混凝土基础理论
刘长顺1,2,3,邢朝阳1,2,甘保柱1,张成银1,张景奎2
摘 要:混凝土碳化是影响钢筋混凝土结构耐久性能的关键因素之一,而养护条件、试件类型、表面状态等边界条件对混凝土加速碳化试验结果存在显著影响。本文选取了三种典型粗骨料级配(工地实际、建筑优化、水利优化),研究了养护条件(标准养护与自然养护)、试件类型(标准试件与芯样试件)和试件面层材料(水泥浆面层、混凝土面层、防护面层、既有碳化面层)对混凝土加速碳化试验结果的影响,建立了不同边界条件下碳化深度之间的定量关系。结果表明:自然养护试件的各龄期碳化深度均大于相应标准养护试件;标准试件各龄期的碳化深度均大于芯样试件;防护面层试件的抗碳化性能最优,混凝土面层试件28 d碳化深度较大;相同碳化龄期下,初始阶段试件自然碳化深度越小,加速碳化试验后的碳化深度也越小,混凝土面层试件相较于既有碳化面层试件的28 d碳化深度大;三种粗骨料级配混凝土在不同边界条件下的抗碳化性能排序保持一致,均为工地实际组>建筑优化组>水利优化组。研究成果可为以试验室加速碳化试验结果评估实际工程混凝土的抗碳化性能提供理论依据。Abstract: Concrete carbonation is one of the key factors affecting the durability of reinforced concrete structures. Boundary conditions such as curing conditions, specimen types and surface states have a significant impact on the results of accelerated carbonation tests of concrete. In this paper, three typical coarse aggregate gradations (practical engineering gradation, building construction optimized gradation and hydraulic optimized gradation) were selected. The influences of curing conditions (standard curing and natural curing), specimen types (standard specimens and core specimens), and specimen surface conditions (cement paste surfaces, concrete surfaces, protective coated surfaces, and existing carbonated surfaces) on the results of accelerated carbonation tests on concrete were investigated. The quantitative relationships between carbonation depths under different boundary conditions were established. The results show that the carbonation depth of specimens using natural curing is greater than that of specimens using standard curing at each age. The carbonation depths of standard specimens at all ages are greater than those of the corresponding core specimens. Specimens with protective coated surface exhibit the best carbonation resistance, while concrete surface specimens present a relatively large carbonation depth at 28 days. At the same carbonation age, the smaller the initial natural carbonation depth of a specimen, the smaller its carbonation depth after the accelerated carbonation test. The 28-day carbonation depths of specimens with concrete surfaces are greater than those of specimens with existing carbonated surfaces. The ranking of the carbonation resistance of the concretes with the three coarse aggregate gradations remains consistent under different boundary conditions, following the order: practical engineering group>building construction optimized group>hydraulic optimized group. The research findings can provide a theoretical basis for evaluating the carbonation resistance of concrete in actual engineering structures based on laboratory accelerated carbonation test results.
刘长顺,邢朝阳,甘保柱,等.边界条件对混凝土试件加速碳化试验结果的影响研究[J].混凝土与水泥制品,2026,53(8):1-6,30. Liu Changshun,Xing Chaoyang,Gan Baozhu,et al.Study on the influence of boundary conditions on accelerated carbonation test results of concrete specimens[J].China Concrete and Cement Products,2026,53(8):1-6,30 (in Chinese).
杨建波1,张利维2,丁小平2,王有佳1,罗国栋1,于本田1,*
摘 要:干燥、大温差的西北地区特殊环境会严重影响混凝土建筑物的服役寿命。因此,开展西北地区混凝土耐久性能演变规律和损伤研究十分有必要。为真实反映服役环境,本文采用宏观、微观相结合的方法研究了高温低湿、大温差低湿环境对混凝土力学性能、早期收缩、微观结构、抗冻性能的影响。结果表明:相较于标准养护,高温低湿和大温差低湿养护混凝土的力学性能均有所降低,其中,大温差低湿养护混凝土的力学性能最低;随着养护时间的延长,混凝土的收缩值先增加后趋于稳定,标准养护混凝土的收缩值最小,大温差低湿养护混凝土的收缩值最大;随着养护时间的延长,混凝土的孔隙率降低,孔隙结构得到优化;标准养护混凝土受冻融循环损伤的影响最小,抗冻性能最优,高温低湿养护混凝土次之,大温差低湿养护混凝土抗冻性能最差。研究结果可为此类特殊环境下混凝土的耐久性能研究提供借鉴。Abstract: The special environment characterized by dryness and large temperature fluctuations in northwestern China significantly affects the service life of concrete structures. Therefore, it is essential to investigate the evolution characteristics of concrete durability and damage under such conditions. To accurately reflect the service environment, this paper used a combined macro-scale and micro-scale analysis method to investigate the influence of high-temperature low-humidity and large-temperature-difference low-humidity environments on the mechanical properties, early shrinkage, microstructure, and frost resistance of concrete. The results show that compared to standard curing, the mechanical properties of concrete cured under high-temperature low-humidity and large-temperature-difference low-humidity conditions decrease. Among them, the mechanical properties of large temperature difference-low humidity curing concrete are the lowest. As the curing time increases, the shrinkage value of concrete first increases and then gradually stabilizes. The shrinkage value of standard curing concrete is the smallest, and the shrinkage value of large temperature difference-low humidity curing concrete is the largest. With the extension of curing time, the porosity of concrete decreases and the pore structure is optimized. Standard curing concrete exhibits the least damage from freeze-thaw cycles and the best frost resistance, followed by high-temperature low-humidity curing concrete. Concrete cured under large-temperature-difference low-humidity conditions demonstrates the poorest frost resistance. The findings provide valuable insights for durability research and engineering applications of concrete structures in harsh environments such as arid regions with extreme temperature fluctuations.
杨建波,张利维,丁小平,等.西北地区特殊环境下混凝土性能演变规律试验研究[J].混凝土与水泥制品,2026,53(8):7-13. Yang Jianbo,Zhang Liwei,Ding Xiaoping,et al.Experimental study on the evolution characteristics of concrete properties under special environmental conditions in northwestern China[J].China Concrete and Cement Products,2026,53(8):7-13 (in Chinese).
王东兴1,刘欣超1,马文菲2,李雪健2,*
摘 要:在极地、高寒、液化天然气(Liquefied natural gas,LNG)储罐等极端超低温工况下,水泥基材料孔隙水易结冰膨胀,造成基体损伤、热学性能劣化,影响工程结构服役安全性。高吸水性树脂(SAP)作为优质的内养护材料,可有效调控水泥净浆孔隙结构与孔隙水状态,对提升水泥基材料超低温适配性具有显著潜力。本文以SAP粒径、水灰比为变量,结合核磁共振(NMR)、差示扫描量热法(DSC)、激光闪射法(LFA)试验,研究了SAP对降温过程(20 ℃至-60 ℃)中水泥净浆样品孔隙结构和热学性能的影响。结果表明:掺入SAP会增加样品的孔隙率,减小孔隙孔径;而增加水灰比、增大SAP粒径均会增大样品中凝胶孔和毛细孔的孔径;掺入SAP、增加水灰比、增大SAP粒径均会导致样品的热流峰高度的增加;降温过程中,样品的热扩散系数α值增加,比热容Cp值和热导率λ值降低;掺入SAP、增大SAP粒径、增加水灰比均会导致样品的α值增加,Cp值、λ值降低。研究成果可为超低温服役环境下水泥基保温防护材料的研发提供参考。Abstract: Under extreme ultra-low temperature conditions, such as those encountered in polar and alpine regions and liquefied natural gas (LNG) storage tanks, pore water in cement-based materials tends to freeze and expand, causing matrix damage and deterioration of thermal properties and thereby endangering the service safety of engineering structures. As a high-quality internal curing agent, superabsorbent polymer (SAP) can effectively regulate the pore structure and pore water state of cement paste, and presents remarkable potential in improving the ultra-low temperature adaptability of cement-based materials. With SAP particle size and water-to-cement ratio as variables, nuclear magnetic resonance (NMR), differential scanning calorimetry (DSC), and laser flash analysis (LFA) tests were conducted to investigate the effects of SAP on the pore structure and thermal performance of cement paste samples during cooling from 20 ℃ to -60 ℃. The results show that the incorporation of SAP increases the porosity and refines the pore size of samples. Increasing both the water-to-cement ratio and the SAP particle size enlarges the sizes of the gel pores and capillary pores. The addition of SAP, a higher water-to-cement ratio, and a larger SAP particle size all raise the heights of the heat-flow peaks. During cooling, the thermal diffusivity α of samples rises, while the specific heat capacity Cp and thermal conductivity λ decline. Similarly, adding SAP, increasing SAP particle size and increasing the water-to-cement ratio can elevate α and reduce Cp and λ of the samples. The findings can provide a reference for the development of cement-based thermal-insulation and protective materials for service in ultra-low temperature environments.
王东兴,刘欣超,马文菲,等.超低温环境下SAP对水泥净浆孔隙结构和热学性能的影响研究[J].混凝土与水泥制品,2026,53(8):14-19. Wang Dongxing,Liu Xinchao,Ma Wenfei,et al.Study on the influence of SAP on pore structure and thermal performances of cement paste under ultra-low temperature[J].China Concrete and Cement Products,2026,53(8):14-19 (in Chinese).
张 宁1,王 岩2,马川义1,杨嘉城2,张圣涛1,管延华2,孙仁娟2,*
摘 要:针对水泥砂浆抗渗性差、易环境劣化的问题,异辛基三乙氧基硅烷(Iso-octyl triethoxysilane,IOTES)乳液可有效提升其表面防护性能,但目前相关研究多侧重材料配比,对涂覆量、涂覆次数及间隔时间等关键涂覆工艺参数的影响尚不明确。鉴于此,本文制备了IOTES乳液,通过分析砂浆表面接触角、IOTES乳液渗透深度和砂浆吸水率,研究了涂覆工艺参数(单次涂覆量、涂覆次数、涂覆间隔时间和防护后静置时间)对砂浆防护性能的影响。结果表明:增加单次涂覆量与涂覆次数均可提高涂覆总量,有效增强了IOTES乳液对试件的防护作用;当涂覆总量相同时,合理选择单次涂覆量和涂覆次数可有效提高IOTES乳液的渗透深度;随着涂覆间隔时间的增加,试件的表面接触角和IOTES乳液渗透深度降低,吸水率增加,吸水率降低比例降低;随防护后静置时间的延长,试件的防护性能先增强后趋于稳定。研究结果可为IOTES乳液在砂浆类水泥基构件中的高效防护施工提供借鉴。Abstract: To address the poor resistance of cement mortar to water penetration and its susceptibility to environmental deterioration, iso-octyl triethoxysilane (IOTES) emulsion can be used to improve its surface protective performance. Nevertheless, existing relevant research mostly focuses on material mix proportions, while the effects of key coating process parameters including coating amount, number of coatings, and coating interval remain unclear. In view of this, an IOTES emulsion was prepared in this paper. By analyzing the surface contact angle of mortar, the penetration depth of IOTES emulsion into the mortar and the water absorption rate of mortar, the effects of coating process parameters (coating amount per application, number of coatings, coating interval time and post-treatment standing time) on the protective performance of mortar were investigated. The results show that increasing the coating amount per application and number of coatings can raise the total coating amount and significantly senhance the protective effect of IOTES emulsion on the specimens. At the same total coating amount, reasonably matching single-layer coating amount and number of coatings can effectively increase the penetration depth of IOTES emulsion. As the coating interval increases, the surface contact angle of the specimens and the penetration depth of the IOTES emulsion into the mortar decrease, the water absorption rate rises, and the percentage reduction in water absorption decreases. As the post-treatment standing time increases, the protective performance of the specimens increases at first and then tends to be stable. The findings can provide a reference for the efficient application of IOTES emulsion in the protective treatment of mortar-based cementitious components.
张宁,王岩,马川义,等.涂覆工艺参数对异辛基三乙氧基硅烷乳液改性砂浆防护性能的影响[J].混凝土与水泥制品,2026,53(8):20-24. Zhang Ning,Wang Yan,Ma Chuanyi,et al.Influence of coating process parameters on protective performance of mortar modified with iso-octyl triethoxysilane emulsion[J].China Concrete and Cement Products,2026,53(8):20-24 (in Chinese).
许万强1,2
许万强.不同载体微生物自修复混凝土的裂缝修复规律及矿化机制[J].混凝土与水泥制品,2026,53(8):25-30. Xu Wanqiang.Crack-healing behavior and mineralization mechanism of microbial self-healing concrete with various carriers[J].China Concrete and Cement Products,2026,53(8):25-30 (in Chinese).