全部文章

水泥制品与建筑结构

陆云才1,董晓农2,*, 窦铁生2,李 萌2,罗纬邦1,陈国庆2,杨 森2

摘   要:西北高盐渍地区预应力钢筒混凝土管(Prestressed concrete cylinder pipe,PCCP)保护层易发生Cl-侵蚀,而目前关于长期轴向拉伸荷载与腐蚀环境耦合作用下的劣化机理研究仍较为薄弱,本文以立式浇筑PCCP混凝土保护层为研究对象,设计了一种卧式轴拉侵蚀试验装置,开展了不同荷载水平与侵蚀时间下的Cl-扩散试验,探究了PCCP保护层Cl-的侵蚀演化规律。结果表明:随着侵蚀时间的增加,Cl-扩散深度和 Cl-浓度均呈缓慢增大趋势;表面Cl-浓度与侵蚀时间呈非线性正相关关系,而Cl-扩散系数与侵蚀时间呈非线性负相关关系;拉伸荷载会诱发混凝土内部微裂纹萌生、张开与扩展,裂纹延展方向与Cl-扩散方向一致,这会加速Cl-渗透进程。研究成果可为高盐渍地区PCCP保护层耐久性能设计、病害防控与服役寿命评估提供理论参考,也可为后续多因素耦合作用下耐久性能衰减模型的构建提供参考。Abstract: In the high-salinity regions of Northwest China, the protective layer of prestressed concrete cylinder pipe (PCCP) is susceptible to Cl- erosion. However, current research on the deterioration mechanisms under the coupling effect of long-term axial tensile loading and corrosive environments remains insufficient. In this study, the concrete cover of vertically cast PCCP is taken as the research object, and a horizontal axial tensile erosion testing device is designed. Chloride diffusion tests are conducted under various load levels and erosion times to investigate the Cl- erosion evolution law in the PCCP protective layer. The results indicate that with increasing erosion time, both the Cl- diffusion depth and Cl- concentration exhibit a gradually increasing trend. The surface Cl- concentration shows a nonlinear positive correlation with erosion time, whereas the Cl- diffusion coefficient exhibits a nonlinear negative correlation with erosion time. Tensile loading induces the initiation, opening, and propagation of microcracks within the concrete, and the crack propagation direction aligns with the Cl- diffusion direction, thereby accelerating the Cl- penetration process. The findings can provide a theoretical reference for the durability design, disease prevention and control, and service life assessment of PCCP protective layers in high-salinity regions, and also offer a basis for the subsequent establishment of durability degradation models under multi-factor coupling conditions.
陆云才,董晓农,窦铁生,等.长期轴向拉伸荷载与Cl-侵蚀耦合作用下PCCP混凝土保护层的Cl-扩散规律[J].混凝土与水泥制品,2026,53(9):57-61. Lu Yuncai,Dong Xiaonong,Dou Tiesheng,et al.Cl- diffusion behavior in the concrete cover of PCCP under the coupling effect of long-term axial tensile loading and Cl- erosion[J].China Concrete and Cement Products,2026,53(9):57-61 (in Chinese).

刘祎霖,肖 明,徐传阳*,韩文龙,吕晚晴,马明凤,孙 浩

刘祎霖,肖明,徐传阳,等.密肋夹芯保温外挂墙板结构设计方法及工程应用[J].混凝土与水泥制品,2026,53(9):62-67,72. Liu Yilin,Xiao Ming,Xu Chuanyang,et al.Structural design method and engineering application of multi-ribbed sandwich insulated external wall panels[J].China Concrete and Cement Products,2026,53(9):62-67,72 (in Chinese).
摘   要:针对广澳高速公路改扩建工程软土路基易产生不均匀沉降、渗透变形等问题,为优化水泥土搅拌桩加固效果、提升桩体强度与抗渗性能,同时实现工业固废资源化利用,本文采用磷石膏复配早强剂改性水泥土,通过正交试验研究磷石膏掺量、水泥掺量及早强剂掺量对固化水泥土力学性能与渗透性能的影响。结果表明:水泥掺量对7 d和28 d无侧限抗压强度的影响最大;磷石膏掺量对7 d和28 d渗透系数的影响最显著,水泥掺量和早强剂掺量对7 d和28 d渗透系数的影响不显著;综合考虑无侧限抗压强度和渗透系数,建议最优配合比组合为A3B3C2,即磷石膏、水泥、早强剂掺量分别为10%、25%、1.0%,此时试件的28 d无侧限抗压强度和渗透系数均满足该路基工程要求。研究成果可为磷石膏在类似软土地基加固工程中的应用提供参考。Abstract: To address issues such as uneven settlement and seepage deformation in soft soil subgrades during the reconstruction and expansion project of the Guangzhou-Macao Expressway, and to optimize the reinforcement effect of cement-soil mixing piles, enhance their strength and impermeability, while simultaneously promoting the resource utilization of industrial solid waste, this study employs phosphogypsum compounded with an early-strength agent to modify the cement-soil. Orthogonal experiments were conducted to investigate the effects of phosphogypsum content, cement content, and early-strength agent content on the mechanical properties and permeability characteristics of the solidified cement-soil. The results indicate that cement content exerts the greatest influence on the 7-day and 28-day unconfined compressive strength. Phosphogypsum content shows the most significant effect on the 7-day and 28-day permeability coefficients, whereas the influences of cement content and early-strength agent content on these coefficients are not significant. Considering both unconfined compressive strength and permeability coefficient comprehensively, the optimal mix proportion is recommended as A3B3C2, namely 10% phosphogypsum, 25% cement, and 1.0% early strength agent. Under this formulation, both the 28-day unconfined compressive strength and the permeability coefficient meet the requirements of this subgrade project. The findings can provide a reference for the application of phosphogypsum in similar soft soil foundation reinforcement projects.
项许,牛智勇,栾从起,等.磷石膏复配早强剂改良滨海地区软土路基水泥土搅拌桩的试验研究[J].混凝土与水泥制品,2026,53(9):68-72. Xiang Xu,Niu Zhiyong,Luan Congqi,et al.An experimental study on cement-soil mixing piles improved by phosphogypsum compound early-strength agent in coastal soft soil subgrade[J].China Concrete and Cement Products,2026,53(9):68-72 (in Chinese).