复掺粉煤灰和矿粉对3D玻璃纤维织物增强水泥耐久性的研究

Study of Mixed Fly Ash and Slag Powder on Durability of 3D Glass Fiber Fabric Reinforced Cement

浏览量:

关键词:

GRC;碱度;抗弯强度;耐久性

Key words:

GRC; Alkalinity; Flexural strength; Durability

刊期:

2016年第8期

DOI:

文章编号:

1000-4637(2016)08-46-04

基金项目:

国家科技支撑计划项目(2013BAJ10B03)

作者:

朱雪峰1,张 朋1,李清海2,李东旭1

单位:

1.南京工业大学材料科学与工程学院,210009;2.中国建筑材料科学研究总院,北京 100024)

摘要

摘   要:从Ca(OH)2含量、碱度、抗弯强度三个方面考察了复掺粉煤灰、矿粉对3D玻璃纤维织物增强水泥耐久性的影响。结果表明,复掺粉煤灰、矿粉降低了试件的碱度,减少了碱对玻璃纤维的侵蚀,同时还可提高试件强度,改善3D玻璃纤维增强水泥的耐久性。

 Abstract: The influences of mixed fly ash and slag powder on durability of 3D glass fiber fabric reinforced cement from three aspects of Ca(OH)2, alkalinity and flexural strength are studied.  The results indicate that, it can reduce alkalinity of mixed fly ash and slag powder, which can also reduce corrosion of glass fiber, meanwhile, strength of specimens is increased, durability of 3D glass fiber fabric reinforced cement is improved. 

结论

(1)在3D玻璃纤维织物增强水泥中复掺粉煤灰和矿粉可以减少试件中Ca(OH)2含量,降低试件的碱度,减少试件中碱对玻璃纤维的侵蚀。
(2)在基体中复掺粉煤灰和矿粉,经高温加速老化后,试件的抗弯强度呈先增大后减小的变化趋势:一方面,高温促进了矿物掺合料的水化;另一方面,矿物掺合料水化会消耗试件中的碱性物质,但随着试件中的玻璃纤维侵蚀,试件强度下降。同时,经高温加速老化后,掺加矿物掺合料试件的抗弯强度高于空白试件。 

参考文献

[1] 沈荣熹,崔琪,李清海.新型纤维增强水泥基复合材料[M]. 北京:中国建材工业出版社,2004.
[2] 王燕谋.中国玻璃纤维增强水泥[M].北京:中国建材工业出版社,2000.
[3] 刘志成,崔琪,李清海.不同维度玻璃纤维对 GRC 力学性能影响研究[J].混凝土与水泥制品,2015(5):46-49.
[4] UK. BS EN-1170-5:1998  Precast concrete products-Test method for glass-fibre reinforced cement-Part 5 Measuring bending strength,‘Complete bending test’method[S].London:BSI publication,1998.
[5] 葛敦世.玻璃纤维碱侵蚀机理和耐碱性的探讨[J].玻璃纤维,2007(1):1-9.
[6] 杨南如. 机非金属材料测试方法[M].武汉:武汉工业大学出版社,1990.
[6] 胡红梅,沈雅雯,王昊.粉煤灰与矿粉的复合效应研究[J].粉煤灰,2013(1):11-13.
[7] 周万良,方坤河,詹炳根.掺粉煤灰、矿粉混凝土抗碳化性能研究[J].混凝土与水泥制品,2012(12):14-19. 

引用本文


上一个: 端锚CFRP-混凝土黏结界面受剪性能试验研究

下一个: 挤扩支盘桩的研究进展

相关文件