全部文章

混凝土基础理论

胡伟华1,2,吴 彬3,*,周文瑞3

摘   要:研究了不同加载速率(10-5、5×10-5、10-4、5×10-4、10-3、5×10-3、10-2 s-1)下长龄期(112、183、345、810、1 248、1 550 d)混凝土的单轴压缩强度,并对混凝土强度与龄期的双曲线、对数、指数模型进行了评价。结果表明:当龄期相同时,试件的单轴压缩强度基本随加载速率的增加而增加;当加载速率相同时,随着龄期的增加,试件的单轴压缩强度先快速增加然后缓慢增加最后趋于稳定,增幅随着龄期的增加呈波动增加的趋势;双曲线模型与指数模型能较好地反映长龄期混凝土强度与龄期的关系。Abstract: The uniaxial compressive strength of concrete at different loading rates (10-5、5×10-5、10-4、5×10-4、10-3、5×10-3、10-2 s-1) and long ages (112, 183, 345, 810, 1 248, 1 550 d) was studied. The hyperbolic, logarithmic, and exponential models describing the relationship between concrete strength and age were evaluated. The results show that when the age is the same, the uniaxial compressive strength of the specimen increases with increasing loading rate. When the loading rate is the same, with the increase of age, the uniaxial compressive strength of the specimens increases rapidly, then slowly increases, and finally tends to stabilize, and the growth rate shows a fluctuating increasing trend with the increase of age. The hyperbolic and exponential models more accurately represent the relationship between the strength and age in long age concrete.
胡伟华,吴彬,周文瑞.不同加载速率下长龄期混凝土的强度变化研究[J].混凝土与水泥制品,2026,53(3):22-26. HU W H,WU B,ZHOU W R.Study on strength changes of long age concrete under different loading rates[J].China Concrete and Cement Products,2026,53(3):22-26 (in Chinese).
摘   要:活性MgO(f-MgO)因其在混凝土中具有补偿收缩、抑制裂缝发展的作用而受到广泛关注。为系统研究不同影响因素下f-MgO的作用效果,并提高工程使用效能,本文研究了f-MgO在不同掺入方式(内掺、外掺)、养护温度(20、40、60 ℃)和约束条件(无约束、一维限制约束)下对砂浆变形的影响。结果表明:无论f-MgO以哪种方式掺入,其均可以显著增加砂浆的膨胀变形;与内掺相比,外掺f-MgO对砂浆膨胀变形的增幅更显著;养护温度的变化对外掺f-MgO组砂浆的膨胀变形影响更显著;f-MgO掺入方式的变化对试件膨胀变形的影响在60 ℃饱水养护和无约束条件下最显著。研究结果可为混凝土裂缝的预防与控制提供参考。Abstract:  Active MgO (f-MgO) has garnered significant attention for its role in compensating for shrinkage and inhibiting crack development in concrete. In order to systematically investigate the effects of f-MgO under various influencing factors and enhance its engineering application effectiveness, the influence of different f-MgO addition methods (internal or external addition), curing temperatures (20, 40, 60 ℃), and constraint conditions (unconstrained, one-dimensional constraint) on the deformation performance of mortar was studied. The results indicate that regardless of the addition method of f-MgO, it can significantly increase the expansion deformation of mortar. Compared with the internal addition, the external addition of f-MgO has a more significant increase in the expansion deformation of mortar. The change of curing temperature has a more significant impact on the expansion deformation of mortar with external addition of f-MgO. The change of the addition methods of f-MgO has the most significant effect on the expansion deformation of specimens under 60 ℃ water-saturated curing and unconstrained conditions. The findings can provide valuable references for the prevention and control of concrete cracks.
王志鹏,付传祥,张守治,等.不同活性MgO掺入方式、养护温度、约束条件对砂浆变形性能的影响[J].混凝土与水泥制品,2026,53(3):18-21,26. WANG Z P,FU C X,ZHANG S Z,et al.Influence of different addition methods of active MgO, curing temperatures, and constraint conditions on the deformation performance of mortar[J].China Concrete and Cement Products,2026,53(3):18-21,26 (in Chinese).
摘   要:研发了一种不掺速凝剂的超高性能喷射混凝土(Ultra-high performance shotcrete,UHPSC),研究了偏高岭土掺量(0、5%、10%)、钢纤维种类(L13D20、CML10、L8D12)、纤维素醚种类(HEMC、HPMC)对其抗压、抗折强度的影响,并优选了最佳配合比,对比了UHPSC与防腐修复砂浆的性能,并进行了墙体实喷试验。结果表明:UHPSC的最佳配合比为偏高岭土掺量5%、钢纤维采用L8D12、纤维素醚采用HEMC;UHPSC的力学性能远高于防腐修复砂浆,28 d膨胀率也较防腐修复砂浆有所提高,其他性能基本与防腐修复砂浆持平;墙体实喷试验效果较好,一次性喷射UHPSC厚度4 cm左右无任何垂挂现象,墙面喷射样品及大板切割试块致密性较好,大板切割试块的抗压强度高于现场浇筑试件。Abstract: A type of ultra-high performance shotcrete (UHPSC) without the addition of accelerator was developed. The effects of metakaolin content(0, 5%, 10%), steel fiber type(L13D20, CML10, L8D12), and cellulose ether type (HEMC, HPMC) on compressive and flexural strength were studied, and the optimal mix proportion was selected. The performance of UHPSC and anti-corrosion repair mortar was compared, and wall actual spray test was conducted. The results show that the optimal mix proportion of UHPSC is metakaolin content of 5%, using L8D12 steel fiber, and HEMC cellulose ether. The mechanical properties of UHPSC are much higher than those of anti-corrosion repair mortar, and the 28 d expansion rate is also improved compared to anti-corrosion repair mortar. Other properties are comparable to anti-corrosion repair mortar. The wall actual spray test shows good results, with a one-time spraying of UHPSC with a thickness of about 4 cm without any hanging phenomenon. The wall spray samples and large board cutting test blocks have good density, and the compressive strength of the large board cutting test block is higher than that of the on-site pouring specimen.
胡文佩.无速凝剂超高性能喷射混凝土的制备与性能研究[J].混凝土与水泥制品,2026,53(3):13-17. HU W P.Preparation and properties of ultra-high performance shotcrete without accelerator[J].China Concrete and Cement Products,2026,53(3):13-17 (in Chinese).

王朴炎1,张 洁1,周东杰1,胡慧峰1,杨艳婷1,俞梦迪1,贺 阳2,3,*

摘   要:研究了不同水泥型号(P·O 42.5级水泥、P·O 52.5级水泥)、硅灰掺量(5%~20%)、粉煤灰掺量(10%~30%)和矿渣粉掺量(10%~30%)对超高性能混凝土(Ultra-high performance concrete,UHPC)抗压强度的影响,并结合生命周期评价(Life cycle assessment,LCA)方法探讨了UHPC的环境效益。结果表明:与P·O 42.5级水泥相比,采用P·O 52.5级水泥的UHPC抗压强度更高;掺入适量矿物掺合料可有效提升UHPC的抗压强度,同时兼顾环境效益,实现力学性能与绿色性能的协同优化,硅灰、粉煤灰和矿渣粉的最佳掺量分别为10%、20%和20%。Abstract: The effects of different cement types (P·O 42.5 grade cement, P·O 52.5 grade cement), silica fume contents (5%~20%), fly ash contents (10%~30%), and slag powder contents (10%~30%) on the compressive strength of ultra-high performance concrete(UHPC) were studied, and the environmental benefits of UHPC were explored by using the life cycle assessment(LCA) method. The results show that compared with P·O 42.5 grade cement, UHPC with P·O 52.5 grade cement has higher compressive strength. Adding appropriate content of mineral admixtures can effectively improve the compressive strength of UHPC, while also considering environmental benefits, achieving synergistic optimization of mechanical properties and green properties. The optimal contents of silica fume, fly ash, and slag powder are 10%, 20%, and 20%, respectively.
王朴炎,张洁,周东杰,等.基于胶凝材料体系优化的超高性能混凝土(UHPC)的抗压强度与环境效益研究[J].混凝土与水泥制品,2026,53(3):7-12. WANG P Y,ZHANG J,ZHOU D J,et al.Research on the compressive strength and environmental benefits of ultra-high performance concrete (UHPC) based on optimization of cementitious material system[J].China Concrete and Cement Products,2026,53(3):7-12 (in Chinese).
摘   要:采用小幅震荡剪切测试研究了掺多种矿物掺合料的复合胶凝材料浆体结构形成过程,采用等温量热法测试了复合胶凝材料浆体的水化放热速率,分析了浆体结构的储能模量和相位角的经时变化。结果表明:根据储能模量和相位角的经时变化,复合胶凝材料浆体结构形成过程可分为初始阶段、线性增长阶段、指数增长阶段这3个阶段,其分别对应胶凝材料水化的初始期、诱导期和加速期初始阶段;相位角趋于稳定的时间点是初始阶段与线性增长阶段的转变点;储能模量开始指数增长的时间与胶凝材料水化诱导期的结束时间基本一致;矿物掺合料的细度(比表面积)、活性和颗粒表面状态可明显影响复合胶凝材料浆体结构的形成速率。Abstract: The paste structure build-up process of composite binders containing various kinds of mineral admixture was studied by using small amplitude oscillatory shear test. The hydration heat release rate of composite binder paste was tested by using isothermal calorimetry. The time-dependent variation of storage modulus and the phase angle of paste structure was obtained. The results show that the paste structure build-up process of binders can be divided to 3 stages: the initial stage, the stage of linear growth and the stage of exponential growth, and they correspond respectively to the initial stage, the induction stage and the initial accelerating stage of the hydration of composite binders. The time when the phase angle becomes stable is the transition point between the initial and linear growth stage. The time of the exponential growth of storage modulus is almost the same as the ending time of the induction stage of the hydration of composite binders. The fineness (specific surface area), activity and particle surface characteristics of mineral admixtures can significantly affect the paste structure build-up rate of composite binders.
阎培渝,刘宇.复合胶凝材料浆体结构形成过程与初始水化的关系[J].混凝土与水泥制品,2026,53(3):1-6,12. YAN P Y,LIU Y.The relationship between the paste structure build-up process of composite binders and their initial hydration[J].China Concrete and Cement Products,2026,53(3):1-6,12 (in Chinese).