房建材料及制品
朱号令,邵永健*,张 威
摘 要:设计制作了25个高强钢筋页岩陶粒混凝土构件,研究了其局部受压破坏形态,分析了混凝土强度等级、钢筋骨架等参数对局部受压构件可靠度指标的影响。结果表明:局部受压构件的破坏模式为劈裂破坏;随着混凝土强度等级的提高,构件的可靠度指标降低;Ab /Al对构件可靠度指标的影响很小;随着Acor /Al的增大,构件的可靠度指标增大;配置钢筋骨架和间接钢筋能有效提高局部受压构件的可靠度指标,仅配置钢筋骨架对局部受压构件的可靠度指标无明显提升作用。
Abstract: A total of 25 high-strength reinforced shale ceramsite concrete components were designed to investigate their local compression failure modes. The influence of concrete strength grade, reinforcement cages and other parameters on the reliability index of local compression components was analyzed. The results indicate that the failure mode of local compression components is splitting failure. With the increase of concrete strength grade, the reliability index of components decreases. The impact of Ab /Al on the reliability index of components is minimal. As the value of Acor /Al increases, the reliability index of the component also increases. Configuring reinforcement cages and indirect steel bar can effectively improve the reliability index of local compression components, however, configuring only reinforcement cages does not enhance the reliability index.
朱号令,邵永健,张威.高强钢筋页岩陶粒混凝土构件局部受压性能研究及可靠度分析[J].混凝土与水泥制品,2025(3):64-68.
ZHU H L,SHAO Y J,ZHANG W.Study on local compression and reliability analysis of high-strength reinforced shale ceramsite concrete components[J].China Concrete and Cement Products,2025(3):64-68.
严 俊1,彭 胜2,*,瞿 聪2,陈凤琪2
摘 要:制备了超高韧性水泥基复合材料(UHTCC)-再生骨料混凝土(RAC)叠合楼板试件,研究了UHTCC层的厚度(0、10、20 mm)和纤维种类(PE纤维、PVA纤维、钢纤维)对RAC的约束效果,分析了浆体的流动度和试件的轴压性能,并进行了微观分析。结果表明:纤维的掺入降低了浆体的流动度;UHTCC能有效约束RAC破坏,使RAC的破坏模式从脆性破坏转变为纵向剪切及横向屈曲联合破坏;与PE纤维和钢纤维相比,PVA纤维对试件延性的改善效果更好。
Abstract: Ultra-high toughness cement-based composite material(UHTCC)-recycled aggregate concrete (RAC) composite floor slab specimens were prepared, and the confinement effects of varying UHTCC layer thickness (0, 10, 20 mm) and different fiber types (PE fiber, PVA fiber, steel fiber) on RAC were studied. The flowability of the slurry and the axial compression performance of the specimens were evaluated, along with microscopic analysis. The results indicate that the addition of fibers decreases the flowability of the slurry. UHTCC can effectively mitigate the failure of RAC, altering its failure mode from brittle failure to a combination of longitudinal shear and transverse buckling failure. Among the fiber types, PVA fiber exhibits superior performance in enhancing the ductility of specimens.
严俊,彭胜,瞿聪,等.超高韧性水泥基复合材料层对RAC叠合楼板性能的影响[J].混凝土与水泥制品,2025(3):69-72.
YAN J,PENG S,QU C,et al.Effect of ultra-high toughness cement-based composite material layer on properties of RAC composite floor slab[J].China Concrete and Cement Products,2025(3):69-72.
杨 萍,刘 洋,张阿瑶,华靖文*
摘 要:通过正交试验研究了减水剂用量(2.1~2.5 g)、羟丙基甲基纤维素醚(HPMC)用量(0.8~1.2 g)、不同粒径(0.08~0.30 mm、0.30~0.60 mm)砂用量对水泥基自流平砂浆流动度的影响。结果表明:HPMC用量对水泥基自流平砂浆流动度的影响最大,其次为减水剂用量,最后为不同粒径砂用量;优化后的水泥基自流平砂浆配合比组合为减水剂用量2.3 g、HPMC用量1.0 g、粒径0.08~0.30 mm砂用量460 g、不掺粒径0.30~0.60 mm砂,其初始、20 min流动度分别为151 mm、134 mm,满足相关标准要求。
Abstract: The effects of water reducing agent dosage (2.1~2.5 g), hydroxypropyl methyl cellulose ether (HPMC) dosage (0.8~1.2 g), and sand dosage with different particle sizes(0.08~0.30 mm, 0.30~0.60 mm) on the flowability of cementitious self-levelling mortar were investigated through orthogonal experiments. The results show that the HPMC dosage has the most significant impact on the flowability, followed by the water reducing agent dosage, and lastly the sand dosage with different particle sizes. The optimized mix proportion of cementitious self-levelling mortar is 2.3 g of water reducing agent, 1.0 g of HPMC, 460 g of sand with particle size of 0.08~0.30 mm, and no sand with particle size of 0.30~0.60 mm. Under those conditions, the initial and 20 min flowability are 151 mm and 134 mm, respectively, which meets the requirements of the relevant standard.
杨萍,刘洋,张阿瑶,等.基于正交试验的水泥基自流平砂浆流动度研究[J].混凝土与水泥制品,2025(3):73-76.
YANG P,LIU Y,ZHANG A Y,et al.Study on flowability of cementitious self-levelling mortar based on orthogonal experiment[J].China Concrete and Cement Products,2025(3):73-76.