全部文章
绿色低碳与环保利废
孟 可1,童建勇2,张 傲3,钟 茜4,魏 洋5,*,杨 航5
摘 要:为明晰高掺量及不同细度下石灰石粉对水泥基材料水化热与抗压强度的作用机理,本文研究了石灰石粉掺量(0、10%、15%、20%、25%)与细度(比表面积为408、537、649 m2/kg)对胶凝体系水化热、砂浆及混凝土抗压强度的影响,并揭示了胶凝体系水化热与水泥基材料力学性能之间的关联。结果表明:随着石灰石粉掺量的增加,胶凝体系的水化放热量降低,水化诱导期缩短,第二水化放热峰峰值减小,砂浆1 d、3 d及混凝土28 d抗压强度均降低;随着石灰石粉比表面积的增大,胶凝体系水化放热量先减后增,第二放热峰出现时间先延迟后提前,第二水化放热峰峰值先降后升,砂浆1 d、3 d及混凝土28 d抗压强度均提高;胶凝体系水化放热量与砂浆早期抗压强度的相关性受石灰石粉掺量与细度共同调控;综合考虑胶凝体系水化放热特性与水泥基材料力学性能,石灰石粉的最佳掺量为20%、最佳比表面积为649 m2/kg,此时砂浆3 d 抗压强度为35.4 MPa,混凝土28 d 抗压强度为45.7 MPa。研究成果可为高掺量石灰石粉低碳水泥基材料的工程应用与性能优化提供参考。Abstract: To clarify the mechanism of limestone powder with high content and different fineness affecting the hydration heat and compressive strength of cement-based materials, this study investigated the effects of limestone powder content (0, 10%, 15%, 20%, and 25%) and fineness (specific surface areas of 408, 537, and 649 m2/kg) on the hydration heat of the cementitious system as well as the compressive strength of mortar and concrete, and revealed the correlation between the hydration heat of the cementitious system and the mechanical properties of cement-based materials. The results show that with the increase of limestone powder content, the hydration heat of cementitious system decreases, the hydration induction period is shortened, and the intensity of the second hydration exothermic peak decreases, accompanied by the reduction in 1-day and 3-day compressive strength of mortar and 28-day compressive strength of concrete. As the specific surface area of limestone powder increases, the hydration heat firstly decreases and then increases, the occurrence time of the second exothermic peak is delayed initially and advanced subsequently, and its peak intensity first decreases and then increases, while the 1-day and 3-day compressive strength of mortar and 28-day compressive strength of concrete are all improved. The correlation between hydration heat of the cementitious system and the early compressive strength of mortar is jointly regulated by the content and fineness of limestone powder. Considering comprehensively the hydration heat characteristics of cementitious system and mechanical properties of cement-based materials, the optimal content of limestone powder is 20% with the specific surface area of 649 m2/kg. Under this condition, the 3-day compressive strength of mortar reaches 35.4 MPa and the 28-day compressive strength of concrete is 45.7 MPa. The research findings can provide reference for the engineering application and performance optimization of low-carbon cement-based materials blended with high-content limestone powder.
孟可,童建勇,张傲,等.石灰石粉掺量与细度对水泥基材料水化特性及力学性能的影响[J].混凝土与水泥制品,2026,53(7):93-99. Meng Ke,Tong Jianyong,Zhang Ao,et al.Effects of content and fineness of limestone powder on hydration characteristics and mechanical properties of cement-based materials[J].China Concrete and Cement Products,2026,53(7):93-99 (in Chinese).
马川义1,薛兴杰2,杨 帅3,邵滢璇 2,吕晶晶2,*,葛 智2,张洪智2
摘 要:为实现粉煤灰(Fly ash,FA)与电石渣(Calcium carbide residue,CS)固废协同资源化及CO2矿化封存,通过湿法矿化法用CS对FA进行了改性,制备得到了CFA-CS复合粉体,研究了原状FA、CFA-CS掺量(20%、30%、40%、50%)对净浆凝结时间、收缩性能、水化程度的影响,并进行了微观分析。结果表明:经矿化改性后,CFA-CS的比表面积提升了23.2%,粒径≤20 μm的颗粒占比增大,表面富集团簇状CaCO3晶体,颗粒粗糙度较高;随着原状FA掺量的增加,净浆的初、终凝时间延长,而提高CFA-CS掺量则基本缩短了净浆的初、终凝时间;随着原状FA、CFA-CS掺量的增加,净浆的7 d化学收缩值、自收缩值均减小,各龄期非蒸发水含量均降低;在相同掺量下,掺CFA-CS净浆的凝结时间、化学收缩值与自收缩值均低于掺原状FA净浆,而非蒸发水含量显著高于掺原状FA净浆;原状FA体系中生成了单硫酸盐Ms,易加剧基体收缩;CFA-CS体系中未生成Ms,但生成大量的单碳酸盐Mc、半碳酸盐Hc及AFt,优化了浆体微观结构与密实度。研究成果可为FA-CS固废协同矿化低碳胶凝材料的开发、水泥基材料体积稳定性调控及固废碳封存资源化利用提供理论依据。Abstract: To realize the synergistic resource utilization of fly ash (FA) and calcium carbide residue (CS) solid wastes, as well as CO2 mineralization and sequestration, FA was modified with CS via the wet mineralization method to prepare CFA-CS composite powder. The effects of raw FA and CFA-CS content (20%, 30%, 40% and 50%) on the setting time, shrinkage behavior and hydration degrees of cement paste were investigated, and microscopic analysis was also conducted. The results show that after mineralization modification, the specific surface area of CFA-CS increases by 23.2%, the proportion of particles with size ≤20 μm rises, and the particle surface is enriched with clustered CaCO3 crystals with higher particle roughness. With the increase of raw FA content, the initial and final setting time of paste is prolonged, while increasing the content of CFA-CS basically shortens the initial and final setting time of paste. The 7-day chemical shrinkage and autogenous shrinkage values of paste decrease, and the non-evaporable water content at each curing age declines with increasing content of both raw FA and CFA-CS. At the same replacement level, paste blended with CFA-CS exhibits shorter setting time, chemical shrinkage and autogenous shrinkage, but significantly higher non-evaporable water content than that blended with raw FA. Monosulphate (Ms) is formed in the raw FA system, which tends to aggravate the matrix shrinkage. No Ms is generated in the CFA-CS system, instead, more monocarbonate (Mc), hemicarbonate (Hc) and AFt are generated, which optimizes the microstructure and compactness of the paste. The research findings can provide a theoretical basis for the development of low-carbon cementitious materials based on synergistically mineralized FA-CS solid wastes, the regulation of volume stability of cement-based materials, and solid waste resource utilization coupled with carbon sequestration.
马川义,薛兴杰,杨帅,等.粉煤灰-电石渣CO2协同矿化改性及其对复合浆体收缩及水化性能的影响[J].混凝土与水泥制品,2026,53(7):100-105. Ma Chuanyi,Xue Xingjie,Yang Shuai,et al.Synergistic CO2 mineralization modification of fly ash and calcium carbide residue and its effect on shrinkage and hydration behavior of composite paste[J].China Concrete and Cement Products,2026,53(7):100-105 (in Chinese).
郑俊峰,熊 燕,殷晓明,丁 涛
郑俊峰,熊燕,殷晓明,等.矿物掺合料-无碱速凝剂协同调控改善喷射混凝土性能研究[J].混凝土与水泥制品,2026,53(7):106-111,133. Zheng Junfeng,Xiong Yan,Yin Xiaoming,et al.Study on the synergistic regulation of mineral admixtures and alkali-free accelerator for enhancing shotcrete performance[J].China Concrete and Cement Products,2026,53(7):106-111,133 (in Chinese).
摘 要:针对钢渣活性低、易磨性差,传统试错法优化胶凝材料配合比效率低、精度不足的问题,本文采用物理粉磨与化学激发协同改性技术来提升钢渣的活性,系统研究了钢渣研磨时间(50、70、90、110 min)、钢渣与矿渣的质量比(以下简称钢矿比,0.07、0.22、0.42、0.73、1.16、1.88)以及激发剂单掺、复掺对复合胶凝材料力学性能的影响,并确定了最优试验参数;基于此,构建了GA-BP神经网络模型,评价了各龄期抗压强度模型预测精度与泛化能力,并依托模型对复合胶凝材料的配合比进行了优化。结果表明:钢渣的最优研磨时间为90 min,最佳钢矿比为0.73,NaOH为本体系最优激发剂;各龄期抗压强度预测模型的拟合优度均高于0.83,模型整体预测精度与泛化性能良好;各龄期抗压强度预测模型精度由高到低依次为7 d、3 d、28 d抗压强度模型;经模型优化得到的最优配合比(质量分数)为钢渣27.18%、矿渣61.29%、脱硫石膏11.53%、NaOH 3.47%、水胶比0.5、胶砂比1∶3。该配合比下,复合胶凝材料各龄期抗压强度预测值与实测值相对误差均低于3.1%,实现了固废基胶凝材料配合比高效精准优化。该研究成果可为钢渣无害化、资源化高效利用及固废基胶凝材料的配合比智能优化提供参考。Abstract: To address the issues of low reactivity and poor grindability of steel slag, and the low efficiency and insufficient accuracy of traditional trial-and-error methods for optimizing the mix proportions of cementitious materials, this paper employs a synergistic modification technology combining physical grinding and chemical activation to improve the activity of steel slag. The effects of steel slag grinding time (50, 70, 90, 110 min), the mass ratio of steel slag to slag (hereinafter referred to as the steel slag-to-slag ratio: 0.07, 0.22, 0.42, 0.73, 1.16, 1.88), and the single or compound addition of activators on the mechanical properties of the composite cementitious materials were systematically investigated, and the optimal experimental parameters were determined. Based on this, a GA-BP neural network model was established to evaluate the prediction accuracy and generalization ability of the compressive strength models at various ages, and the mix proportion of the composite cementitious materials was optimized based on the model. The results indicate that the optimal grinding time for steel slag is 90 min, the optimal steel slag-slag ratio is 0.73, and NaOH is the optimal activator for this system. The goodness of fit for the compressive strength prediction models at each age exceeds 0.83, indicating good overall prediction accuracy and generalization performance. The prediction accuracy of compressive strength models at various ages ranks in descending order of 7 d, 3 d, and 28 d. The optimal mix proportion (mass fraction) obtained via model optimization is as follows: 27.18% steel slag, 61.29% slag, 11.53% desulfurization gypsum, 3.47% NaOH, water-binder ratio of 0.5, and binder-sand ratio of 1∶3. Under this mix proportion, the relative errors between predicted and measured compressive strengths at all curing ages are less than 3.1%, realizing an efficient and precise optimization of mix proportions for solid waste-based cementitious materials. The research findings can provide a reference for the harmless treatment, high-value resource utilization of steel slag, and intelligent mix proportion optimization of solid waste-based cementitious materials.
刘文艳.钢渣-矿渣复合胶凝材料物理-化学协同活化机制及基于GA-BP的配合比优化[J].混凝土与水泥制品,2026,53(7):112-119. Liu Wenyan.Physicochemical synergistic activation mechanism of steel slag-slag composite cementitious materials and mix proportion optimization based on GA-BP[J].China Concrete and Cement Products,2026,53(7):112-119 (in Chinese).
摘 要:为研发兼具轻质、耐火协同性能的混凝土,本文分别用粉煤灰微珠(Fly ash microsphere,FAM)、矿渣粉(Ground granulated blast furnace slag,GGBS)和硅灰等体积取代河砂、等质量取代水泥制备轻质混凝土,系统研究了FAM掺量(0、50%、75%、100%)、GGBS掺量(0、10%、20%、30%、40%)及硅灰掺量和掺入方式对轻质混凝土干密度、力学性能、导热系数与耐火性能的影响。结果表明:随着FAM掺量的增加,轻质混凝土的干密度、抗压强度、劈裂抗拉强度及导热系数呈下降趋势,试件的高温表观完整性与耐火隔热时长明显提升,当FAM掺量为100%时,轻质混凝土的干密度为1 142.8 kg/m3,90 d抗压、劈裂抗拉强度分别为33.8、2.51 MPa,导热系数为0.383 W/(m·K),耐火隔热时长为232 min;用10%硅灰等质量取代水泥可有效提升轻质混凝土的力学性能与导热系数,但会小幅缩短耐火隔热时长;随着GGBS掺量的增加,轻质混凝土的力学性能先增后降,导热系数逐步上升,耐火隔热时长持续缩短,20%为GGBS最优掺量;复掺硅灰、GGBS组试件的耐火隔热时长均超过3 h,满足相关标准要求。该研究成果可为FAM基高性能轻质混凝土的性能优化及在高防火要求建筑构件中的工程应用提供参考。Abstract: To develop concrete with lightweight and fire resistance performance, river sand was partially replaced with an equal volume of fly ash microspheres (FAM), while cement was partially replaced with an equal mass of ground granulated blast furnace slag (GGBS) and silica fume, to prepare lightweight concrete in this study. The effects of FAM content (0, 50%, 75%, 100%), GGBS content (0, 10%, 20%, 30%, 40%), as well as silica fume content and mixing methods on the dry density, mechanical properties, thermal conductivity and fire resistance performance of lightweight concrete were systematically investigated. The results show that with the increase of FAM content, the dry density, compressive strength, splitting tensile strength and thermal conductivity of lightweight concrete all decrease, while the high-temperature surface integrity and fire insulation duration of specimens are significantly improved. When the FAM content is 100%, the dry density of lightweight concrete is 1 142.8 kg/m3, the 90-day compressive strength and splitting tensile strength are 33.8 MPa and 2.51 MPa, respectively. And the thermal conductivity is 0.383 W/(m·K), and the fire insulation duration is 232 min. Replacing cement with 10% silica fume by mass effectively improves the mechanical properties and thermal conductivity of lightweight concrete, but slightly shortens the fire insulation duration. With the increase of GGBS content, the mechanical properties of lightweight concrete first increase and then decrease, the thermal conductivity rises gradually, and the fire insulation duration decreases continuously, with 20% being the optimal GGBS content. The fire insulation duration of specimens mixed with silica fume and GGBS all exceeds 3 hours, meeting the requirements of relevant standards. The research results can provide a reference for the performance optimization of FAM-based high-performance lightweight concrete and its engineering application in building components with high fire protection requirements.
胡光林.粉煤灰微珠轻质混凝土力学与热工性能研究[J].混凝土与水泥制品,2026,53(7):120-125. Hu Guanglin.Study on mechanical and thermal properties of fly ash microsphere lightweight concrete[J].China Concrete and Cement Products,2026,53(7):120-125 (in Chinese).
摘 要:为制备绿色低碳、低收缩的碱激发胶凝材料,以矿粉、粉煤灰为原材料,碳酸钠与硅酸钠为碱性激发剂,通过正交试验研究了粉煤灰掺量(A)、硅酸钠掺量(B)、碳酸钠掺量(C)对碱激发胶凝材料凝结时间、抗压强度与干燥收缩的影响,并结合水化热、XRD、SEM揭示微观作用机理。结果表明:JD1、JD2、JD4、JD5、JD7组初凝时间满足相关标准要求;各因素对碱激发胶凝材料初、终凝时间影响程度排序均为B>A>C,对3 d抗压强度影响程度排序为B>A>C,对28 d抗压强度影响程度排序为C>A>B,对90 d干燥收缩值影响程度排序为B>C>A;综合性能优选出较优配合比为A2B1C2(粉煤灰20%、硅酸钠4%、碳酸钠8%);硅酸钠激发体系的水化速率更快、第二放热峰出现时间更早,对凝结时间与3 d抗压强度作用更显著;碳酸钠激发体系后期水化更充分、结构更致密,对28 d抗压强度影响显著。该研究成果可为低收缩、高性能碱激发胶凝材料的制备与工程应用提供理论依据。Abstract: To prepare green, low-carbon, and low-shrinkage alkali-activated cementitious materials, mineral powder and fly ash were used as raw materials, while sodium carbonate and sodium silicate as alkaline activators. Orthogonal tests were conducted to investigate the effects of fly ash content (A), sodium silicate content (B) and sodium carbonate content (C) on the setting time, compressive strength, and drying shrinkage of alkali-activated cementitious materials. Hydration heat analysis, XRD and SEM were employed to reveal the microscopic mechanism. The results show that the initial setting times of groups JD1, JD2, JD4, JD5 and JD7 meet the relevant standard requirements. The influence sensitivity ranking for initial and final setting time follows B>A>C, for the 3-day compressive strength is B>A>C, for the 28-day compressive strength is C>A>B, and for the 90-day drying shrinkage value is B>C>A. The optimal mix proportion based on comprehensive performance is A2B1C2 (fly ash 20%, sodium silicate 4%, sodium carbonate 8%). The sodium silicate-activated system exhibits a faster hydration rate and an earlier occurrence of the second exothermic peak, exerting a significant influence on the setting time and 3-day compressive strength. The sodium carbonate-activated system presents more sufficient later hydration and a denser microstructure, showing a remarkable effect on the 28-day compressive strength. The research findings can provide a theoretical basis for the preparation and engineering application of high-performance and low-shrinkage alkali-activated cementitious materials.
秦节发.碱激发胶凝材料配合比优化及微观机理分析[J].混凝土与水泥制品,2026,53(7):126-133. Qin Jiefa.Mix proportion optimization and microscopic mechanism analysis of alkali-activated cementitious materials[J].China Concrete and Cement Products,2026,53(7):126-133 (in Chinese).