铁尾矿颗粒形貌对砂浆尺寸稳定性影响的研究
Effects Research of Particle Morphology of Iron Tailing on Dimension Stability of Mortar
2016年第9期
铁尾矿;颗粒形貌;砂浆试件;尺寸收缩
Iron ore tailing; Particle morphology; Mortar specimen; Dimensional shrinkage
2016年第9期
1000-4637(2016)09-86-05
李晓光,陈 婷,卢 攀
长安大学建筑工程学院,西安 710061

李晓光,陈 婷,卢 攀

浏览量:
1000
摘 要:为研究铁尾矿颗粒形貌对砂浆尺寸稳定性的影响,利用光学显微镜观察了铁尾矿砂、天然河砂和普通机制砂的颗粒形貌并对其进行了定量描述,探索量化指标对砂浆尺寸稳定性的影响规律。试验结果表明,三种细骨料中,铁尾矿砂的针片状、非球形程度最高,其颗粒表面光滑但存在最多的尖锐棱角。在干燥环境下,细骨料较低的OR值和RK值将显著增加砂浆试件的收缩值。由于铁尾矿砂这两个指标最低,其砂浆试件的尺寸稳定性低于天然河砂和普通机制砂砂浆试件。不同粒级的铁尾矿砂所配制的砂浆试件尺寸稳定性试验证明,此时影响砂浆尺寸稳定性主要因素不是颗粒形貌,而是粒级范围,粒级范围越小,则铁尾矿砂浆试件的尺寸收缩越大。 Abstract: The influence of particle morphology for iron ore tailing on dimension stability of mortar was studied, particle morphology for iron tailings sand(IOT), nature river sand(NS) and manufactured sand(MS) was observed by optical microscope, influence rules of quantitative description and indicators on stability of mortar dimension is carried out. The results show that, The results show that IOT sand is flakiness, has greater degree of irregular shape and smoother surface, which exists the most sharper edges and corners in three kinds of fine aggregates. Under dry environment, lower OR value and RK value for fine aggregates will be increased obviously through shrinkage value. Dimension stability of mortar specimens is lower than that of NS specimens and MS specimens, because of lowest OR value and RK value. Experiment of dimension stability for mortar specimens is proved by prepared IOT with different grain size, the main effecting factors of dimension stability of mortar is grain rang, not particle morphology, demensional shrinkage of IOT mortar specimens becomes greater with smaller grain range.
英文名 : Effects Research of Particle Morphology of Iron Tailing on Dimension Stability of Mortar
刊期 : 2016年第9期
关键词 : 铁尾矿;颗粒形貌;砂浆试件;尺寸收缩
Key words : Iron ore tailing; Particle morphology; Mortar specimen; Dimensional shrinkage
刊期 : 2016年第9期
DOI :
文章编号 : 1000-4637(2016)09-86-05
基金项目 :
作者 : 李晓光,陈 婷,卢 攀
单位 : 长安大学建筑工程学院,西安 710061

李晓光,陈 婷,卢 攀

摘要
参数
结论
参考文献
引用本文

摘   要:为研究铁尾矿颗粒形貌对砂浆尺寸稳定性的影响,利用光学显微镜观察了铁尾矿砂、天然河砂和普通机制砂的颗粒形貌并对其进行了定量描述,探索量化指标对砂浆尺寸稳定性的影响规律。试验结果表明,三种细骨料中,铁尾矿砂的针片状、非球形程度最高,其颗粒表面光滑但存在最多的尖锐棱角。在干燥环境下,细骨料较低的OR值和RK值将显著增加砂浆试件的收缩值。由于铁尾矿砂这两个指标最低,其砂浆试件的尺寸稳定性低于天然河砂和普通机制砂砂浆试件。不同粒级的铁尾矿砂所配制的砂浆试件尺寸稳定性试验证明,此时影响砂浆尺寸稳定性主要因素不是颗粒形貌,而是粒级范围,粒级范围越小,则铁尾矿砂浆试件的尺寸收缩越大。

Abstract: The influence of particle morphology for iron ore tailing on dimension stability of mortar was studied, particle morphology for iron tailings sand(IOT), nature river sand(NS) and manufactured sand(MS) was observed by optical microscope, influence rules of quantitative description and indicators on stability of mortar dimension is carried out. The results show that, The results show that IOT sand is flakiness, has greater degree of irregular shape and smoother surface, which exists the most sharper edges and corners in three kinds of fine aggregates. Under dry environment, lower OR value and RK value for fine aggregates will be increased obviously through shrinkage value. Dimension stability of mortar specimens is lower than that of NS specimens and MS specimens, because of lowest OR value and RK value. Experiment of  dimension stability for mortar specimens is proved by prepared IOT with different grain size, the main effecting factors of dimension stability of mortar is grain rang, not particle morphology, demensional shrinkage of IOT mortar specimens becomes greater with smaller grain range.

关键词:
铁尾矿;颗粒形貌;砂浆试件;尺寸收缩
扫二维码用手机看
未找到相应参数组,请于后台属性模板中添加
(1)分别用光学显微镜观察了铁尾矿砂、天然河砂及普通机制砂的几何形貌,并计算了三种细骨料的形貌特征值。与天然河砂和普通机制砂相比,铁尾矿的等效圆周长比(AIECP)值最大,其颗粒表面较光滑。而铁尾矿砂的轮廓比率(OR)值、平均圆度(RK)值和等效椭圆周长比(AIEEP)值均最小,等效圆周长比值(AIECP)最大,表明其颗粒形貌呈针片状、非球形程度较高,颗粒表面虽然较光滑但存在较多尖锐的棱角。
(2)测试试件的尺寸稳定性表明,采用规定级配的三类细骨料制备的建筑砂浆中,干燥环境中铁尾矿砂砂浆试件的收缩值高于天然河砂试件和普通机制砂试件。通过计算该级配下三种细骨料的形貌特征值可知,铁尾矿砂的OR值、RK值均低于其他两种细骨料。由此可以推断,细骨料较低OR值和RK将可能引起砂浆试件在干燥环境中产生较大的收缩。
(3)采用不同粒级范围的铁尾矿砂所制作的砂浆试件,其形貌指标对砂浆试件尺寸的稳定性影响不大,而其颗粒粒级对砂浆尺寸的稳定性影响较大。在干燥环境下,颗粒粒级范围越小,砂浆试件收缩越大。
 
[1] 佘晓燕,吴小淦,林勇康,等.铁尾矿细砂修补砂浆的配制及影响因素研究[J].新型建筑材料,2014(5):30-32.
[2] MATSCHULLAT J,BORBA R P,DESCHAMPS E.Human and environmental contamination in the iron quadrangle[J]. Applied Geochemistry,2000(15):193-200.
[3] DAS S K,KUMAR S,RAMAEHANDRARO P.Exploitation of the development of ceramietiles[J]. Waste Management,2000(20):725-729.
[4] 洪乃丰.震后反思“海砂屋”[J].腐蚀与防护,2008(7):426-428.
[5] 陆厚根.粉体工程导论[M].上海:同济大学出版社,1993.
[6] 徐飞.粗骨料颗粒形状评定方法的研究[J].扬州大学学报:自然科学版,2002(2):61-63.
[7] Chun Yi Kuo, Reed B. Freeman Imaging Indices for Quantification of Shape, Angularity, and Surface Texture of Aggregates[C]. Transportation Research Board,79th Annual Meeting January,2000:9-13.
[8] 徐定华,徐敏. 混凝土材料学概论[M].北京:中国标准出版社,2002.
[9] C.F.Mora, A.K.H.Kwan. Sphericity, shape factor and convexity measurement of coarse aggregate for concrete using digital image processing[J]. Cement and Concrete Research,2000,30(3):351-358.
[10] KRUMBEIN W C. Measure and geological significance of shape and roundness of sedimentary particles[J].Journal of Sedimentary Petrology,1941(11):64-72.
[11] 李晓光,景帅帅,马玉平.铁尾矿水泥砂浆的力学性能及孔结构特征[J].混凝土,2014(6):124-128.

相关文件

暂时没有内容信息显示
请先在网站后台添加数据记录。

关注《混凝土与水泥制品》

总访问量 468,401   网站统计

官方微信公众号关闭
苏州混凝土水泥制品研究院有限公司

关于我们    |    联系我们    |    订购杂志    |    回到顶部

版权所有:中国混凝土与水泥制品网  苏ICP备10086386号   网站建设:中企动力 苏州

版权所有:中国混凝土与水泥制品网

苏ICP备10086386号

网站建设:中企动力 苏州