全部文章
绿色低碳与环保利废
王欣欣,张永虹,杨博豪
为了促进废旧风机叶片的资源化利用,可将其用于3D打印混凝土中,但应用时存在可打印性不佳的问题。为解决此问题,本文研究了减水剂(掺量为0.14%、0.15%、0.16%)、增稠剂(掺量为0.03%、0.04%、0.05%)、引气剂(掺量为0.01%、0.02%、0.03%)对掺废旧风机叶片3D打印混凝土(以下简称3D打印混凝土)流变性能、可打印性的影响。结果表明:3D打印混凝土的最佳外加剂掺量为减水剂0.15%、增稠剂0.05%、引气剂0.03%,在此掺量下,3D打印混凝土的流变性能、可打印性均较好。研究成果可为废旧风机叶片在建筑3D打印领域的高值化利用提供理论依据。In order to promote the resource utilization of waste wind turbine blades, they can be applied in 3D printed concrete. However, such material exhibits poor printability in practical applications. To address this issue, this paper investigated the effects of water reducers (dosages of 0.14%, 0.15%, and 0.16%), thickeners (dosages of 0.03%, 0.04%, and 0.05%), and air-entraining agents (dosages of 0.01%, 0.02%, and 0.03%) on the rheological properties and printability of 3D printed concrete containing waste wind turbine blades (3D printed concrete). The results show that the optimal admixture dosages are 0.15% water reducer, 0.05% thickener, and 0.03% air-entraining agent. Under the optimal mix proportion, the 3D printed concrete exhibits excellent rheological properties and printability. The research results can provide a theoretical basis for the high-value utilization of waste wind turbine blades in the field of architectural 3D printing.
王欣欣,张永虹,杨博豪.不同功能型外加剂对掺废旧风机叶片3D打印混凝土性能的影响研究[J].混凝土与水泥制品,2026,53(4):91-96. WANG X X,ZHANG Y H,YANG B H.Research on the influence of different functional additives on the properties of 3D printed concrete containing waste wind turbine blades[J].China Concrete and Cement Products,2026,53(4):91-96 (in Chinese).
苟余江1,张荣华1,*,韩跃伟1,关素敏1,欧阳征1,蒋章和2
为了优化C30混凝土的配合比设计,充分利用地方骨料资源,明确机制砂岩性与细度对C30混凝土性能的作用规律,本文研究了不同岩性(花岗岩、石灰岩)及比粒度(5.5、4.7、4.3)机制砂对C30混凝土坍落度、扩展度、抗压强度、抗碳化性能的影响。结果表明:相同比粒度时,花岗岩混凝土的保坍效果优于石灰岩混凝土,但在抗压强度和抗碳化性能方面,石灰岩混凝土较花岗岩混凝土更具优势;整体上,对于花岗岩机制砂,当比粒度为4.7时,其制备的混凝土综合性能相对较好;对于石灰岩机制砂,当比粒度为4.3时,其制备的混凝土综合性能相对较好。研究结果可为工程中细骨料的合理选用及C30混凝土的质量控制提供参考。In order to optimize the mix proportion of C30 concrete, fully utilize local aggregate resources, and clarify the influence of manufactured sand lithology and fineness on the performance of C30 concrete, the influences of different lithologies (granite, limestone) and specific granularities (5.5, 4.7, 4.3) of manufactured sand on the slump, slump-flow, compressive strength, and anti-carbonation performance of C30 concrete were studied in this article. The results show that when the specific granularity is the same, the collapse retention effect of granite concrete is better than that of limestone concrete, but in terms of compressive strength and anti-carbonation performance, limestone concrete has more advantages than granite concrete. Overall, for granite manufactured sand, when the specific granularity is 4.7, the comprehensive performance of the prepared concrete is relatively good. For limestone manufactured sand, when the specific granularity is 4.3, the comprehensive performance of the prepared concrete is relatively good. The research results can provide reference for the rational selection of fine aggregates in engineering and the quality control of C30 concrete.
苟余江,张荣华,韩跃伟,等.不同岩性、比粒度机制砂对C30混凝土性能的影响研究[J].混凝土与水泥制品,2026,53(4):87-90. GOU Y J,ZHANG R H,HAN Y W,et al.Study on the influence of different lithologies and specific granularities of manufactured sand on the performance of C30 concrete[J].China Concrete and Cement Products,2026,53(4):87-90 (in Chinese).
黄小川,时 宇,陈小辉,肖世玉,朱金华,陶 俊*
黄小川,时宇,陈小辉,等.多元复合胶凝体系低碳泡沫混凝土的制备及其性能研究[J].混凝土与水泥制品,2026,53(4):81-86. HUANG X C,SHI Y,CHEN X H,et al.Preparation and performance study of low-carbon foamed concrete with multi-component cementitious system[J].China Concrete and Cement Products,2026,53(4):81-86 (in Chinese).
陈 捷1,王慧斌1,吴海华1,崔 通1,杨东来1,张同生2,*
为实现铝土矿冶炼浸出渣的高值化资源化利用,以浸出渣为主要原材料煅烧水泥熟料,研究了煅烧温度(1 300、1 350、1 380、1 410 ℃)、保温时间(30 min、60 min)和浸出渣比表面积(319 m2/kg、380 m2/kg)对熟料f-CaO、R2O、MgO含量及烧失量的影响,并进行了微观分析。结果表明:适当升高煅烧温度可优化熟料烧成效果与矿物发育,当煅烧温度为1 410 ℃时,熟料内部孔洞基本消失、f-CaO基本被消耗,熟料矿物发育良好;当保温时间由30 min增至60 min时,熟料烧失量与f-CaO含量均下降,微观结构小幅改善,但物相组成无明显变化;适当增大浸出渣比表面积可使熟料中f-CaO、R2O、MgO含量及烧失量呈小幅下降趋势,且均满足相关标准要求,同时能提升矿物发育程度、改善矿物形貌。研究成果可为浸出渣制备水泥熟料的工业化应用提供技术支撑。In order to achieve high-value resource utilization of bauxite smelting leaching residues, cement clinker was calcined with leaching residues as the primary raw material. The effects of calcination temperature(1 300, 1 350, 1 380, 1 410 ℃), insulation time (30 min, 60 min), and specific surface area (319 m2/kg, 380 m2/kg) of the leaching residues on the contents of f-CaO, R2O, MgO, and loss on ignition of the clinker were investigated, and microstructural analysis was conducted. The results indicate that appropriately increasing the calcination temperature optimizes clinker firing effect and mineral phase development. When the calcination temperature is 1 410 ℃, there are almost no pores in the clinker, f-CaO is basically consumed, and the clinker minerals are well-developed. With insulation time increasing from 30 min to 60 min, the loss on ignition and f-CaO content both decrease, the microstructure is slightly improved, while the phase composition remains basically unchanged. Appropriately increasing the specific surface area of leaching residues leads to a slight decrease in the f-CaO, R2O, MgO contents, and loss on ignition of the clinker, all of which meet the requirements of relevant standards, and simultaneously enhances mineral development and improves mineral morphology. The findings can provide technical support for the industrial application of leaching residues in cement clinker preparation.
陈捷,王慧斌,吴海华,等.铝土矿冶炼浸出渣制备水泥熟料的试验研究[J].混凝土与水泥制品,2026,53(4):74-80. CHEN J,WANG H B,WU H H,et al.Experimental study on the preparation of cement clinker from bauxite smelting leaching residues[J].China Concrete and Cement Products,2026,53(4):74-80 (in Chinese).
杜渊博1,2,吴志刚1,2,3,刘 伟1,杨雪超1,王雪敏1,韩宇栋1,2
高原特殊环境会对混凝土的水化反应过程及性能产生显著影响。为探究铜尾矿粉掺量与高原低气压环境对混凝土水化特性、力学及耐久性能的影响,在常压与高原低气压环境下开展水化放热、抗压强度、电通量、碳化及冻融试验。结果表明:在两种环境下,随着铜尾矿粉掺量的增加,胶凝材料体系第二水化放热峰峰值、水化放热量逐渐降低,峰位出现时间基本不变;混凝土各龄期抗压强度、抗氯离子渗透性能、抗碳化及抗冻性能均呈先提升后下降趋势,当铜尾矿粉掺量为10%时,混凝土的各项性能最优;在相同龄期与铜尾矿粉掺量下,相较于常压环境,高原低气压环境下混凝土28 d、90 d抗压强度均较低,抗氯离子渗透性能、抗碳化及抗冻性能明显下降。研究成果可为高原环境下铜尾矿粉混凝土的工程应用提供试验依据与理论参考。The special plateau environment has a significant impact on the hydration process and performance of concrete. To investigate the effects of copper tailings powder content and plateau low atmospheric pressure environment on the hydration characteristics, mechanical properties and durability of concrete, tests of hydration heat, compressive strength, electric flux, carbonation and freeze-thaw were conducted under normal atmospheric pressure and plateau low atmospheric pressure environments. The results show that with the increase of copper tailings powder content, the peak value of the second hydration exothermic peak and the total hydration heat of the cementitious material system decrease gradually, while the occurrence time of the peak remains basically unchanged under both environments. The compressive strength at all ages, chloride ion penetration resistance, carbonation resistance and frost resistance of concrete first increase and then decrease, and all properties reach the optimum when the copper tailings powder content is 10%. At the same curing age and copper tailings powder content, compared with normal atmospheric environment, the 28 d and 90 d compressive strengths of concrete under plateau low atmospheric pressure are lower, and its chloride ion penetration resistance, carbonation resistance and frost resistance decrease significantly. The research results can provide experimental basis and theoretical reference for the engineering application of concrete mixed with copper tailings powder in plateau environments.
杜渊博,吴志刚,刘伟,等.高原低气压环境下铜尾矿粉对混凝土水化及性能的影响[J].混凝土与水泥制品,2026,53(4):68-73,80. DU Y B,WU Z G,LIU W,et al.Effects of copper tailings powder on the hydration and properties of concrete under plateau low atmospheric pressure environment[J].China Concrete and Cement Products,2026,53(4):68-73,80 (in Chinese).
李世伟,何 鑫*,甘 月,余世杰,马晨雨,魏永红
为实现水基岩屑的高值资源化利用,本文基于响应面法研究了水基岩屑掺量(40%、50%、60%)、水固比(0.11、0.12、0.13)及碱当量(4%、6%、8%)对水基岩屑免烧砖 28 d 抗压强度的影响,并优化了配合比。结果表明:水基岩屑免烧砖的主要水化产物为 C-S-H 凝胶与 AFt,水化产物相互交织、紧密黏结并填充体系内部空隙,有效提升基体密实度;水基岩屑免烧砖的最佳配合比组合为水基岩屑掺量 42.28%、水固比 0.117、碱当量 4.21%,该条件下 28 d 抗压强度实测值与预测值的误差仅为2.5%,模型预测精度较高;在最佳配合比下,水基岩屑免烧砖的 28 d 抗压强度、冻后抗压强度、冻后质量损失率、吸水率及软化系数均满足相关标准要求。研究成果可为水基岩屑的规模化、高值资源化利用提供技术支撑,同时为同类工业固废制备免烧砖的配合比设计及性能调控提供参考。In order to achieve the high-value resource utilization of water-based cuttings, the effects of water-based cuttings content (40%, 50%, 60%), water-solid ratio (0.11, 0.12, 0.13), and alkali equivalent (4%, 6%, 8%) on the 28 d compressive strength of unfired bricks with water-based cuttings were investigated based on the response surface methodology, and the mix proportion was optimized. The results show that the main hydration products of the unfired bricks with water-based cuttings are C-S-H gel and AFt. The hydration products interweave, bond tightly, and fill the internal voids of the system, effectively improving the compactness of the matrix. The optimal mix proportion combination for unfired bricks with water-based cuttings is as follows: a water-based cuttings content of 42.28%, a water-solid ratio of 0.117, and an alkali equivalent of 4.21%. Under this condition, the error between the measured and predicted values of the 28 d compressive strength is only 2.5%, indicating a high prediction accuracy of the model. Under the optimal mix proportion, the 28 d compressive strength, compressive strength after freeze-thaw cycles, mass loss rate after freeze-thaw cycles, water absorption rate, and softening coefficient of unfired bricks with water-based cuttings all meet the requirements of relevant standards. The research results can provide technical support for the large-scale and high-value resource utilization of water-based cuttings, and also offer a reference for the mix proportion design and performance regulation of unfired bricks prepared from similar industrial solid wastes.
李世伟,何鑫,甘月,等.基于响应面法的水基岩屑免烧砖配合比优化及验证分析[J].混凝土与水泥制品,2026,53(4):62-67. LI S W,HE X,GAN Y,et al.Optimization and verification analysis of mix proportion of unfired bricks with water-based cuttings based on response surface methodology[J].China Concrete and Cement Products,2026,53(4):62-67 (in Chinese).