全部文章

固废活化改性与低碳胶凝材料体系创新

摘   要:镍铁渣是一种冶炼工业废渣,常被资源化加工为辅助胶凝材料或骨料,但镍铁渣粉的水化活性偏低,且其作为细骨料易诱发碱-硅酸反应(Alkali-silica reaction,ASR),制约了镍铁渣的工程应用。为此,本文采用碱-湿碳化法制备碳化镍铁渣粉,通过膨胀和质量变化试验,研究了碳化镍铁渣粉掺量(0、10%、30%、50%)对镍铁渣细骨料混凝土ASR的抑制作用,并进行了微观分析。结果表明:碳化镍铁渣粉的掺入显著降低了试件的28 d膨胀率和质量变化率;碳化镍铁渣粉中的CaCO3晶体能在碱性环境中稳定存在,并降低体系中的Ca(OH)2含量,从而有效抑制ASR;碳化镍铁渣粉能促进生成低钙硅比的C-S-H凝胶,其具有较强的碱金属离子吸附能力和较低的吸水率,能有效抑制ASR凝胶的形成和膨胀;碳化镍铁渣粉可减小界面过渡区厚度,增强浆体-骨料界面结合力,并通过填充孔隙显著降低体系孔隙率,从而抑制ASR发展。研究成果可为镍铁渣的高值资源化利用提供参考。Abstract: Ferronickel slag is a smelting industrial waste residue that is often valorized as a supplementary cementitious material or aggregate. However, the hydration activity of ferronickel slag powder is relatively low, and its use as fine aggregate tends to induce alkali-silica reaction (ASR), which restricts the engineering application of ferronickel slag. To address this issue, this study prepared carbonated ferronickel slag powder using an alkali-wet carbonation method. Through expansion and mass change tests, the inhibitory effects of carbonated ferronickel slag powder at different dosages (0, 10%, 30%, and 50%) on ASR in concrete containing ferronickel slag fine aggregate were investigated, along with microstructural analysis. The results show that the incorporation of carbonated ferronickel slag powder significantly reduces the 28-day expansion rate and mass change rate of the specimens. The CaCO3 crystals present in the carbonated ferronickel slag powder remain stable in the alkaline environment and reduce the Ca(OH)2 content in the system, thereby effectively suppressing ASR. The carbonated ferronickel slag powder promotes the formation of C-S-H gel with a low Ca/Si ratio, which exhibits strong alkali metal ion adsorption capacity and low water absorption, effectively inhibiting the formation and expansion of ASR gel. In addition, the carbonated ferronickel slag powder reduces the thickness of the interfacial transition zone, enhances the paste-aggregate interfacial bonding, and significantly lowers the porosity of the system through pore filling, thus restraining ASR development. The findings can provide a reference for the high-value resource utilization of ferronickel slag.
王心茹,于淇,王伟,等.碳化镍铁渣粉对镍铁渣细骨料混凝土碱-硅酸反应的抑制机理[J].混凝土与水泥制品,2026,53(10):1-6. Wang Xinru,Yu Qi,Wang Wei,et al.The inhibition mechanism of carbonated ferronickel slag powder on the alkali-silica reaction in ferronickel slag fine aggregate concrete[J].China Concrete and Cement Products,2026,53(10):1-6 (in Chinese).

贾斯博1,王玉池2,黄想禄2,刘君实1,李欣欣1,郭厚良1,任福民1,*

贾斯博,王玉池,黄想禄,等.碳化赤泥-磷石膏复合胶凝材料体系协同性能与机理研究[J].混凝土与水泥制品,2026,53(10):7-13. Jia Sibo,Wang Yuchi,Huang Xianglu,et al.Study on synergistic properties and mechanism of carbonated red mud-phosphogypsum composite cementitious material system[J].China Concrete and Cement Products,2026,53(10):7-13 (in Chinese).

赵 栋1,冯 元2,把永神1,韩耀凯1,赵 刚1,于本田1,*

摘   要:地聚物与工程水泥基复合材料(Engineering cement-based composite,ECC)协同作用,在降低环境负荷的同时可提升结构的整体性能。为优化二者复掺配合比并揭示其拉伸演变规律,本文研究了液固比、激发剂模数、激发剂浓度对碱激发粉煤灰-矿渣ECC拉伸性能、抗压和抗折强度的影响,并分析了其水化产物组成及微观形貌。结果表明:随着液固比的增加,试件的拉伸性能先增后降,抗压和抗折强度降低;随着激发剂模数的增加,试件的初裂应力、拉伸应力、抗折和抗压强度均先增后降,拉伸应变增加;随着激发剂浓度的增加,试件的拉伸性能、抗压和抗折强度均先增后降;综合来看,当液固比为0.525、激发剂模数为1.5、激发剂浓度为6%时,碱激发地聚物ECC的性能最优。研究成果可为碱激发地聚物ECC的配合比优化及在绿色建筑结构中的应用提供参考。Abstract: The synergistic effect between geopolymer and engineered cementitious composite (ECC) can improve the overall structural performance while reducing environmental burden. To optimize the mix proportion of the two components and reveal the evolution of tensile property, this paper investigated the effects of liquid-solid ratio, activator modulus and activator concentration on the tensile property, compressive and flexural strengths of alkali-activated fly ash-slag ECC, and characterized the hydration product composition and microscopic morphology. The results reveal that with increasing liquid-solid ratio, the tensile performance of specimens rises first and then declines, accompanied by decreasing compressive and flexural strengths. As the activator modulus increases, the initial cracking stress, tensile stress, flexural strength and compressive strength all increase initially followed by a decrease, whereas tensile strain keeps growing. Increasing activator concentration leads to an initial improvement and subsequent deterioration in tensile performance, compressive strength and flexural strength. Overall, alkali-activated geopolymer ECC achieves optimal performance at a liquid-solid ratio of 0.525, activator modulus of 1.5 and activator concentration of 6%. The research findings provide references for mix proportion optimization of alkali-activated geopolymer ECC and its application in green building structures.
赵栋,冯元,把永神,等.碱激发粉煤灰-矿渣地聚物ECC的拉伸性能研究[J].混凝土与水泥制品,2026,53(10):14-19. Zhao Dong,Feng Yuan,Ba Yongshen,et al.Study on the tensile property of alkali-activated fly ash-slag geopolymer ECC[J].China Concrete and Cement Products,2026,53(10):14-19 (in Chinese).

宋丽莎1,贺烨萌1,贾东洋2,李长明2,*,王耀宗2

宋丽莎,贺烨萌,贾东洋,等.活化白云石粉改性纤维增强水泥基复合材料强度及变形性能的研究[J].混凝土与水泥制品,2026,53(10):20-26. Song Lisha,He Yemeng,Jia Dongyang,et al.Study on the strength and deformation properties of fiber-reinforced cementitious composites with activated dolomite powder[J].China Concrete and Cement Products,2026,53 (10):20-26 (in Chinese).

刘小敏1,伍思则1,2,*,孙其星1,蒋建国2,钱若滢1

刘小敏,伍思则,孙其星,等.煅烧活化油页岩渣水化特性及其作为水泥混合材的应用研究[J].混凝土与水泥制品,2026,53(10):27-32. Liu Xiaomin,Wu Size,Sun Qixing,et al.Hydration characteristics of calcined oil shale residue and its application as cement admixture[J].China Concrete and Cement Products,2026,53(10):27-32 (in Chinese).

徐为海1,吴晓亮1,罗宇栋2,苗永红2,*,殷 杰2,张兆昌2

徐为海,吴晓亮,罗宇栋,等.石英粉与粉煤灰对砂浆性能、水化特性与碳排放的影响[J].混凝土与水泥制品,2026,53(10):33-39. Xu Weihai,Wu Xiaoliang,Luo Yudong,et al.Effects of quartz powder and fly ash on mortar properties, hydration characteristics, and carbon emissions[J].China Concrete and Cement Products,2026,53(10):33-39 (in Chinese).