韩云婷1,2,张 博1,2,*,杨利香1,2
摘 要:针对再生骨料植生混凝土水化产物碱性过高,孔隙环境抑制植物萌发与生长的工程难题,本文采用正交试验探究了矿渣粉(Ground granulated blast furnace slag powder,GBFS)、粉煤灰(Fly ash,FA)、FeSO4掺量对复合胶凝体系碱度的影响,确定了最优复配比例;在此基础上,设置了纯水泥基准组F0、原材料降碱组(矿物掺合料等质量取代水泥,复配FeSO4)F1、聚氨酯涂层降碱组F2,对比了2种降碱工艺对再生骨料植生混凝土碱度、抗压强度、连续孔隙率及植生性能的影响。结果表明:各组分对复合胶凝体系碱度影响的高低顺序依次为FA掺量、GBFS掺量、FeSO4掺量,最佳掺量为GBFS 30%、FA 30%、FeSO4 3%;相较F0组,F1组体系碱度明显下降,28 d抗压强度与植生性能同步优化;F2组降碱效果更突出,但力学、植生性能衰减明显;矿物掺合料协同FeSO4的降碱方案可兼顾材料的力学与生态功能。研究成果可为再生骨料植生混凝土性能优化及工程应用提供参考。Abstract: In order to solve the core problem of inhibiting plant growth in high alkali environment of recycled aggregate planting concrete, orthogonal tests were carried out to investigate the effects of ground granulated blast furnace slag powder (GBFS), fly ash (FA) and FeSO4 content on the alkalinity of composite cementitious systems, and the optimal mixing ratio was determined. On this basis, three groups were prepared, including a plain cement reference group F0, a raw material alkali-reduction group F1 (cement partially replaced by mineral admixtures at equal mass, and combined with FeSO4), and a polyurethane coating alkali-reduction group F2. The influences of the two alkali-reduction technologies on alkalinity, compressive strength, continuous porosity and planting performance of recycled aggregate planting concrete were compared. The results show that the descending order of each component according to the effect on the alkalinity of composite cementitious system follows: FA content, GBFS content, and FeSO4 content. And the optimal contents are 30% GBFS, 30% FA and 3% FeSO4. Compared with group F0, the alkalinity of group F1 decreases significantly, and both 28-day compressive strength and planting performance are improved simultaneously. Although group F2 achieves a more remarkable alkali reduction effect, its mechanical and planting performance degrade obviously. The alkali-reduction scheme combining mineral admixtures and FeSO4 can balance mechanical performance and planting performance simultaneously. The research results can provide references for performance optimization and engineering application of recycled aggregate planting concrete.
韩云婷,张博,杨利香.双路径降碱工艺下再生骨料植生混凝土碱度、力学及植生性能协同调控研究[J].混凝土与水泥制品,2026,53(8):64-69,78. Han Yunting,Zhang Bo,Yang Lixiang.Study on synergistic regulation of alkalinity, mechanical and planting performances of recycled aggregate planting concrete under dual-path alkali-reduction processes[J].China Concrete and Cement Products,2026,53(8):64-69,78 (in Chinese).
曾思清1,2,杜俊朋1,王洪泰1,张同生1,*,杨东来3
曾思清,杜俊朋,王洪泰,等.细颗粒组分调控骨架结构对砖混渣土基水泥稳定材料路用性能的影响及低碳综合效益分析[J].混凝土与水泥制品,2026,53(8):70-78. Zeng Siqing,Du Junpeng,Wang Hongtai,et al.Effect of skeleton structure regulated by fine particle fractions on pavement performance of brick-concrete residues-based cement-stabilized materials and analysis on their low-carbon comprehensive benefits[J].China Concrete and Cement Products,2026,53(8):70-78 (in Chinese).
陈 锋1,刘崇远2,莫宗云3,*
摘 要:针对传统超高性能混凝土(Ultra-high performance concrete,UHPC)水泥用量大、碳排放高、生产成本偏高的问题,同时考虑养护湿度对水泥基材料水化进程、微观结构及力学性能发展的重要性,本文采用偏高岭土、石灰石粉部分替代水泥制备了UHPC,研究了养护湿度对单掺、复掺偏高岭土和石灰石粉UHPC力学性能的影响,测试了偏高岭土的活性反应程度,分析了偏高岭土与石灰石粉的协同作用机制,并对试件的物相组成、孔结构和微观形貌进行了表征。结果表明:复掺适量偏高岭土可有效提升试件的力学性能;提高养护湿度可显著改善掺偏高岭土试件的抗折强度,但对抗压强度影响较小;养护湿度对偏高岭土的活性反应程度无明显作用,但可有效促进偏高岭土与石灰石粉的协同效应,细化基体孔结构;提高养护湿度可显著提升未掺偏高岭土试件的水泥水化程度、优化微观结构,但对复掺偏高岭土试件的水化反应与微观形貌的调控作用微弱。研究成果可为绿色低碳UHPC的养护制度优化及工程应用提供参考。Abstract: Aiming at the drawbacks of traditional ultra-high performance concrete (UHPC), including high cement dosage, large carbon emission and high production cost, and considering the critical influence of curing humidity on the hydration process, microstructure and mechanical property evolution of cement-based materials, UHPC specimens were prepared by partially replacing cement with metakaolin and limestone powder in this study. The effects of curing humidity on the mechanical properties of UHPC with single incorporation and co-incorporation of metakaolin and limestone powder were investigated. The degree of pozzolanic reaction of metakaolin was measured, the synergistic mechanism between metakaolin and limestone powder was analyzed, and the phase composition, pore structure and micro-morphology of specimens were characterized. The results show that appropriate combined incorporation of metakaolin can effectively improve the mechanical properties of specimens. Increasing curing humidity significantly enhances the flexural strength of metakaolin-containing specimens, while its effect on compressive strength is minor. Curing humidity shows negligible impact on the degree of pozzolanic reaction of metakaolin, yet it can effectively promote the synergistic effect between metakaolin and limestone powder and refine the pore structure of matrix. Increasing curing humidity remarkably promotes the cement hydration degree and optimizes the microstructure of specimens without metakaolin, whereas it exerts a weak regulatory effect on the hydration reaction and micro-morphology of metakaolin-containing specimens. The research findings can provide a reference for the optimization of curing system and engineering application of green and low-carbon UHPC.
陈锋,刘崇远,莫宗云.养护湿度调控下偏高岭土-石灰石粉复掺协同效应对UHPC性能的影响[J].混凝土与水泥制品,2026,53(8):79-84. Chen Feng,Liu Chongyuan,Mo Zongyun.Influence of the synergistic effect of metakaolin-limestone powder co-incorporation on UHPC performance under curing humidity regulation[J].China Concrete and Cement Products,2026,53(8):79-84 (in Chinese).
黄从斌,邰洪生
摘 要:为解决碱激发矿渣胶凝材料(Alkali-activated slag cementitious materials,AAS)收缩变形显著、易开裂、工程应用受限的问题,同时克服传统无机膨胀剂掺量高、膨胀时效与AAS早期收缩特征不匹配、易劣化基体力学性能等缺陷,本文采用氮气膨胀剂对AAS性能进行了改性,系统探究了不同掺量(0~4%)氮气膨胀剂对AAS工作性、收缩与力学性能及水化产物的影响。结果表明:氮气膨胀剂具有明显的缓凝增流效果,可有效延长AAS初、终凝时间并提高浆体扩展度;氮气膨胀剂通过缓凝效应与膨胀效应,降低了AAS化学收缩与自收缩变形,在1%~4%掺量下,试件28 d自收缩值最大降幅达52.5%,体积稳定性得到明显改善;氮气膨胀剂会阻滞AAS早期水化,随着其掺量增加,试件3 d、7 d抗压强度基本降低,而28 d抗压强度表现出明显的掺量阈值效应,适量掺入可提高抗压强度,过量掺入会因孔隙缺陷富集造成抗压强度下降;适量氮气膨胀剂可实现AAS收缩性能的高效调控与综合性能优化。研究成果可为低收缩型碱激发矿渣胶凝材料的性能优化及工程应用提供参考。Abstract: To address the prominent shrinkage deformation, cracking susceptibility and limited engineering application of alkali-activated slag cementitious materials (AAS), and to overcome the drawbacks of traditional inorganic expansive agents, such as high content requirement, mismatched expansion timing with the early-age shrinkage characteristics of AAS, and deterioration of the mechanical properties of the matrix, this paper adopts a nitrogen expansive agent to modify the performance of AAS. The effects of nitrogen expansive agent at various contents (0~4%) on the workability, shrinkage performance, mechanical properties and hydration products of AAS are systematically investigated. The results reveal that the nitrogen expansive agent exerts remarkable retarding and fluidizing effects, which effectively prolong the initial and final setting times of AAS and increase the slump flow of fresh paste. Combining retarding and expansive effects, the nitrogen expansive agent mitigates the chemical shrinkage and autogenous shrinkage of AAS, and at contents ranging from 1% to 4%, the maximum reduction in 28-day autogenous shrinkage value of specimens reaches 52.5%, substantially improving the volume stability of the material. The nitrogen expansive agent hinders the early hydration of AAS, resulting in a general reduction in the 3-day and 7-day compressive strength as the content increases. By contrast, the 28-day compressive strength of AAS exhibits an obvious content threshold effect, moderate addition improves compressive strength, while excessive content triggers accumulation of pore defects and consequently reduces compressive strength. Appropriate incorporation of the nitrogen expansive agent enables efficient regulation of shrinkage and comprehensive performance optimization of AAS. The research findings provide a theoretical reference for the performance optimization and engineering application of low-shrinkage alkali-activated slag cementitious materials.
黄从斌,邰洪生.氮气膨胀剂对碱激发矿渣胶凝材料工作性、收缩与力学性能的影响[J].混凝土与水泥制品,2026,53(8):85-89. Huang Congbin,Tai Hongsheng.Effect of nitrogen expansive agent on workability, shrinkage and mechanical properties of alkali-activated slag cementitious materials[J].China Concrete and Cement Products,2026,53(8):85-89 (in Chinese).
摘 要:针对磷尾矿堆存造成的环境与资源利用问题,为推进大宗固废资源化利用与低碳胶凝材料研发,本文以磷尾矿、矿渣、硅灰为复合原材料制备碱激发全固废胶凝材料,系统研究了水胶比、碱性激发剂模数、碱当量及胶凝组分比例对该材料抗压强度与干燥收缩的影响,并进行了微观分析。结果表明:随着水胶比的增大,碱激发全固废胶凝材料各龄期抗压强度降低,干燥收缩值增大;随着碱性激发剂模数与碱当量的升高,碱激发全固废胶凝材料各龄期抗压强度均先增后降,干燥收缩值增大;增大磷尾矿占比、减小矿渣占比会导致碱激发全固废胶凝材料抗压强度下降,干燥收缩值增大;适量掺入硅灰可提升碱激发全固废胶凝材料各龄期抗压强度,但掺量过大会导致抗压强度回缩,加剧干燥收缩;兼顾固废消纳量、力学性能与体积稳定性,碱激发全固废胶凝材料的最优配合比为水胶比0.30,碱性激发剂模数1.3,碱当量5%,m磷尾矿∶m矿渣∶m硅灰=65∶30∶5;适宜的碱当量能够有效激发矿物组分,水化凝胶连续均匀,基体密实度高,但当碱当量过高时,水化产物包裹固相颗粒,阻碍原材料进一步解聚,基体密实度降低。研究成果可为实现磷尾矿资源化利用及碱激发全固废胶凝材料性能优化提供参考。Aiming at the environmental problems and low resource utilization caused by accumulated phosphorus tailings, this study develops low-carbon cementitious materials and promotes the resource recovery of bulk solid wastes. Alkali-activated all-solid-waste cementitious materials were prepared using phosphorus tailings, slag and silica fume as composite raw materials. The effects of water-binder ratio, modulus of alkali activator, alkali equivalent and cementitious components ratio on compressive strength and drying shrinkage were systematically investigated, combined with microscopic characterizations. The results show that increasing the water-binder ratio of alkali-activated all-solid-waste cementitious materials reduces the compressive strength at all curing ages and raises drying shrinkage value. With the rise of modulus of alkali activator and alkali equivalent, the compressive strengths of alkali-activated all-solid-waste cementitious materials first increase and then decrease at all ages, while the drying shrinkage value increases. Increasing the ratio of phosphorus tailings and decreasing the ratio of slag leads to a decrease in the compressive strength of alkali-activated all-solid-waste cementitious materials and an increase in drying shrinkage value. Moderate addition of silica fume improves mechanical properties, whereas excessive silica fume leads to strength regression and aggravated shrinkage. Considering solid waste consumption, mechanical performance and volume stability, the optimal mix proportion of alkali-activated all-solid-waste cementitious materials is determined as follows: water-binder ratio of 0.30, modulus of alkali activator of 1.3, alkali equivalent of 5%, mphosphorus tailings∶mslag∶msilica fume = 65∶30∶5. Appropriate alkali equivalent can effectively activate mineral phases and form continuous hydration gels, resulting in a highly dense matrix, whereas excess alkali will form a coating layer on solid particles, restrain further mineral depolymerization and reduce matrix compactness. The research can provide experimental support for high-value utilization of phosphorus tailings and performance optimization of alkali-activated all-solid-waste cementitious materials.
杨大伟.碱激发全固废胶凝材料力学与干燥收缩性能研究[J].混凝土与水泥制品,2026,53(8):90-95,100. Yang Dawei.Study on mechanical properties and drying shrinkage of alkali-activated all-solid-waste cementitious materials[J].China Concrete and Cement Products,2026,53(8):90-95,100 (in Chinese).
陈 瑶,谭慧静*,王馨浒,崔曦月,郑云天,王宇昊
陈瑶,谭慧静,王馨浒,等.物理发泡矿渣-粉煤灰基地聚物地热井保温复合材料的制备及性能研究[J].混凝土与水泥制品,2026,53(8):96-100. Chen Yao,Tan Huijing,Wang Xinhu,et al.Preparation and properties of physically foamed slag-fly ash-based geopolymer thermal insulation composites for geothermal wells[J].China Concrete and Cement Products,2026,53(8):96-100 (in Chinese).