基于正交试验的水泥基自流平砂浆流动度研究
Study on flowability of cementitious self-levelling mortar based on orthogonal experiment
2025年第3期
正交试验;水泥基自流平砂浆;配合比;流动度;减水剂;羟丙基甲基纤维素醚
Orthogonal experiment; Cementitious self-levelling mortar; Mix proportion; Flowability; Water reducing agent; Hydroxypropyl methyl cellulose ether
2025年第3期
10.19761/j.1000-4637.2025.03.073.04
杨 萍,刘 洋,张阿瑶,华靖文*
陕西凝远新材料科技股份有限公司,陕西 西安712034

杨 萍,刘 洋,张阿瑶,华靖文*

杨萍,刘洋,张阿瑶,等.基于正交试验的水泥基自流平砂浆流动度研究[J].混凝土与水泥制品,2025(3):73-76.

YANG P,LIU Y,ZHANG A Y,et al.Study on flowability of cementitious self-levelling mortar based on orthogonal experiment[J].China Concrete and Cement Products,2025(3):73-76.

浏览量:
1000
摘   要:通过正交试验研究了减水剂用量(2.1~2.5 g)、羟丙基甲基纤维素醚(HPMC)用量(0.8~1.2 g)、不同粒径(0.08~0.30 mm、0.30~0.60 mm)砂用量对水泥基自流平砂浆流动度的影响。结果表明:HPMC用量对水泥基自流平砂浆流动度的影响最大,其次为减水剂用量,最后为不同粒径砂用量;优化后的水泥基自流平砂浆配合比组合为减水剂用量2.3 g、HPMC用量1.0 g、粒径0.08~0.30 mm砂用量460 g、不掺粒径0.30~0.60 mm砂,其初始、20 min流动度分别为151 mm、134 mm,满足相关标准要求。 Abstract: The effects of water reducing agent dosage (2.1~2.5 g), hydroxypropyl methyl cellulose ether (HPMC) dosage (0.8~1.2 g), and sand dosage with different particle sizes(0.08~0.30 mm, 0.30~0.60 mm) on the flowability of cementitious self-levelling mortar were investigated through orthogonal experiments. The results show that the HPMC dosage has the most significant impact on the flowability, followed by the water reducing agent dosage, and lastly the sand dosage with different particle sizes. The optimized mix proportion of cementitious self-levelling mortar is 2.3 g of water reducing agent, 1.0 g of HPMC, 460 g of sand with particle size of 0.08~0.30 mm, and no sand with particle size of 0.30~0.60 mm. Under those conditions, the initial and 20 min flowability are 151 mm and 134 mm, respectively, which meets the requirements of the relevant standard.
英文名 : Study on flowability of cementitious self-levelling mortar based on orthogonal experiment
刊期 : 2025年第3期
关键词 : 正交试验;水泥基自流平砂浆;配合比;流动度;减水剂;羟丙基甲基纤维素醚
Key words : Orthogonal experiment; Cementitious self-levelling mortar; Mix proportion; Flowability; Water reducing agent; Hydroxypropyl methyl cellulose ether
刊期 : 2025年第3期
DOI : 10.19761/j.1000-4637.2025.03.073.04
文章编号 :
基金项目 :
作者 : 杨 萍,刘 洋,张阿瑶,华靖文*
单位 : 陕西凝远新材料科技股份有限公司,陕西 西安712034

杨 萍,刘 洋,张阿瑶,华靖文*

杨萍,刘洋,张阿瑶,等.基于正交试验的水泥基自流平砂浆流动度研究[J].混凝土与水泥制品,2025(3):73-76.

YANG P,LIU Y,ZHANG A Y,et al.Study on flowability of cementitious self-levelling mortar based on orthogonal experiment[J].China Concrete and Cement Products,2025(3):73-76.

摘要
参数
结论
参考文献
引用本文

摘   要:通过正交试验研究了减水剂用量(2.1~2.5 g)、羟丙基甲基纤维素醚(HPMC)用量(0.8~1.2 g)、不同粒径(0.08~0.30 mm、0.30~0.60 mm)砂用量对水泥基自流平砂浆流动度的影响。结果表明:HPMC用量对水泥基自流平砂浆流动度的影响最大,其次为减水剂用量,最后为不同粒径砂用量;优化后的水泥基自流平砂浆配合比组合为减水剂用量2.3 g、HPMC用量1.0 g、粒径0.08~0.30 mm砂用量460 g、不掺粒径0.30~0.60 mm砂,其初始、20 min流动度分别为151 mm、134 mm,满足相关标准要求。

Abstract: The effects of water reducing agent dosage (2.1~2.5 g), hydroxypropyl methyl cellulose ether (HPMC) dosage (0.8~1.2 g), and sand dosage with different particle sizes(0.08~0.30 mm, 0.30~0.60 mm) on the flowability of cementitious self-levelling mortar were investigated through orthogonal experiments. The results show that the HPMC dosage has the most significant impact on the flowability, followed by the water reducing agent dosage, and lastly the sand dosage with different particle sizes. The optimized mix proportion of cementitious self-levelling mortar is 2.3 g of water reducing agent, 1.0 g of HPMC, 460 g of sand with particle size of 0.08~0.30 mm, and no sand with particle size of 0.30~0.60 mm. Under those conditions, the initial and 20 min flowability are 151 mm and 134 mm, respectively, which meets the requirements of the relevant standard.

关键词:
the
mm
用量
of
0.30
dosage
hpmc
and
0.60
扫二维码用手机看
未找到相应参数组,请于后台属性模板中添加

(1)各因素对水泥基自流平砂浆初始和20 min流动度的影响主次顺序均为:HPMC用量B>减水剂用量A>不同粒径砂用量C。
(2)随着减水剂用量的增加,水泥基自流平砂浆的初始和20 min流动度均先增大后减小。
(3)随着HPMC用量的减少,水泥基自流平砂浆的初始和20 min流动度均增大。HPMC用量过低易出现泌水现象,过高则会降低流动度,实际应用时,需根据工程情况确定合适的HPMC用量。
(4)随着粒径0.30~0.60 mm砂用量的增加,即粒径0.08~0.30 mm砂用量减少,水泥基自流平砂浆的初始、20 min流动度均呈先下降后趋于平缓的趋势。选用合适的砂颗粒级配能使水泥基自流平砂浆具有良好的流动度。
(5)优化后的水泥基自流平砂浆的配合比组合为A2B2C1,即减水剂用量2.3 g、HPMC用量1.0 g、粒径0.08~0.30 mm砂用量460 g、不掺粒径0.30~0.60 mm砂,其初始、20 min流动度分别为151 mm、134 mm,满足JC/T 985—2017要求。

[1] 中华人民共和国工业和信息化部.地面用水泥基自流平砂浆:JC/T 985—2017[S].北京:建材工业出版社,2017.
[2] 逄鲁峰,黄凌苗,杜诗寒,等.自制悬浮稳定剂对水泥基自流平砂浆性能的影响[J].混凝土与水泥制品,2023(4):14-17.
[3] 戴浩,宋旭艳,孔俊俊,等.脱硫石膏基与磷石膏基自流平砂浆的性能差异研究[J].混凝土与水泥制品,2024(8):91-96.
[4] ONISHI K,BIER T A.Investigation into relations among technological properties, hydration kinetics and early age hydration of self-leveling underlayments[J].Cement and Concrete Research,2010,40(7):1034-1040.
[5] 戴浩,张树鹏,琚诚兰,等.复合水泥基自流平材料的研究进展[J].材料导报,2015,29(21):103-106.
[6] 逄鲁峰,贾广贺,孙立刚.石膏基自流平砂浆流动性研究与应用[J].混凝土与水泥制品,2023(7):31-34,38.
[7] 周文娟,周丹.添加剂对自流平砂浆流变性能和力学性能的影响研究[J].北京建筑大学学报,2015,31(3):23-26.
[8] 侯云芬,郑东昊,周文娟.再生细骨料级配对自流平砂浆强度的影响[J].混凝土与水泥制品,2019(7):96-100.
[9] 沈嫣秋.砂的颗粒级配对自流平砂浆性能的影响[J].低温建筑技术,2012,34(4):20-21.
[10] 王栋民,张琳.干混砂浆原理与配方指南[M].北京:化学工业出版社,2010.
[11] 张建隽,靳秀芝,韩涛,等.自流平砂浆流动性的影响因素研究[J].中北大学学报(自然科学版),2014,35(5):620-624.
[12] 张彬,贺鸿珠,钟世云.纤维素醚在水泥砂浆中的作用机理及影响因素[J].上海建材,2008(3):32-34.
[13] 范帅鹏,袁琦,何小芳.外加剂对水泥基自流平砂浆流动性和力学性能的影响[J].砖瓦,2020(9):93-95,97.
[14] 张明涛,王泽萍,唐晗,等.纤维素醚对石膏基自流平砂浆性能的影响研究[J].混凝土与水泥制品,2024(11):70-74.
[15] 彭家惠,董素芬,黄智德.水泥基自流平砂浆流动性与保水性的试验研究[J].混凝土与水泥制品,2009(1):4-6,19.

杨萍,刘洋,张阿瑶,.基于正交试验的水泥基自流平砂浆流动度研究[J].混凝土与水泥制品,2025(3):73-76.

YANG P,LIU Y,ZHANG A Y,et al.Study on flowability of cementitious self-levelling mortar based on orthogonal experiment[J].China Concrete and Cement Products,2025(3):73-76.

相关文件

暂时没有内容信息显示
请先在网站后台添加数据记录。

关注《混凝土与水泥制品》

总访问量 468,401   网站统计

官方微信公众号关闭
苏州混凝土水泥制品研究院有限公司

关于我们    |    联系我们    |    订购杂志    |    回到顶部

版权所有:中国混凝土与水泥制品网  苏ICP备10086386号   网站建设:中企动力 苏州

版权所有:中国混凝土与水泥制品网

苏ICP备10086386号

网站建设:中企动力 苏州