杭美艳,杨午杰,俞柯楠,等.消泡型聚羧酸减水剂对水泥-矿渣复合胶砂性能的影响研究及微观机理分析[J].混凝土与水泥制品,2026,53(7):1-5,11. Hang Meiyan,Yang Wujie,Yu Kenan,et al.Effects of defoaming-type polycarboxylate superplasticizer on performance of cement-slag composite mortar and its microscopic mechanism[J].China Concrete and Cement Products,2026,53(7):1-5,11 (in Chinese).

陈俊松,王 伟,蔡景顺,曾鲁平,赵 爽,朱伯淞,刘光严

摘   要:富水隧道长期处于高水压、高离子侵蚀的复杂水环境中,初期支护喷射混凝土易遭受地下水持续作用引发钙溶蚀、硫酸盐侵蚀等多重劣化效应,严重威胁隧道结构长期安全服役。为了提升富水隧道环境下初支喷射混凝土的抗钙溶蚀与抗硫酸盐侵蚀性能,本文研究了不同掺量(20、30、40 kg/m3)疏水性侵蚀抑制剂(TIA)对喷射混凝土抗压强度、Ca2+溶出量、吸水率、抗氯离子迁移系数、接触角、抗压强度耐蚀系数的影响。结果表明:加速溶蚀条件下,掺TIA组试件1~7 d的抗压强度相较于JZ(基准)组并没有大幅提高或降低,14 d、28 d的抗压强度仍然保持缓慢增长,抗压强度损失率基本不变;TIA的掺入可以显著降低试件的Ca2+溶出量,降低吸水率与氯离子迁移系数,增大接触角;TIA的掺入可以有效提升试件的抗硫酸盐侵蚀性能。研究成果可为喷射混凝土耐久性能的提升及地下工程结构的安全服役提供参考。Abstract: Water-rich tunnels are long-term exposed to a complex water environment with high water pressure and severe ion erosion. The shotcrete used for primary support is prone to various deterioration effects caused by continuous groundwater action, such as calcium leaching and sulfate attack, which seriously threatens the long-term safety of tunnel structures. To improve the resistance of initial-support shotcrete to calcium leaching and sulfate attack in water-rich tunnel environments, this study investigated the effects of a hydrophobic erosion inhibitor (TIA) at different dosages (20, 30, and 40 kg/m3) on compressive strength, Ca2+ leaching amount, water absorption, chloride ion migration coefficient, contact angle, and corrosion resistance coefficient of compressive strength of shotcrete. The results show that under accelerated leaching conditions, the compressive strength of specimens incorporating TIA at 1 to 7 days does not significantly increase or decrease compared to the JZ (reference) group. The compressive strength continues to grow slowly at 14 and 28 days, and the compressive strength loss rate remains basically unchanged. The addition of TIA can significantly reduce the Ca2+ leaching amount, water absorption and chloride ion migration coefficient of specimens, and increase the contact angle. Meanwhile, the incorporation of TIA can effectively improve the sulfate attack resistance of specimens. The findings can provide a reference for enhancing the durability of shotcrete and the safe service of underground engineering structures.
陈俊松,王伟,蔡景顺,等.疏水性侵蚀抑制剂对喷射混凝土抗钙溶蚀及抗硫酸盐侵蚀性能的影响[J].混凝土与水泥制品,2026,53(7):6-11. Chen Junsong,Wang Wei,Cai Jingshun,et al.Effects of hydrophobic erosion inhibitor on calcium leaching resistance and sulfate attack resistance of shotcrete[J].China Concrete and Cement Products,2026,53(7):6-11 (in Chinese).

许艺煌1,夏红岩2,*,牛恩宽2,张莉亚2

许艺煌,夏红岩,牛恩宽,等.阵列式冲击回波法在水下混凝土结构内部缺陷检测中的应用[J].混凝土与水泥制品,2026,53(7):150-155. Xu Yihuang,Xia Hongyan,Niu Enkuan,et al.Application of array-based impact-echo method in internal defect detection of underwater concrete structures[J].China Concrete and Cement Products,2026,53(7):150-155 (in Chinese).

李 翔1,王希浩1,宁方端1,刘洪超2,金祖权2,王鹏刚2,*

摘   要:海洋重大基础设施中大体积混凝土易因早期收缩产生有害裂缝,严重影响结构服役安全与使用寿命,为解决某海底隧道明挖段侧墙大体积混凝土温差收缩开裂难题,本文设计了掺钙镁复合型抗裂剂的抗裂混凝土,研究了其力学及耐久性能,并采用“水化-温度-湿度-约束”多场耦合收缩模型,探究了大体积混凝土的裂缝控制技术,分析了抗裂剂、浇筑长度、入模温度及冷却措施对混凝土开裂风险的影响规律。结果表明:抗裂混凝土的力学性能和抗氯离子渗透性能均满足工程要求,且具有较好的抗碳化性能;掺入钙镁复合型抗裂剂可显著降低侧墙混凝土的开裂风险;缩短分段浇筑长度、降低入模温度、布设冷却水管可进一步优化温控防裂效果。工程实践表明,通过原材料质量管控、配合比优化、施工工艺调整等措施,可有效解决侧墙大体积混凝土的早期收缩开裂问题,浇筑成型后的侧墙结构密实,表面无明显裂缝。研究成果可为滨海同类隧道大体积混凝土温控防裂、施工优化及质量管控提供参考。Abstract: Mass concrete applied in major marine infrastructure is prone to harmful cracks induced by early-age shrinkage, which seriously threatens structural safety and service life. To address the problem of temperature and shrinkage cracking of mass concrete in the open-cut sidewalls of an undersea tunnel, this paper develops a crack-resistant concrete containing a calcium-magnesium composite anti-cracking agent. The mechanical properties and durability of the concrete are tested. Based on the hydration-temperature-humidity-constraint multi-field coupled shrinkage model, crack control technologies for mass concrete are investigated, and the influence of anti-cracking agent, pouring length, placing temperature and cooling measures on the cracking risk of concrete is analyzed. The results show that the mechanical properties, chloride penetration resistance and carbonation resistance of the developed crack-resistant concrete fully meet the engineering requirements. The addition of calcium-magnesium composite anti-cracking agent can significantly reduce the cracking risk of sidewall concrete. Reducing the pouring length, lowering the placing temperature and installing cooling water pipes can further improve temperature-control and crack-prevention effects. Engineering practice verifies that comprehensive measures including raw material quality control, mix proportion optimization and construction technology adjustment can effectively eliminate early-age shrinkage cracking of mass concrete for sidewalls. The cast sidewall structures feature dense interiors and crack-free surfaces. The findings can provide a reference for temperature control, crack prevention, construction optimization and quality control of mass concrete in similar coastal tunnel projects.
李翔,王希浩,宁方端,等.明挖现浇侧墙大体积混凝土裂缝防控技术研究与工程应用[J].混凝土与水泥制品,2026,53(7):134-139,144. Li Xiang,Wang Xihao,Ning Fangduan,et al.Research on crack control technology for mass concrete in open-cut cast-in-place sidewalls and its engineering application[J].China Concrete and Cement Products,2026,53(7):134-139,144 (in Chinese).

叶胜利1,眭素刚1,2,*,曹邑泽1,成 立1

摘   要:为提高沿海地区钢筋混凝土结构的防腐蚀性能,以山东日照某钢铁精品基地工程为背景,分析了钢筋混凝土腐蚀原理,检测了该工程水土条件的腐蚀性能,设计并优选了混凝土的最佳水胶比,提出了钢筋混凝土防腐建议。结果表明:沿海地区钢筋混凝土在干湿循环条件下最容易腐蚀;C30、C35、C40混凝土的最佳水胶比分别为0.402、0.378、0.354;建议通过增加混凝土保护层厚度、适当掺入阻锈剂或矿物掺合料、设置垫层、提高混凝土强度等级、重视浇筑及养护工序来提高钢筋混凝土的防腐蚀性能。Abstract: To improve the corrosion resistance of reinforced concrete structures serving in coastal environments, based on a high-quality steel base project in Rizhao, Shandong, the corrosion mechanism of reinforced concrete was analyzed, and the corrosive characteristics of on-site groundwater and soil in the project were evaluated. The optimal water-binder ratio for concrete was designed and optimized, and corrosion resistance suggestions for reinforced concrete were proposed. The results indicate that reinforced concrete in coastal areas is most vulnerable to corrosion under dry-wet cycling conditions. The optimal water-binder ratios for C30, C35, and C40 concrete are 0.402, 0.378, and 0.354, respectively. To enhance corrosion resistance of reinforced concrete, it is recommended to increase the concrete cover for protecting reinforcement, incorporate suitable corrosion inhibitors or mineral admixtures, provide a protective bedding layer, use higher-grade concrete, and ensure strict control over casting and curing procedures.
叶胜利,眭素刚,曹邑泽,等.沿海地区钢筋混凝土结构的防腐蚀性能研究及对策[J].混凝土与水泥制品,2026,53(7):140-144. Ye Shengli,Sui Sugang,Cao Yize,et al.Research and countermeasures on corrosion resistance of reinforced concrete structures in coastal areas[J].China Concrete and Cement Products,2026,53(7):140-144 (in Chinese).

丁 健1,邓学民1,郑少鑫1,朱泽乾1,刘郑琦2,张 坚3,杨 睿3,徐 文3,*

丁健,邓学民,郑少鑫,等.高速铁路无砟轨道道床板混凝土抗裂技术研究与应用[J].混凝土与水泥制品,2026,53(7):145-149,155. Ding Jian,Deng Xuemin,Zheng Shaoxin,et al.The application of anti-cracking technology for ballastless track bed slab concrete of high-speed railway[J].China Concrete and Cement Products,2026,53(7):145-149,155 (in Chinese).