in Chinese).
史鹏飞1,邹 伟1,于诚谦2,王 凯2,马俊杰3
摘 要:采用热泼-热闷联合处理工艺对钢渣进行改性,研究了水泥用量(3.0%、3.5%、4.0%)与成型静置时间(0、1、2、3 h)对工业废渣稳定材料最佳含水率、最大干密度、压实度及无侧限抗压强度的影响,优选出该稳定材料的最优配合比,并将其应用于实际工程。结果表明:采用热泼-热闷联合处理工艺可显著改善钢渣的级配、f-CaO含量及体积安定性;工业废渣稳定材料的最优配合比为m水泥∶m粉煤灰∶m碎石∶m钢渣∶m水=3.5∶6.5∶56.0∶34.0∶6.0,且混合料成型静置时间需严格控制在2 h内;工业废渣稳定材料应用于路面底基层时,其各项性能均满足相关标准要求;在实际应用过程中,可通过优化配合比、精准调控拌合含水率、改进摊铺碾压工艺、规范施工环境等措施提升施工质量。研究成果可为钢渣资源化利用及道路工程绿色建设提供技术支撑。Abstract: Steel slag was modified by the combined hot-pouring and hot-steaming treatment process. The effects of cement content (3.0%, 3.5%, 4.0%) and molding standing time (0, 1, 2, 3 h) on the optimum moisture content, maximum dry density, compaction degree and unconfined compressive strength of the industrial waste residue stabilized material were investigated. On this basis, the optimal mix proportion of the stabilized material was screened out, and its application in practical engineering was further implemented. The results show that the gradation, f-CaO content and volume stability of steel slag are significantly improved by the combined hot-pouring and hot-steaming treatment process. The optimal mix proportion of the industrial waste residue stabilized material is as follows: mcement∶mfly ash∶mcrushed stone∶msteel slag∶mwater=3.5∶6.5∶56.0∶34.0∶6.0. Meanwhile, the molding standing time of the mixture is required to be strictly controlled within 2 h. When the industrial waste residue stabilized material is applied to the pavement subbase, its properties meet the requirements of relevant standards. In the actual application process, the construction quality can be effectively improved by optimizing mix proportion, accurately regulating mixing moisture content, improving paving and rolling technology, and standardizing construction environment. The research findings can provide technical support for the resource utilization of steel slag and the green construction of road engineering.
史鹏飞,邹伟,于诚谦,等.工业废渣稳定材料性能优化及其在路面底基层中的应用[J].混凝土与水泥制品,2026,53(3):110-115. SHI P F,ZOU W,YU C Q,et al.Performance optimization of industrial waste residue stabilized material and its application in pavement subbase[J].China Concrete and Cement Products,2026,53(3):110-115 (in Chinese).
崔安哲1,蒋文广2,*,胡小虎3,董 芸2,马洪玉3,吕兴栋2
摘 要:为了有效提高堆石坝面板混凝土的耐久性能,本文研究了3种功能性外加剂(膨胀剂、抗裂剂、水化热抑制剂)对堆石坝面板混凝土力学性能、热学性能、干燥收缩、抗裂性能的影响。结果表明:掺入适量抗裂剂、膨胀剂、水化热抑制剂均会导致混凝土各龄期抗压强度、轴拉强度、极限拉伸值降低;掺入适量抗裂剂、膨胀剂有利于降低混凝土的干燥收缩,而掺入适量水化热抑制剂对降低干燥收缩的作用相对较小;掺入适量抗裂剂、膨胀剂,混凝土的绝热温升降低,掺入适量水化热抑制剂减缓了水泥的水化进程,使混凝土的绝热温升过程延长,但不会影响水泥的最终水化;掺入适量抗裂剂、膨胀剂、水化热抑制剂均有利于混凝土抗裂性能的改善。Abstract: In order to effectively improve the durability of rockfill dam face slab concrete, the effects of three functional admixtures (expansion agent, crack resistance agent, and hydration heat inhibitor) on the mechanical properties, thermal properties, drying shrinkage, and crack resistance performance of rockfill dam face slab concrete were studied in this paper. The results indicate that the addition of appropriate amounts of crack resistance agent, expansion agent, and hydration heat inhibitor can lead to a decrease in the compressive strength, axial tensile strength, and ultimate tensile value of concrete at various ages. Adding an appropriate amount of crack resistance agent and expansion agent is beneficial for reducing the drying shrinkage of concrete, while adding an appropriate amount of hydration heat inhibitor has a relatively small effect on reducing drying shrinkage. Adding an appropriate amount of crack resistance agent and expansion agent reduces the adiabatic temperature rise of concrete. Adding an appropriate amount of hydration heat inhibitor slows down the hydration process of cement, prolongs the adiabatic temperature rise process of concrete, but does not affect the final hydration of cement. Adding an appropriate amount of crack resistance agent, expansion agent, and hydration heat inhibitor is beneficial for improving the crack resistance performance of concrete.
崔安哲,蒋文广,胡小虎,等.功能性外加剂对堆石坝工程用面板混凝土性能的影响研究[J].混凝土与水泥制品,2026,53(3):105-109. CUI A Z,JIANG W G,HU X H,et al.Study on the influence of functional admixtures on the performance of face slab concrete for rockfill dam engineering[J].China Concrete and Cement Products,2026,53(3):105-109 (in Chinese).
蒋梦涵1a,廖宜顺1a,1b,1c,*,周 琦2,李文华2
摘 要:研究了偏高岭土掺量(0、10%、20%、30%)对铁铝酸盐水泥工作性、抗压强度、电阻率、抗硫酸盐侵蚀性能等的影响,并分析了其水化产物及水化放热情况。结果表明:随着偏高岭土掺量的增加,铁铝酸盐水泥浆体的流动度降低,凝结时间缩短,试件的抗压强度基本降低;适量掺入偏高岭土可以在一定程度上促进铁铝酸盐水泥早期水化,促进钙矾石的生成,且不会生成新的水化产物,在一定程度上提高试件的抗硫酸盐侵蚀性能。Abstract: The effects of metakaolin content (0, 10%, 20%, 30%) on the workability, compressive strength, electrical resistivity, and sulfate corrosion resistance of ferroaluminate cement were studied. The hydration products and hydration heat release were analyzed. The results show that with the increase of metakaolin content, the fluidity of ferroaluminate cement paste decreases, the setting time is shortened, and the compressive strength of the specimens basically decreases. Appropriate addition of metakaolin can promote the early hydration of ferroaluminate cement and the formation of ettringite to a certain extent, without generating new hydration products, thus improving the sulfate corrosion resistance of specimens to a certain extent.
蒋梦涵,廖宜顺,周琦,等.偏高岭土对铁铝酸盐水泥性能的影响研究[J].混凝土与水泥制品,2026,53(3):99-104. JIANG M H,LIAO Y S,ZHOU Q,et al.Study on the influence of metakaolin on the properties of ferroaluminate cement[J].China Concrete and Cement Products,2026,53(3):99-104 (in Chinese).
樊俊江,王 琼,杨利香
摘 要:为了探索超高性能混凝土(Ultra-high performance concrete,UHPC)的低碳化技术路径,设计了UC120、UC130 两个强度等级的 UHPC 基准组 JZ#1、JZ#2。在JZ#1基础上,通过掺入粉煤灰或矿粉、调整硅灰掺量,研究了矿物掺合料对UHPC拌合物性能、力学性能及减碳效果的影响;在JZ#2基础上,通过调整钢纤维掺量和砂胶比,研究了二者对UHPC力学性能和减碳效果的影响。结果表明:当粉煤灰掺量不超过10%、矿粉掺量不超过20%、硅灰掺量在10%~25%范围内时,对UHPC的拌合物性能和抗压强度无显著影响;适当降低钢纤维掺量至2.0%或提高砂胶比至0.9,均不会对UHPC的抗压强度产生显著影响;在UHPC的拌合物性能与力学性能均满足设计要求的前提下,掺入适量粉煤灰或矿粉,合理调整硅灰掺量、钢纤维掺量和砂胶比,均可实现显著的减碳效果。研究成果可为UHPC 的低碳化设计提供量化技术依据与优化方案,同时为建材行业实现“双碳”目标提供切实可行的技术路径。Abstract: In order to explore the low-carbon technical path of ultra-high performance concrete (UHPC), two UHPC reference groups (JZ#1 and JZ#2) with strength grades of UC120 and UC130 were designed. Based on JZ#1 group, the effects of mineral admixtures on the mixture performance, mechanical properties and carbon reduction effect of UHPC were investigated by incorporating fly ash or slag powder and adjusting the silica fume content. Based on JZ#2 group, the effects of steel fiber content and sand-binder ratio on the mechanical properties and carbon reduction effect of UHPC were studied by adjusting the two parameters. The results indicate that when the fly ash content does not exceed 10%, the slag powder content does not exceed 20%, and the silica fume content is within the range of 10% to 25%, there is no significant impact on the mixture performance and compressive strength of UHPC. Moreover, appropriately reducing the steel fiber content to 2.0% or increasing the sand-binder ratio to 0.9 will not significantly affect the compressive strength of UHPC. On the premise that both the mixture performance and mechanical properties of UHPC meet the design requirements, the incorporation of an appropriate content of fly ash or slag powder, and rational adjustment of silica fume content, steel fiber content and sand-binder ratio, can all achieve a remarkable carbon reduction effect. The research results can provide a quantitative technical basis and optimization schemes for the low-carbon design of UHPC, and meanwhile offer a feasible technical path for the building materials industry to achieve the "dual carbon" goals.
樊俊江,王琼,杨利香.低碳超高性能混凝土(UHPC)的配合比优化设计与减碳效果研究[J].混凝土与水泥制品,2026,53(3):93-98,109. FAN J J,WANG Q,YANG L X.Research on mix proportion optimization design and carbon reduction effect of low-carbon ultra-high performance concrete (UHPC)[J].China Concrete and Cement Products,2026,53(3):93-98,109 (in Chinese).
苏佶智1,徐日昌2,王义超2,*,王丽欢1,李 燕3,张戊晨1
摘 要:为改善石膏基复合材料的韧性,根据工程水泥基复合材料(ECC)材料微观设计原理,选择聚乙烯(PE)纤维作为增强材料,研发了具有应变硬化和优异变形能力的超高延性石膏基复合材料,并分析了其在室内、绝干、浸水3种养护条件下的工作性、力学性能、耐水性能。结果表明:3种养护条件下,试件均呈现出显著的应变硬化特性,试件的抗拉强度在1.8~6.5 MPa之间,拉伸应变在4%~7%之间;纤维的掺入并未明显改善试件的耐水性能,但可显著改善试件的拉伸、压缩性能,提高拉伸变形能力和峰后压缩变形能力。Abstract: In order to improve the toughness of gypsum-based composites materials, polyethylene (PE) fiber was selected as a reinforcing material according to the micro-design principle of engineered cementitious composite(ECC) materials. The ultra-high ductility gypsum-based composite materials with strain hardening and excellent deformation capacity was developed, and its workability, mechanical properties and water resistance under indoor, absolute dryness and immersion curing conditions were analyzed. The results show that under 3 types of curing conditions, the specimens all show significant strain hardening characteristics, the tensile strengths of the specimens are between 1.8 MPa and 6.5 MPa, and the tensile strain is between 4% and 7%. The addition of fibers do not significantly improve the water resistance of the specimens, but it can significantly improve their tensile and compressive properties, as well as their tensile deformation ability and post peak compression deformation ability.
苏佶智,徐日昌,王义超,等.超高延性石膏基复合材料的力学及耐水性能研究[J].混凝土与水泥制品,2026,53(3):87-92. SU J Z,XU R C,WANG Y C,et al.Study on mechanical properties and water resistance of ultra-high ductility gypsum-based composite materials[J].China Concrete and Cement Products,2026,53(3):87-92 (in Chinese).