全部文章

第五期

摘   要:为准确评估钢管混凝土界面脱空对其性能的危害,量化脱空风险并厘清其关键影响因素,本文采用MIDAS FEA NX软件模拟计算了钢管混凝土的脱空风险系数和脱空高度,并研究了钢管尺寸和混凝土性能对脱空的影响。结果表明:在相同混凝土性能的情况下,钢管直径越小,厚度越大,脱空风险就越大,脱空发生时间也越早,钢管直径越大,脱空高度越大,但在钢管直径相同的情况下,钢管厚度对脱空高度的影响较小;在相同钢管尺寸的情况下,混凝土的自收缩越大,脱空风险越大,脱空发生时间越早;混凝土中掺入膨胀材料可有效降低脱空风险,膨胀峰值越大,峰值时间越晚,抵抗脱空的效果越好;混凝土的绝热温升对脱空的影响较小。研究结果可为钢管混凝土设计、施工质量控制及服役期安全预警提供参考。Abstract: In order to accurately assess the harm of interface voids to the performance of concrete-filled steel tubes, quantify the void risk and clarify its key influencing factors, this paper adopts MIDAS FEA NX software to simulate and calculate the void risk coefficient and void height of concrete-filled steel tubes, and investigates the effects of steel tube dimensions and concrete properties on the occurrence of voids. The results show that under the same concrete properties, the smaller the steel tube diameter and the larger its thickness, the greater the void risk and the earlier the void initiation time. The larger the steel tube diameter, the higher the void height, while the steel tube thickness has a slight effect on the void height for concrete-filled steel tubes with the same diameter. Under the same steel tube dimensions, the greater the autogenous shrinkage of concrete, the higher the void risk and the earlier the void initiation time. Adding an expansive material to concrete can effectively reduce the void risk, and the larger the expansion peak value and the later its peak time, the better the anti-void performance. The adiabatic temperature rise of concrete exerts a minor influence on the generation of voids. The research results can provide a reference for the design, construction quality control and service period safety early warning of CFST structures.
杨睿,徐文.钢管混凝土脱空风险和脱空高度模拟及影响因素研究[J].混凝土与水泥制品,2026,53(5):113-119. YANG R,XU W,et al.Study on void risk, void height simulation and influencing factors of concrete-filled steel tubes[J].China Concrete and Cement Products,2026,53(5):113-119 (in Chinese).

黄 灿a,曹国栋a,*,邓代强b,姜胜强b

摘   要:在混凝土浇筑过程中,钢筋密集区域易发生粗骨料堵塞现象,严重影响浇筑密实度与施工质量。为研究新拌混凝土间隙通过能力及堵塞风险的影响因素,基于离散元法(Discrete element method,DEM)搭建了仿真模型,结合J环试验验证了模型可靠性,探究了粗骨料形状和最大粒径、钢筋间距及混凝土体积对混凝土间隙通过能力与堵塞概率的影响。结果表明:搭建的DEM仿真模型可靠性良好,可有效表征新拌混凝土的间隙通过与堵塞行为;粗骨料形状、最大粒径、钢筋间距及混凝土体积均显著影响堵塞风险,其中,碎石的堵塞概率高于卵石,粗骨料最大粒径越大、钢筋间距越小、混凝土体积越大,堵塞风险越高,当钢筋间距增至90 mm时,无堵塞现象发生;堵塞概率计算结果与试验及仿真规律高度吻合,可为堵塞风险预判提供可靠数值手段。研究成果可通过合理调控相关参数降低钢筋密集区混凝土堵塞风险,为实际浇筑施工质量控制提供理论依据与技术参考。Abstract: During the concrete pouring process, coarse aggregate blockage is prone to occur in areas with dense reinforcement, which seriously affects the pouring compactness and construction quality. To investigate the factors influencing the void-passing capacity and blockage risk of fresh concrete, a simulation model was developed based on the discrete element method (DEM), and the reliability of the model was verified using the J-ring test. The effects of coarse aggregate shape and maximum particle size, reinforcement spacing, and concrete volume on the void-passing capacity and blockage probability were examined.  The results indicate that the developed DEM simulation model is reliable and can effectively characterize the void-passing and blockage behavior of fresh concrete. The shape of coarse aggregate, maximum coarse aggregate size, reinforcement spacing, and concrete volume all significantly influence the risk of blockage. Specifically, crushed stone exhibits a higher probability of blockage than pebble. The risk of blockage increases as the maximum coarse aggregate size increases, reinforcement spacing decreases, and concrete volume increases. When reinforcement spacing is increased to 90 mm, no blockage occurs. The calculated blockage probabilities are in close agreement with experimental and simulation results, providing a reliable numerical method for predicting blockage risks. The research findings can help reduce the risk of concrete blockage in areas with dense reinforcement by appropriately adjusting relevant parameters, thereby providing a theoretical basis and technical reference for quality control in actual concrete pouring operations.
黄灿,曹国栋,邓代强,等.基于离散元法的多因素条件下新拌混凝土堵塞规律研究[J].混凝土与水泥制品,2026,53(5):105-112,119. HUANG C,CAO G D,DENG D Q,et al.Study on blockage law of fresh concrete under multi-factor conditions based on the discrete element method[J].China Concrete and Cement Products,2026,53(5):105-112,119 (in Chinese).
蒋文涛,曹国栋.基于CFD-DEM的混凝土泵送压力损失研究[J].混凝土与水泥制品,2026,53(5):100-104. JIANG W T,CAO G D.Study on concrete pumping pressure loss based on CFD-DEM method[J].China Concrete and Cement Products,2026,53(5):100-104 (in Chinese).
摘   要:水泥基材料是工程结构中至关重要的基础材料之一,其碳化反应是导致结构耐久性能退化的主要机制,而现有相关研究多依托宏观性能指标开展,难以精准表征碳化过程中的三维应变演化规律与细观损伤特征。为此,本文联合X射线微断层成像(X-ray microtomography,X-μCT)与数字体图像相关法(Digital volume correlation,DVC)技术,开展了碳化过程中砂浆试件内部应变分布与裂纹演化的三维定量表征研究,揭示了界面过渡区的应变集中与碳化诱导裂纹张开机制。结果表明:试件在碳化过程中整体表现出持续收缩的特征,而裂缝、孔隙等缺陷区域会出现局部膨胀效应;收缩主要集中于水泥浆体区域,尤其在细骨料与浆体的界面过渡区更为明显,但整体分布未呈现显著方向性规律;碳化会诱导试件出现裂缝张开现象,表明碳化反应不仅导致基体收缩,还可诱发裂纹扩展。研究成果揭示了碳化过程中水泥基材料微观结构与应变场的演化规律,可为理解碳化对材料耐久性能退化的机制提供试验依据,也可为工程结构的寿命预测与耐久性能设计提供参考。Abstract: Cementitious materials are among the most important basic materials in engineering structures, and their carbonation reaction constitutes a primary mechanism leading to structural durability degradation. However, most existing studies are conducted based on macroscopic performance indicators, which makes it difficult to accurately characterize the three-dimensional strain evolution and mesoscopic damage characteristics during carbonation. To address this issue, this study combines X-ray micro-computed tomography (X-μCT) and digital volume correlation (DVC) techniques to conduct three-dimensional quantitative characterization of the internal strain distribution and crack evolution in mortar specimens during carbonation, revealing strain concentration in the interfacial transition zone and the mechanism of carbonation-induced crack opening. The results show that the specimens exhibit continuous overall shrinkage during carbonation, while local expansion effects occur in defective regions such as cracks and pores. Shrinkage is mainly concentrated in the cement paste matrix, particularly in the interfacial transition zone between fine aggregates and the paste, without an obvious directional pattern in the overall distribution. Carbonation can induce crack opening in specimens, indicating that the carbonation reaction not only causes matrix shrinkage, but also promotes crack propagation. The findings reveal the evolution laws of the microstructure and strain field of cementitious materials during carbonation, which can provide 
张冬梅,左晓宝.基于X-μCT与DVC技术的水泥基材料碳化应变定量表征[J].混凝土与水泥制品,2026,53(5):94-99. ZHANG D M,ZUO X B.Quantitative characterization of carbonation-induced strain in cementitious materials using X-μCT and DVC techniques[J].China Concrete and Cement Products,2026,53(5):94-99 (in Chinese).

景 凯1,2,蔡紫阳1,殷旭峰1,倪彤元1,3,*,孔德玉1,3,王时辉2

景凯,蔡紫阳,殷旭峰,等.基于图像分析的改进清水混凝土表面孔洞评价方法[J].混凝土与水泥制品,2026,53(5):88-93,104. JING K,CAI Z Y,YIN X F,et al.Improvement of surface bughole method of fair-faced concrete based on image analysis[J].China Concrete and Cement Products,2026,53(5):88-93,104 (in Chinese).
摘   要:为了揭示透水混凝土力学与透水性能的协同变化规律,并实现对其性能的精准预测与协同设计,本文研究了矿物掺合料总掺量(等质量取代0、20%、25%的水泥)、粉煤灰掺量(0、5%、10%、15%、20%、25%)、硅灰掺量(0、5%、10%、15%、20%、25%)、设计孔隙率(10%、20%)对透水混凝土抗压强度、透水系数的影响,并基于SSA-BP神经网络模型对透水混凝土性能进行了预测。结果表明:掺入矿物掺合料可以有效提高透水混凝土的抗压强度;当矿物掺合料总掺量为25%、硅灰掺量为10%、粉煤灰掺量为15%、设计孔隙率为10%时,透水混凝土的抗压强度最优;当矿物掺合料总掺量相同时,随着硅灰掺量的增加,透水混凝土的透水系数降低;其他条件相同情况下,设计孔隙率增加,透水混凝土的透水系数增加;SSA-BP神经网络模型在透水混凝土性能预测方面精度较高。研究成果可为透水混凝土的研发及应用提供参考。Abstract: In order to reveal the synergistic variation patterns between the mechanical properties and water pervious properties of pervious concrete and to achieve accurate performance prediction and coordinated design, the effects of total mineral admixture content (0, 20%, and 25% replacement of cement by equal mass), fly ash content (0, 5%, 10%, 15%, 20%, 25%), silica fume content (0, 5%, 10%, 15%, 20%, 25%), and design porosity (10%, 20%) on the compressive strength and permeability coefficient of pervious concrete were investigated in this article. Additionally, the performance of pervious concrete was predicted using the SSA-BP neural network model. The results indicate that incorporating mineral admixtures can effectively enhance the compressive strength of pervious concrete. When the total mineral admixture content is 25%, the content of silica fume is 10%, the content of fly ash is 15%, and the design porosity is 10%, the compressive strength of pervious concrete is optimal. At the same total mineral admixture content, the permeability coefficient of pervious concrete decreases as the silica fume content increases. Under identical conditions, an increase in design porosity leads to a higher permeability coefficient. The SSA-BP neural network model demonstrates high accuracy in predicting the performance of pervious concrete. The research results can provide reference for the development and application of pervious concrete.
王卫,陈小华,王冠潮,等.粉煤灰与硅灰对透水混凝土性能的影响及SSA-BP神经网络预测模型研究[J].混凝土与水泥制品,2026,53(5):83-87. WANG W,CHEN X H,WANG G C,et al.Study on the influence of fly ash and silica fume on the properties of pervious concrete and the SSA-BP neural network prediction model[J].China Concrete and Cement Products,2026,53(5):83-87 (in Chinese).